| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 4.50 GPa | 653 ksi | ASTM D790 |
|
Niche Polymer PA66MI40BK Nylon 66, 40% Mineral Fiber Filled, Impact Modified
Information provided by Niche Polymer
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
|
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin
Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim
|
|||
| Flexural Modulus |
4.50
GPa <br>@Temperature 90.0 °C
|
653
ksi <br>@Temperature 194 °F
|
ISO 178, ASTM D790 |
|
Nilit Nilamid A3 H6 G5 25% Glass Reinforced PA66
Description: Nilamid A3 H6 G5 is a 25% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
|
|||
| Flexural Modulus |
4.50
GPa <br>@Temperature 23.0 °C
|
653
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou..
|
|||
| Flexural Modulus | 4.50 - 31.0 GPa | 653 - 4500 ksi | Average value: 15.4 GPa Grade Count:50 |
|
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | ASTM D790 |
|
PolyOne Stat-Tech™ PI-05CF/000 Polyetherimide - 5% Carbon Fibers - ESD Applications
(discontinued **)
Data provided by PolyOne.
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | ASTM D790 |
|
PolyOne Edgetek® NJ-10GF/000 Nylon 12 - 10% Glass Fiber
(discontinued **)
Data provided by PolyOne.
|
|||
| Flexural Modulus |
4.50
-
15.4443
GPa <br>@Temperature -40.0 - 121 °C
|
653
-
2240.03
ksi <br>@Temperature -40.0 - 250 °F
|
Average value: 9.91 GPa Grade Count:3 |
|
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | |
|
Lehmann & Voss LUVOCOM® 1100-8401 Polyether sulfone, unreinforced
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | |
|
Lehmann & Voss LUVOCOM® 1100-8166 Polyether sulfone, with glass fiber, easy flowing
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP RX03643H PA 66
LNP* LUBRICOMP* RX03643H is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM 2100F PEI (Europe-Africa-Middle East)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no l..
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Ultem 2110F PEI (Europe-Africa-Middle East)
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be supported with biocompatibility informati..
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM HU2100 PEI
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom..
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM PW2100 PEI (Europe-Africa-Middle East)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified...
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Valox® 815F PBT+PET
PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics NORYL IGN5531 PPE+PS
Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor..
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Asia Pacific)
Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor..
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP AF002XXC ABS
LNP THERMOCOMP* AF002XXC is a compound based on ABS resin containing 10% Glass Fiber.
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Asia Pacific)
Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl ..
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
|
Unitika M1030DH PA6, Dry
Nano composite nylonInformation provided by Unitika Ltd.
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
|
Polyram PlusTek PA355M6 Nylon 6.6 for Injection Molding, 30% Mineral Filled, Flame Retardant
30% Minerals filled, flame retardant Nylon 6.6 for injection molding applications.Information provided by Polyram.
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
|
Polyram Polytron P30N03 Polypropylene, 30% Long Glass Fibers
A chemically coupled 30% long glass fibers reinforced natural polypropylene, heat stabilized, for injection molding applications. These products have significantly improved impact performance chara..
|
|||
| Flexural Modulus |
4.50
GPa <br>@Temperature 200 °C
|
653
ksi <br>@Temperature 392 °F
|
ISO 178 |
|
DSM Stanyl® OCD2300 BLK PA46-GF50
50% Glass Reinforced, Heat Stabilized
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | DIN 52457 |
|
CP-Polymer-Technik Wellamid® 6600 MR 309 HWCP 30% Mineral Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | ISO 178 |
|
Cossa Polimeri ESTABLEND PA 1050 GF HI ABS / Nylon 6 Blend, 25% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.25% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi..
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | DAM; ISO 178 |
|
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66
(Unverified Data**)
36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan..
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | ASTM D790 |
|
Adell AT-33 Nylon 66, 15% Glass Reinforced; Impact Modified
Data provided by Adell Plastics, Inc.
|
|||
| Flexural Modulus | 4.50 GPa | 653 ksi | 2 mm/min; ISO 178 |
|
Sax Polymers SAXALEN PPC345G30 Polypropylene Copolymer, 30% Glass Filled
SAXALEN PPC345G30 is a 30% glass filled Polypropylene - Copolymer intended for injection molding.Information provided by SAX Polymers
|
|||