| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 3.65 GPa | 530 ksi | Resin |
|
Renegade Materials Corporation RM-5003 Cyanate Ester Prepreg 4581 Quartz Fabric
Low dielectric and loss, high performance prepreg. 350°F Cure Developed with consistent handling and superior performance Designed for demanding electrical, radome and antennae applications Del..
|
|||
| Flexural Modulus | 3.65 GPa | 530 ksi | Tangent; ASTM D790 |
|
Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled
Information provided by FIBERFIL Engineered Plastics
|
|||
| Flexural Modulus | 3.65 GPa | 530 ksi | ASTM D790 |
|
Techmer ES Electrablend® PA6/6 IM C BK
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Additive: Impact ModifierFeatures: Conductive and Impact ModifiedAppearance: BlackInformation provided by TP..
|
|||
| Flexural Modulus | 3.65 GPa | 530 ksi | secant; ASTM D790 |
|
Spartech PP5420 Glass Fiber Reinforced Homopolymer
Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech
|
|||
| Flexural Modulus | 3.65 GPa | 530 ksi | ASTM D790 |
|
Techmer ES HiFill® PA6/6 GF10 L 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 3.65 GPa | 530 ksi | ASTM D790 |
|
Techmer ES HiFill® PA6/6 GF6 HS BK 6% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 6% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance:..
|
|||
| Flexural Modulus | 3.65 GPa | 530 ksi | ASTM D790 |
|
Techmer ES Luriblend® PA6 GL15 Nylon 6
Availability: North AmericaForms: PelletsAdditive: Graphite Powder Lubricant(15%)Features: LubricatedInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 3.65 GPa | 530 ksi | 0.125 in, injection molded, unannealed; ASTM D790 |
|
Styron EMERGEâ„¢ 4731-8 Polycarbonate
EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability ..
|
|||
| Flexural Modulus | 3.65 GPa | 530 ksi | Tangent; ASTM D790 |
|
Washington Penn Homopolymer Polypropylene 20% Glass Reinforced
Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. ..
|
|||
| Flexural Modulus |
3.65
GPa @Temperature 22.8 °C |
530
ksi @Temperature 73.0 °F |
ASTM D790 |
|
Ensinger Tecapeek® Polyetheretherketone (PEEK)
TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti..
|
|||
| Flexural Modulus | 3.65 GPa | 530 ksi | ASTM D790 |
|
Asahi Kasei Thermylene® P6-20FG-0153 20% Glass Fiber Reinforced, UV Stable
Information provided by Asahi Thermofil
|
|||
| Flexural Modulus | 3.65 GPa | 530 ksi | ASTM D790 |
|
Asahi Kasei Thermylene® P6-30FG-0877A 30% Glass Fiber Reinforced, UV Stabilized
Information provided by Asahi Thermofil
|
|||
| Flexural Modulus | 3.65 - 5.03 GPa | 530 - 730 ksi | |
|
Bulk Molding Compounds BMC T60 Grey Wear Resistant Molding Compound
BMC T60 Grey is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu..
|
|||
| Flexural Modulus | 3.65 GPa | 530 ksi | ASTM D790 |
|
Asahi Kasei Thermylene® P6-40FB-Y947 40% Glass Fiber/Glass Bead, Heat Stabilized
Information provided by Asahi Thermofil
|
|||
| Flexural Modulus | 3.65 GPa | 530 ksi | ASTM D790 |
|
ScanTube PEEK Tubing
Information provided by ScanTube, Inc.
|
|||
| Flexural Modulus | 3.65 - 11.4 GPa | 530 - 1650 ksi | Average value: 9.18 GPa Grade Count:50 |
|
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
|
|||
| Flexural Modulus | 3.65 - 5.03 GPa | 530 - 730 ksi | |
|
Bulk Molding Compounds BMC T60-6006 Wear Resistant Molding Compound
BMC T60-6006 is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu..
|
|||