| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Nylene® PA6 Glass/Mineral Filled 7115 HS Nylon 6
15% Glass; 25% Mineral; Dry as molded.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
PolyOne Edgetek® ES-20GF-15GM/000 Polyethersulfone - 20% Glass Fiber - 15% Milled Glass
(discontinued **)
Data provided by PolyOne.
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP DCL32 PC (Europe-Africa-Middle East)
LNP* LUBRICOMP* DCL32 is a compound based on Polycarbonate resin contqaining Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive.
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL36 PC (Europe-Africa-Middle East)
LNP* Lubricomp* DFL-4036 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE.
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Plenco 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **)
Plaslok 201 is a two-stage, woodflour and mineral-filled phenolic molding compound formulated to have an excellent balance of molded properties. The material provides good electrical insulation val..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Plenco 204 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **)
Plaslok 204 is a two-stage, woodflour and mineral-filled phenolic molding compound formulated to accommodate a wide range of molding situations. In addition, it is recommended for use in thin wall ..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Plenco 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **)
Plaslok 308 is a two-stage, mineral and flock-filled phenolic molding compound designed to withstand the hostile environment of high abrasion and high tangential speed of engine pulleys. It is char..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Plenco 308 Black (INJ) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **)
Plaslok 308 is a two-stage, mineral and flock-filled phenolic molding compound designed to withstand the hostile environment of high abrasion and high tangential speed of engine pulleys. It is char..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Plenco 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **)
Plaslok 309 is a two-stage, mineral and fiber-filled phenolic molding compound having excellent impact strength; and as such, is considered a good candidate for replacing chopped-fiber filled compou..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Plenco 309 Black (INJ) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **)
Plaslok 309 is a two-stage, mineral and fiber-filled phenolic molding compound having excellent impact strength; and as such, is considered a good candidate for replacing chopped-fiber filled compou..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Plaslok 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 201 is a two-stage, woodflour and min..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Plaslok 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 308 is a two-stage, mineral and flock..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Plaslok 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Plaslok 309 Black (INJ) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Global 508 30% Glass Filled PBT Gray
Information provided by Global Polymers Corporation.
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | |
|
Haysite ETS-FR-II Glass Reinforced Polyester Sheet, Electrical Grade (GPO2)
A NEMA GPO-2 glass mat reinforced thermoset polyester molded sheet. ETS-FR-II is UL recognized with a flame rating of 94V-0 and arc resistance of 185 seconds. This grade is an IEEE Thermal Class B, ..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | DIN 53452; ASTM D790 |
|
Kolon Kopa® KN163G30 Nylon 6 Resin
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI
LNP* LUBRICOMP* EX06405 is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible, Easy Molding.
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Sumitomo Bakelite North America 775 CAF Mineral Filled Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ISO 178 |
|
Polyplastics Duranex® CN5315 Polybutylene Terephthalate (PBT), Higher gloss, Better surface appearance, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
|
|||
| Flexural Modulus |
6.90
GPa @Temperature 120 °C |
1000
ksi @Temperature 248 °F |
ISO 178 |
|
DSM Stanyl® OCD2300 BLK PA46-GF50
50% Glass Reinforced, Heat Stabilized
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Adell AT-37 Nylon 66, 35% Glass Reinforced; Impact Modified
Data provided by Adell Plastics, Inc.
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Ashley Polymers Ashlene® 68MG Nylon 66, Glass/Mineral reinforced
A glass/mineral reinforced nylon offering excellent dimensional stability and rigidity.Data provided by the manufacturer
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Ashley Polymers Ashlene® 742L-33G Nylon 6/66, 33% Glass Reinforced
6/66 Copolymer with high surface gloss in addition to high stiffness and strength, 33% Glass Reinforced.Data provided by the manufacturer
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Plaslok 5440 Black General Purpose Phenolic Molding Compound
(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5440 is the replacement material for ..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Plaslok 308 Black (INJ) Mineral/Flock Filled Phenolic Molding Compound
(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 308 is a two-stage, mineral and flock..
|
|||