| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178, ASTM D790 |
|
Nilit Nilamid A G5 FR PH2 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous)
Description: Nilamid A G5 FR PH2 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim..
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178 |
|
Nilit FRIANYL B63 GV30 Nylon 6 for injection molding, 30% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Modulus | 7.20 - 27.6 GPa | 1040 - 4000 ksi | Average value: 14.0 GPa Grade Count:45 |
|
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP RX05050 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RX05050 is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As..
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66
LNP LUBRILOY* RF206 is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant, Added features of this material includes: Wear Resistant.
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Valox® K4560 PBT (Europe-Africa-Middle East)
30% glass reinforced PBT. Impact modified, high flow, hydrolytically stable.
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP DF006ER PC (Europe-Africa-Middle East)
LNP* Thermocomp* DF006ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific)
DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility.
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | 2mm/min; ISO 178 |
|
Teijin Panlite® BN-8110R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin
CF 10% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona..
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP WFB44 PBT (Europe-Africa-Middle East)
LNP* Thermocomp* WFB44 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Glass Bead.
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178 |
|
Solvay TECHNYL® AR 218 V25 Nylon 66, 25% glass fiber, DRY
Description: Polyamide PA66 reinforced with 25% of glass fiber, heat stabilized, containing recycled material.Available in: Europe and North AmericaProduct Applications: TECHNYL® AR 218 V25 BLACK..
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP Thermocomp EF006R PEI (Europe-Africa-Middle East)
LNP* Thermocomp* EF006R is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Mold Release.This data was supplied by SABIC-IP for the Europe-A..
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East)
Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
|
Plenco 7507 Phenolic, Granular, Injection Molded
PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut..
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178-93 |
|
Wellman EcoLon® MR1660-BK1 Nylon 66, 40% Mineral Reinforced
All information provided by Wellman Engineered Resins.
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | ISO 178-93 |
|
Wellman Wellamid® MRGF30/10 42H-GY1 Nylon 6, 30% Mineral and 10% Glass Reinforced
All information provided by Wellman Engineered Resins.
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | DIN 52457 |
|
CP-Polymer-Technik Wellamid® 6000 MRGV 25/15 HWCP 25% Mineral and 15% Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
|
E-Polymers Tekaloy® G70GR , 30% Glass Reinforced PC/ABS Alloy
30% Glass Fiber reinforced, High stiffness, Dimensional stabilityInformation provided by E-Polymers Co. Ltd.
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
|
E-Polymers TEKAMID® TA210M40 , 40% Mineral Filled PA66, DAM
40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd.
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | DIN 52457 |
|
CP-Polymer-Technik Wellamid® 6000 MRGV 25/15 HWUVCP 25% Mineral and 15% Glass Fiber Nylon 6, UV Stabilized, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | After conditioning at 23°C and 50% RH; ISO 178 |
|
Arkema Group Orgalloy® RS 6630 Polyamide 6.6 Alloy 30% Glass Fiber reinforced
Polyamide Alloy, Rigid grade, Nylon 6.6 basedMolding of Engineering PartsInformation provided by Arkema Group
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | ISO Data |
|
BASF Ultramid® 8267G HS BK-102 15/25% Glass/Mineral Filled PA6 (Dry)
Ultramid 8267G HS BK-102 is a heat stabilized, black pigmented, 40% mineral and glass fiber reinforced nylon 6 injection molding compound. It possesses a balance of engineering properties in combin..
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | ISO Data |
|
BASF Ultramid® 8333G HI 33% Glass Filled PA6 (Dry)
Ultramid 8333G HI is a 14% glass reinforced, impact modified PA6 injection molding compound developed for applications requiring improved dry as molded toughness in combination with a
balance of st..
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
|
Ashley Polymers Ashlene® 630-33GU Nylon 6, 33% Glass Reinforced
Nylon 6, 33% glass reinforced resin, utility grade. Also available: 630S - 33GU Heat Stabilized, 630 - 33GBU Black, 630S - 33GBU Black with H.S.Data provided by the manufacturer
|
|||
| Flexural Modulus | 7.20 GPa | 1040 ksi | ASTM D790 |
|
Ashley Polymers Ashlene® 266 PPO, 30% Glass Reinforced
A general purpose, 30% glass reinforced PPO resin for injection molding applications.Data provided by the manufacturer
|
|||
| Flexural Modulus |
7.20
GPa <br>@Temperature 23.0 °C
|
1040
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F..
|
|||