| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 5.50 GPa | 798 ksi | |
|
Plastcom SLOVAMID 6 GF 10 FRA 5 PA6, 10% glass fibre, flame retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 10% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | |
|
Plastcom SLOVAMID 66 GF 10 PA66, 10% glass fibre
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | STN EN ISO 178 |
|
Plastcom SLOVAMID 66 GF 15 Polyamide 66, 15% Glass Fiber
FeaturesChemically reinforced with 15% glass fiber, suitable for mouldings with high strength and toughness also at low temperatures. Used in the automotive, engineering and electrical industry. W..
|
|||
| Flexural Modulus |
5.50
GPa <br>@Temperature 90.0 °C
|
798
ksi <br>@Temperature 194 °F
|
ISO 178, ASTM D790 |
|
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It ..
|
|||
| Flexural Modulus |
5.50
GPa <br>@Temperature 23.0 °C
|
798
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Polykemi AB POLYshine PBT D221 QF30 PBT, Glass and Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Modulus |
5.50
GPa <br>@Temperature 23.0 °C
|
798
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Polykemi AB SCANTEC PC S75R GF20 Polycarbonate, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ASTM D790 |
|
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, at 50% RH
(disc
AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer..
|
|||
| Flexural Modulus |
5.50
GPa <br>@Temperature 23.0 °C
|
798
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Polykemi AB SCANMID 6 B12^ Q40 Nylon 6, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Modulus |
5.50
GPa <br>@Temperature 90.0 °C
|
798
ksi <br>@Temperature 194 °F
|
ISO 178, ASTM D790 |
|
Nilit Nilamid A3 H7 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H7 G6 is a 30% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® 3412ECR PC (Europe-Africa-Middle East)
Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v..
|
|||
| Flexural Modulus | 5.50 - 24.0 GPa | 798 - 3480 ksi | Average value: 14.9 GPa Grade Count:24 |
|
Overview of materials for Polyarylamide, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ASTM D790 |
|
Loxim 330 12HSL Nylon 6
Information provided by Loxim Industries
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ISO 178 |
|
Mitsubishi Xantar® G4F 25 UR Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM 2312EPR PEI
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP LUBRILOY RF203H PA 66
LNP LUBRILOY* RF203H is a compound based on Nylon 66 resin containing 15% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare.
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP DF004ER PC (Europe-Africa-Middle East)
LNP* Thermocomp* DF004ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP JF003XXZ PES
LNP* THERMOCOMP* JF003XXZ is a compound based on Polyethersulfone resin containing 15% Glass Fiber.
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP JF003XXZ PES (Asia Pacific)
LNP* Thermocomp* JF003XXZ is a compound based on Polyethersulfone resin containing Glass Fiber.
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ISO Data |
|
Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Conditioned)
Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | |
|
Shandong Guangyin 1212 Reinforced Nylon
Features and Applications: Wear resistance, higher strength, better tenacity, strong adhesion and better low temperature resistance. It is applicable to surface coating of wires, cables, optical cab..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS
Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ASTM-D790 |
|
Polyram PlusTek PA870G33 Nylon 6.6, 33% Glass Fiber
33% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | D790 |
|
Zhejiang Juner 302-G10 10% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode
Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, ..
|
|||
| Flexural Modulus |
5.50
GPa <br>@Temperature 160 °C
|
798
ksi <br>@Temperature 320 °F
|
ISO 178 |
|
DSM Stanyl® TS250F8 PA46-GF40 FR
40% Glass Reinforced, Flame Retardant, Heat Stabilized
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ASTM D790 |
|
Ascend Performance Materials VYDYNE® R513 Nylon, 13% Glass Reinforced
Typical property data. VYDYNE is a registered trademark of Solutia Inc.
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® 3412ECR PC
Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® 3412ECR PC (Asia Pacific)
Lexan* 3412ECR Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V0 rating and is available in v..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ISO Data |
|
BASF Ultradur B 4040 G3 HT BK5830 15% Glass Filled PBT/PET
Ultradur B 4040 G3 HT BK5830 is a 15% glass filled, pigmented black, injection molding PBT. It is a resin for molding household appliances and equipment which must be resistant to chemicals and oth..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ASTM D790 |
|
PolyOne Lubri-Tech™ ES-20GF/08T Polyethersulfone - 20% Glass Fiber And PTFE
(discontinued **)
Data provided by PolyOne.
|
|||