| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tear Strength | 35.0 kN/m | 200 pli | ASTM D624 |
|
Multibase Multi-Flex® TPE A 8102 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | ISO 34-1 |
|
PolyOne OnFlex™ S HF 80A-3S1986 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | ASTM D624 |
|
PolyOne Dynaflex™ G7431-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7431-1001-00 is an easy processing, performance TPE designed for use in applications requiring a tough, durable material with a low coefficient of friction. - Excellent Heat Stability - ..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die C, 510 mm/min; ASTM D624 |
|
PolyOne Geon™ Vinyl Flexible R5155A White 759 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die C, 510 mm/min; ASTM D624 |
|
PolyOne Geon™ Vinyl Flexible SL60 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die C, 510 mm/min; ASTM D624 |
|
PolyOne Geon™ Vinyl Flexible R5160A Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die C, 510 mm/min; ASTM D624 |
|
PolyOne Geon™ Vinyl Flexible R5257A White 759 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die C |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 4.0 PHR MBTS
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
|
|||
| Tear Strength | >= 35.0 kN/m | >= 200 pli | DIN 53507 |
|
Huntsman AVALON® 75 ABX Thermoplastic Polyurethane
Introduction: AVALON 70 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 70 ABX is part of the AVALON Perform Range and offers a specially designed,..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die B |
|
Momentive Performance Materials Addisilâ„¢ 440 E Healthcare Extrusion Grade Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die B |
|
Momentive Performance Materials Siloprenâ„¢ LSR 2660 ZKS Custom Liquid Silicone Rubber - Automotive
This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die B |
|
Momentive Performance Materials Siloprenâ„¢ LSR 2715/50 Liquid Silicone Rubber - Self-Bonding / Self-Lubricating
This LSR elastomer is a self-bonding, self-lubricating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at e..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die B |
|
Momentive Performance Materials Siloprenâ„¢ LSR 2742 Liquid Silicone Rubber - Self-Bonding
This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die B |
|
Momentive Performance Materials Siloprenâ„¢ LSR 2760 Liquid Silicone Rubber - Self-Bonding
This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die B |
|
Momentive Performance Materials Silplusâ„¢ 40 HS High Strength Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
|
|||
| Tear Strength | >= 35.0 kN/m | >= 200 pli | DIN 53507 |
|
Karina E 65/200 Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die B |
|
Momentive Performance Materials Addisilâ„¢ 1040 E Industrial Extrusion Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die B |
|
Momentive Performance Materials Addisilâ„¢ 442 E Healthcare Extrusion Grade Heat Cured Rubber
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
|
|||
| Tear Strength | <= 35.0 kN/m | <= 200 pli | |
|
TSE Industries Millathane® 28 Millable Polyester Polyurethane Rubber
Millathane 28 has excellent resistance to gas (e.g., nitrogen) permeability as well as very good abrasion resistance and low temperature properties. This polyurethane rubber was designed for automot..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die C |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Talc-Mistron Vapor
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die C |
|
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR MBT
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | with incision; ISO 34B |
|
Lubrizol ESTANE® GP70AE Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Die C |
|
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Black Peroxide Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | Method C; ISO 34 |
|
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Injection Molding, Natural
Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | warp |
|
3M FG7-22 FB-700 Filter Bag Fabric
3M has developed a line of advanced textiles for manufacturing high temperature filter bags which can be used at temperatures up to 700°F (371°C), or for those even higher temperature applications..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | |
|
Trelleborg B643 High Quality Nitrile Rubber
Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi..
|
|||
| Tear Strength | 35.0 kN/m | 200 pli | DIN ISO 34-1/Bb |
|
BASF Elastollan S 60 AWH TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
|
|||