| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 7.97 GPa | 1160 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN
LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati..
|
|||
| Flexural Modulus | 7.97 GPa | 1160 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA 11 (Asia Pacific)
LNP* THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing Glass Fiber.
|
|||
| Flexural Modulus | 7.97 GPa | 1160 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP PF006 PA 6
LNP THERMOCOMP* PF006 is a compound based on Nylon 6 resin containing 30% Glass Fiber.
|
|||
| Flexural Modulus | 7.97 GPa | 1160 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP HF008 PA11
LNP THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing 40% Glass Fiber.
|
|||
| Flexural Modulus | 7.97 GPa | 1160 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6
LNP THERMOCOMP* PF006S is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Flexural Modulus | 7.97 GPa | 1160 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP PF006U PA 6
LNP THERMOCOMP* PF006U is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added features of thie grade are: UV Stabilized.
|
|||