Polymer Property : Modulus of Rupture = 0.783 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00540 GPa

@Temperature 110 °C
0.783 ksi

@Temperature 230 °F
Pyrotek Pyrocast 92AC Tabular Alumina Based Low Cement Castable
Pyrocast 92AC is a tabular alumina based low cement castable, enhanced with non-wetting matrix. The silica-free matrix eliminates the potential for aluminum attack on silica with in the bonding mat..