Polymer Property : Vicat Softening Point = 120 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Vicat Softening Point 120 °C
248 °F
B
Plastcom SLOVALEN PQ 83 T 15 PP, 15% mineral filling, UV stabilization
FeaturesModified PP for injection moulding with the content of 15% mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased ..
Vicat Softening Point 120 °C

@Load 5.001 kg
248 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYblend 65H PC/ABS-Blend
Information provided by Polykemi AB
Vicat Softening Point 120 °C

@Load 1.00 kg,
Thickness 4.00 mm
248 °F

@Load 2.20 lb,
Thickness 0.157 in
ISO 306
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer  (discontinued **)
Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P..
Vicat Softening Point 120 °C
248 °F
ASTM D1525
Ineos K38-20-160 Polyethylene Copolymer
K38-20-160 is a medium density polyethylene copolymer containing an organic yellow pigment system, designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stres..
Vicat Softening Point 120 °C
248 °F
ASTM D1525
Ineos TUB 172 HDPE
TUB 172 is a yellow medium density polyethylene copolymer designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stress life and slow crack growth resistance. T..
Vicat Softening Point 120 °C

@Load 5.00 kg
248 °F

@Load 11.0 lb
50°C/h; ASTM D1525
LG Chemical XR474F ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Exterior Housing (Lamp Housing Etc)CAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical
Vicat Softening Point 120 °C
248 °F
ASTM D1525
Iran Petrochemical (PCC) 52528 High Density Polyethylene
52528 is a HDPE copolymer injection molding grade for thin walled applications requiring a good balance between high flowability and physical properties.Application: caps, thin walled, injection mol..
Vicat Softening Point 120 °C
248 °F
Rate A/50; ISO 306
SABIC Innovative Plastics NORYL SE100 PPE+HIPS (Europe-Africa-Middle East)
NORYL® SE100 is an unfilled, flame retardant material with a Vicat B/120 of 120°C. It has a UL-94 flammability rating V1 @ 1.47 mm, and is halogen free according to VDE/DIN 472 part 815.
Vicat Softening Point 120 °C
248 °F
Rate A/50; ISO 306
SABIC Innovative Plastics NORYL V03505 PPE+HIPS
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Vicat Softening Point 120 °C
248 °F
Rate A/50; ISO 306
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific)
Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Vicat Softening Point 120 °C
248 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC
Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
Vicat Softening Point 120 °C
248 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific)
Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 120 °C
248 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East)
Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Vicat Softening Point 120 °C

@Load 5.10 kg
248 °F

@Load 11.2 lb
50°C/h; ISO 306
Styrolution Luran® HH-120 Alpha-Methylstyrene Acrylonitrile
Luran HH-120 is a grade of AMSAN with high heat resistance and improved mechanical strength. It is suitable for injection molding and extrusion applications and can be used as a modifier for high he..
Vicat Softening Point 120 °C
248 °F
VST/A/50; ISO 306
Styrolution Luran® S KR 2858 GS Colored 15% Glass Filled ASA
Description: Glass-reinforced grade with high stiffness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Vicat Softening Point 120 °C
248 °F
B/120; ISO R306
Samsung Cheil Industries Infino® HA-1011 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Vicat Softening Point 120 °C
248 °F
B/50; ISO R306
Samsung Cheil Industries Infino® WP-1098 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Vicat Softening Point 120 °C
248 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL IN120 PPE+HIPS (Europe-Africa-Middle East)
NORYL IN120 is an unfilled material with a Vicat B/120 of 125 °C according ISO 306. NORYL IN120 has been developed for the interior automotive
Vicat Softening Point <= 120 °C
<= 248 °F
Sibur Discar-SL PC/ABS Compositional Polymer
Composition material PC/ABS with low viscosity of melting with high shock resistance, thermal and atmospheric resistance for large, thin wall structural parts of automobile interiors.
Vicat Softening Point 120 °C
248 °F
ASTM-D1525
Polyram RamLloy PBB701 PC/ABS alloy, UV Stabilized
UV stabilized PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind.
Vicat Softening Point 120 °C

@Load 5.00 kg
248 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTAPROP 0540 GFC V0 Flame Retardant Polypropylene, 20% Glass Filled
PP with 20% chemically coupled glass fiberFlame retardant class V0, excellent mechanical characteristics, excellent heat resistanceInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 120 °C

@Load 5.10 kg
248 °F

@Load 11.2 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTAPROP 1540 GFC V0 H Flame Retardant Polypropylene, 20% Glass Filled
PP with 20% glass fiber reinforcedFlame retardant class UL V0 and class M2 according to NL P92-507Information provided by Cossa Polimeri S.r.l.
Vicat Softening Point 120 °C

@Load 5.00 kg
248 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTAPROP H 0560 GF Polypropylene, 30% Glass Filled
PP homopolymer 30% glass fiber reinforcedGood physical and mechanical characteristicsInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 120 °C
248 °F
Loading 1, Rate A; ASTM D-1525
Chevron Phillips Marlex® HMN TR-942/942G Polyethylene; HDPE
High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and fair flowLong-term UV stabilizationExcellent impact stren..
Vicat Softening Point 120 °C

@Load 5.10 kg
248 °F

@Load 11.2 lb
ISO 306
Eurotec® Tecotek® BC40 UF65 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, standard grade
Information provided by Eurotec®
Vicat Softening Point 120 °C
248 °F
Arkema Group Orevac® 18732 RBP Maleic Anhydride modified Polypropylene
PP base Structure: Repairing and joint Applications: Pipe CoatingInformation provided by Arkema Group
Vicat Softening Point 120 °C
248 °F
ASTM D1525
C.O.I.M. LARIPUR® LPR5850 Modified Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Vicat Softening Point 120 °C

@Load 5.10 kg
248 °F

@Load 11.2 lb
ISO 306
Azoty Tarnow™ Tarnamid® T-27 MTR Polyamide 6 - Transparent
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Transparent up to maximum 2.5 mm.Tarnamid® has the following main properties..
Vicat Softening Point 120 °C
248 °F
Method B; ASTM D-1525
Bhansali Engineering Abstron IMGS20 Glass Reinforced Grade
Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali
Vicat Softening Point 120 °C
248 °F
VST/B/50; ISO 306
Styrolution Luran® S KR 2861/1 C Colored ASA+PC
Description: Grade with high heat resistance for injection molding and extrusion.Applications: Interior and exterior automotive parts, and electrical housings.Information provided by STYROLUTION, wh..