| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 7.00 GPa | 1020 ksi | 1.3 mm/min; ASTM D790 |
|
Ovation Polymers RIGITRON 10030 GF Polycarbonate, 30% Glass Reinforced
PC - Glass reinforced (30 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared accor..
|
|||
| Flexural Modulus |
7.00
GPa @Temperature 23.0 °C |
1020
ksi @Temperature 73.4 °F |
ISO 178 |
|
Polykemi AB SCANTEC PC S60R GF30 Polycarbonate, Glass-Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | |
|
Lehmann & Voss LUVOCOM® 50-7586 Polycarbonate, with carbon fiber
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts with low warpage and..
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | |
|
Lehmann & Voss LUVOCOM® 1105-0706 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | Tangent at 0.05 in/min; ASTM D790A |
|
LyondellBasell Higlass BJ44A Polypropylene Copolymer, 45% Glass Fiber
Key Features: medium melt flow, high modulus, chemically coupled, glass fiber-reinforced polypropylene copolymer, high stiffness, good impact strength, excellent processabilityApplications: grille o..
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
|
Solvay TECHNYL® R AR 218 V30 Nylon 66, 30% glass fiber, DRY
Description: TECHNYL® AR 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. It contains recycled materials. This product is available in black ..
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK (Asia Pacific)
LNP* Thermocomp* LF003 is a compound based on Polyetheretherketone resin containing Glass Fiber.
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Asia Pacific)
LNP* Thermocomp* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features of this material include: Easy Molding.
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP LF004E PEEK (Europe-Africa-Middle East)
LNP* THERMOCOMP* LF004E is a compound based on Polyetheretherketone resin containing Glass Fiber. Added features include: Easy Molding.
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP UF004AS PPA (Europe-Africa-Middle East)
LNP* Thermocomp* UF004AS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL CTI2550 PPE+HIPS (Europe-Africa-Middle East)
NORYL CTI2550 is a glass/mineral filled material with a Vicat B/120 of 160 °C according ISO 306.
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | ASTM D790 |
|
Plenco 7500 Phenolic, Granular, Injection Molded
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi..
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
|
Polyram RamTal PM3007G5 Polyacetal for Injection Molding, 25% Glass Fiber Reinforced
25% Glass fiber reinforced polyacetal for injection molding applications.Information provided by Polyram.
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | ASTM-D790 |
|
Polyram RamTough RZ300G6 Polycarbonate, 30% Glass Fiber
30% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | D790 |
|
Zhejiang Juner 302-G30 30% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
|
Polyram RamLloy PFS301G6 ASA/PBT Alloy, 30% Glass Fiber
30% Glass fiber reinforced ASA/PBT alloy for injection molding applications.Information provided by Polyram.
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | cond; ISO 178 |
|
DSM Stanyl® TE200F8 PA46-GF40
40% Glass Reinforced, Heat Stabilized, for E&E applications
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | 50%RH; ISO 178 |
|
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
|
|||
| Flexural Modulus | >= 7.00 GPa | >= 1020 ksi | IEC 1212-2 5.2 |
|
Hippe PF CC 203 Woven Cotton Cloth Reinforced Phenolic Resin - Sheet
Used in mechanical applications (fine weave: =130 g/m2, >30 threads/cm). Recommended for small parts. Better mechanical properties and poorer electrical properties than type PF CC 204.Information ..
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
|
Eurostar Starflam PF0047E PA6, 20% Glass Filled, Injection Molded
Starflam PF0047E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as EXCP4009)Information provided by Polymer Tech..
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | DAM; ISO 178 |
|
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66
(Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa..
|
|||
| Flexural Modulus |
7.00
GPa @Temperature 65.0 °C |
1020
ksi @Temperature 149 °F |
ASTM Test |
|
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Dry)
Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio..
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
|
Ascend Performance Materials Vydyne® R535 Nylon 66, 35% Glass Reinforced, Conditioned
Vydyne® R535 is general-purpose, hydrolysis-resistant, 35% glass-fiber reinforced PA66 resin. This product is lubricated for improved flow and offers superior surface appearance. Glass-reinforced V..
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | ASTM D790 |
|
Beijing Ranger Chem PBT-201-G20 272 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | ASTM D790 |
|
A. Schulman ComAlloy Hiloy® 242 SAN, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | 50%RH; ISO 178 |
|
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers
|
|||
| Flexural Modulus | 7.00 GPa | 1020 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC (Asia Pacific)
LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated.
|
|||