| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 9.00 GPa | 1310 ksi | ASTM D790 |
|
PolyOne Nymax™ ND633 GF Black Polyamide 6 (Nylon 6)
The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | ASTM D790 |
|
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | ISO 178 |
|
Nilit FRIANYL B63 KF50 Nylon 6 for injection molding, 50% short glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics EXTEM XH2315 TPI Resin
Extem XH2315 Resin
|
|||
| Flexural Modulus |
9.00
GPa @Temperature 23.0 °C |
1310
ksi @Temperature 73.4 °F |
DAM; ISO 178 |
|
DuPont Performance Polymers Zytel® HTN 54G35HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**)
Zytel® HTN54G35HSLR NC010 is a 35% glass reinforced, toughened, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polym..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | |
|
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | |
|
Lehmann & Voss LUVOCOM® 1106-7843 Polyether imide, with glass fiber, PTFE, lubricant modified, easy flowing
Applications: Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Information provided by Lehmann & Voss & Co.KG
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | |
|
Lehmann & Voss LUVOCOM® 1-8491 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | |
|
Lehmann & Voss LUVOCOM® 19-8094 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | |
|
Lehmann & Voss LUVOCOM® 1104-7452 Polyether ketone, with glass fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | |
|
Lehmann & Voss LUVOCOM® 1105/GF/30/BK-1 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | |
|
Lehmann & Voss LUVOCOM® 1105-0779/WT PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High chemical resistance parts, hydrolysis resistance, non flammable.H..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | |
|
Lehmann & Voss LUVOCOM® 1105-0918/EM/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | |
|
Lehmann & Voss LUVOCOM® 1105-8402 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | ISO 178 |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | ASTM D790 |
|
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP STAT-KON RE0029 PA 66
LNP* STAT-KON* RE0029 is a compound based on Nylon 66 resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP SF008 PA 12
LNP* THERMOCOMP* SF008 is a compound based on Nylon 12 resin containing 40% Glass Fiber.
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | ISO 178 |
|
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/BJ356MO
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | 2 mm/min; ISO 178 |
|
Eurostar Staramide RF006SXS PA66, 30% Glass Fiber Filled, Injection Molded
Staramide RF006SXS is a 30% Glass Fiber Reinforced Polyamide 66 Injection Molding Resin (also known as RF1006HS)Information provided by Eurostar.
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | ISO 178 |
|
Eurotec® Tecomid® NA40 GR30 NL RM PA 6.6 30% glass fiber reinforced, low friction and wear
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | ASTM D790 |
|
Adell ER-19 Polypropylene Homopolymer; 43% Glass Reinforced, High Stiffness
Data provided by Adell Plastics, Inc.
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | ASTM D790 |
|
Ashley Polymers Ashlene® 528L-33G Nylon 66, 33% Glass Reinforced
General purpose glass fiber reinforced Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufactur..
|
|||
| Flexural Modulus | 9.00 - 12.0 GPa | 1310 - 1740 ksi | ISO 178 |
|
Bulk Molding Compounds tetra-DUR N 4111 Bulk Molding Compound
Smooth, high gloss surface. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion..
|
|||
| Flexural Modulus | 9.00 GPa | 1310 ksi | ASTM D790 |
|
Sumitomo Bakelite North America RX® 1-501AN Mineral Filled Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ..
|
|||
| Flexural Modulus | 9.00 - 12.0 GPa | 1310 - 1740 ksi | ISO 178 |
|
Bulk Molding Compounds tetra-DUR F 4206 Bulk Molding Compound
General purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), ther..
|
|||