Polymer Property : Flexural Modulus = 551 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 3.80 GPa
<br>@Temperature 23.0 °C
551 ksi
<br>@Temperature 73.4 °F
ISO 178
Polykemi AB POLYblend 45FS GKF2505 PC/ABS-Blend, Glass Fiber reinforced
Information provided by Polykemi AB
Flexural Modulus 3.80 GPa
551 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® C4210 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C4210 is a 10% glass reinforced, non-FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low..
Flexural Modulus 3.80 GPa
551 ksi
ISO 178, ASTM D790
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66
Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app..
Flexural Modulus 3.80 GPa
<br>@Temperature 23.0 °C
551 ksi
<br>@Temperature 73.4 °F
ISO 178
Polykemi AB POLYfill PPH GF5020 PD1 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Flexural Modulus 3.80 GPa
<br>@Temperature 23.0 °C
551 ksi
<br>@Temperature 73.4 °F
ISO 178
Polykemi AB POLYfill PPH T8040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Flexural Modulus 3.80 GPa
<br>@Temperature 23.0 °C
551 ksi
<br>@Temperature 73.4 °F
ISO 178
Polykemi AB SCANAMID 66 A12^ X30 Nylon 66, Glass Fiber Reinforced
Information provided by Polykemi AB
Flexural Modulus 3.80 GPa
<br>@Temperature 23.0 °C
551 ksi
<br>@Temperature 73.4 °F
ISO 178
Polykemi AB SCANTEC PC S75R GF10 Polycarbonate, Glass Fiber Reinforced
Information provided by Polykemi AB
Flexural Modulus 3.80 GPa
551 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC (Europe-Africa-Middle East)
LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone.
Flexural Modulus 3.80 GPa
551 ksi
ASTM D790
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK) &nbsp;(Unverified Data**)
KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist..
Flexural Modulus 3.80 GPa
<br>@Temperature 23.0 °C
551 ksi
<br>@Temperature 73.4 °F
ISO 178
Polykemi AB POLYfill PPH GF5020 PD1 VT2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled, Heat Stabilized
Information provided by Polykemi AB
Flexural Modulus 3.80 GPa
<br>@Temperature 23.0 °C
551 ksi
<br>@Temperature 73.4 °F
ISO 178
Polykemi AB POLYfill PPH T1040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Flexural Modulus 3.80 GPa
551 ksi
ISO 527
Victrex® PEEK 450PF Fine Powder Grade
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, standard flow, FDA food contact complia..
Flexural Modulus 3.80 GPa
551 ksi
2 mm/min; ISO 178
Ineos ABS Lustran® SAN C Injection Molding Grade
Flexural Modulus 3.80 GPa
551 ksi
15 mm/min; ASTM D790
LG Chemical 95HC SAN Resin
Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include make-up cases and other products requiring..
Flexural Modulus 3.80 GPa
551 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific)
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Flexural Modulus 3.80 GPa
551 ksi
ASTM D790
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b..
Flexural Modulus 3.80 GPa
551 ksi
ASTM D790
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK)
KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th..
Flexural Modulus 3.80 GPa
551 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF002ER PC (Europe-Africa-Middle East)
LNP* THERMOCOMP* DF002ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features include Easy Molding, Mold Release.
Flexural Modulus 3.80 GPa
551 ksi
2mm/min; ISO 178
Teijin Panlite® G-3330M Isotropic, Glass Fiber Reinforced Polycarbonate Resin
Reinforced with 30 % of special GF and least anisotropy grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need good appearance and mechanical propertyPrecisio..
Flexural Modulus 3.80 GPa
551 ksi
ASTM-D790
Polyram RamShine PV102 ABS, General Purpose
General purpose ABS for injection molding applicationsInformation provided by Polyram Ram On Ind.
Flexural Modulus 3.80 GPa
551 ksi
ASTM D 790
Cossa Polimeri ESTAPROP H 1080 TG Polypropylene, 40% Mineral Filled
PP homopolymer 40% mineral fillerExcellent stiffness, good dimensional stabilityInformation provided by Cossa Polimeri S.r.l.
Flexural Modulus 3.80 GPa
551 ksi
ISO 178
Cossa Polimeri ESTABLEND PA 1040 GF HI ABS / Nylon 6 Blend, 20% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.20% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi..
Flexural Modulus 3.80 GPa
551 ksi
ASTM D790
Chem Polymer Chemlon 218 GV Nylon 6, 18% Glass Reinforced
A flame retardant, glass reinforced grade of nylon 6. The material is UL94 V0 rated, completely non-halogenated and phosphorus free. It gives excellent surface appearance and is available in a ran..
Flexural Modulus 3.80 GPa
551 ksi
2mm/min; ISO 178
Teijin Panlite® GV-3410R High Flame Retardancy, Glass Fiber Reinforced Polycarbonate Resin
GF 10% reinforced, improved flame retardance and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecis..
Flexural Modulus 3.80 GPa
<br>@Temperature 23.0 °C
551 ksi
<br>@Temperature 73.4 °F
ISO 178
Polykemi AB POLYfill PPH T5040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Flexural Modulus 3.80 GPa
551 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP GX94043L PSU (Europe-Africa-Middle East)
LNP* THERMOCOMP* GX94043L is a compound based on Polysulfone resin containing Mineral.
Flexural Modulus 3.80 GPa
551 ksi
ISO 178
Polyplastics Duracon® GB-25 Acetal Co-polymer (POM), Low warpage, GB 25% filling
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Flexural Modulus 3.80 GPa
551 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL PX2391 PPE+HIPS (Europe-Africa-Middle East)
PX2391 is a 10% glass fiber reinforced, heat stabilized, low odor and low emission NORYL(R) grade for interior automotive applications, especially instrument panels
Flexural Modulus 3.80 GPa
<br>@Temperature 23.0 °C
551 ksi
<br>@Temperature 73.4 °F
ISO 178
Polykemi AB POLYfill PPH T5040 FC VT Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Flexural Modulus 3.80 GPa
<br>@Temperature 23.0 °C
551 ksi
<br>@Temperature 73.4 °F
ISO 178
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac..