| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point |
126
°C @Load 1.00 kg |
259
°F @Load 2.20 lb |
ISO 306/A |
|
Polimeri Europa Eraclene® MM 74 U High Density Polyethylene - Injection Molding
Eraclene MM 74 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution. The polym..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | Rate B/50; ASTM D1525 |
|
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Asia Pacific)
UV stabilized, non-FR PC/ABS of excellent flow and impact performance
|
|||
| Vicat Softening Point | 126 °C | 259 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS
PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Americas region.
|
|||
| Vicat Softening Point |
126
°C @Load 1.00 kg |
259
°F @Load 2.20 lb |
ISO 306/A |
|
Polimeri Europa Eraclene® MS 80 High Density Polyethylene - Injection Molding
Eraclene MS 80 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MS 80 shows a good balance between processability and mechanical pro..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | ASTM D1525 |
|
Chevron Phillips HiD® 9398T HDPE Natural Pipe Resin
(discontinued **)
Resin Type: Linear Copolymer; ASTM D 3350 Classification: 345420A; ASTM D 4976 Classification: PE 235, A 56601Applications:Base Resin for use in Utility and Conduit Pipe ApplicationsData provided by..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | ASTM D1525 |
|
Chevron Phillips HiD® 9412/HiD® 9413 with Antistat HDPE Blow Molding Resin
(discontinued **)
Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | ASTM D1525 |
|
Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **)
Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | ASTM D1525 |
|
Braskem BS 002 HDPE Blow Molding Polyethylene
(discontinued **)
Applications: Bottles for medicines, cleaning products, cosmetics, food products and surface-active agents. Information provided by Braskem
|
|||
| Vicat Softening Point | 126 °C | 259 °F | ASTM D1525 |
|
LyondellBasell Alathon® M6138 High Density Polyethylene
ApplicationsALATHON M 6138, formerly known as XM 6138, is a high density polyethylene resin for use in injection molding applications. This resin exhibits good impact resistance and high stiffness...
|
|||
| Vicat Softening Point | 126 °C | 259 °F | ASTM D1525 |
|
LyondellBasell Petrothene® LR732001 High Density Polyethylene (Sheet & Profile Grade)
ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Regulatory StatusThe base resin LR 7320 meets t..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | ASTM D1525 |
|
Ineos K44-15-122 HDPE
K44-15-122 is a natural high density polyethylene copolymer designed specifically for extrusion of pipe. It has NSF Standard 14 certification for potable water applications, complies with ANSI/NSF S..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | ASTM D1525 |
|
Ineos TUB 121NTW HDPE
TUB121 NTW is a natural high density bimodal polyethylene copolymer designed for extrusion of large diameter, thick wall piping for potable water, industrial and mining applications. When blended wi..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | ASTM D1525 |
|
LG Chemical SEETEC PF150 HDPE
Features: Characteristics: Good impact & tear strength, High speed & superior heat sealing propertiesAdditives: Anti-oxidants, LubricantsApplication: Shopping bags, Thin films, Trash bags, Multiwall..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | ASTM D1525 |
|
Micropol Isoplas P381 Crosslinkable Polyethylene
Information provided by Micropol Limited
|
|||
| Vicat Softening Point | 126 °C | 259 °F | resin; ASTM D1525 |
|
Lotte Chemical Titan TITANZEX® HI1100 High density polyethylene
HI1100 is a non UV stabilised high density polyethylene for injection molding. HI1100 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 ..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | ASTM D1525 |
|
LyondellBasell Petrothene® LP510300 High Density Polyethylene
ApplicationsPETROTHENE LLP 5103-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good drawdown. It is r..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | ASTM D1525 |
|
Solvay Specialty Polymers Polidan® PNT 0555/06 Polyethylene, Crosslinked (XLPE)
POLIDAN® PNT 0555/06 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes...
|
|||
| Vicat Softening Point | 126 °C | 259 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER (Europe-Africa-Middle East)
Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | Rate B/50; ASTM D1525 |
|
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Asia Pacific)
PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Europe-Africa-Middle East)
PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | B/50; ISO R306 |
|
Samsung Cheil Industries Infino® NH-1035 PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
|
|||
| Vicat Softening Point | 126 °C | 259 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Xenoy® XD1607 PBT+PC (Europe-Africa-Middle East)
22% Glass filled PBT+PC with a designed balance between surface appearance and mechanical properties sufficient for automotive doorhandle requirements. Special suitable for gas assist mouldings .Thi..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Xylex X7529 PC+POLYESTER (Europe-Africa-Middle East)
PC+ POLYESTER unreinforced alloy developed for optical or lense market. Good flow with good impact and excellent optical quality. UV 400nm block.This data was supplied by SABIC-IP for the Europe-Afr..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | A (10N); ISO 306 |
|
Borealis Daplen™ EE115T TPO Compound
Daplen EE115T is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE115T is a material with excellent impact /stiffness ratio. Thanks to its low th..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | ASTM D1525 |
|
ExxonMobil HDPE BA53-055 High Density Polyethylene Resin
Product Description: BA53-055 is a high molecular weight, high density polyethylene copolymer.Availability: Latin America, North America and South America Additive: Antistatic: NoApplications: Dru..
|
|||
| Vicat Softening Point |
126
°C @Load 1.02 kg |
259
°F @Load 2.25 lb |
ASTM-D1525 |
|
Braskem GM7746CA HDPE Blow Molding Polyethylene
GM7746CA is a high-density polyethylene specially developed for the manufacturing of blow molding fuel tanks. It has high molar mass and excellent mechanical properties. It also shows excellent tena..
|
|||
| Vicat Softening Point |
126
°C @Load 0.999 kg |
259
°F @Load 2.20 lb |
ISO 306 |
|
Arkema Group OREVAC® 18760 Grafted Maleic Anhydride Polypropylene
OREVAC 18760 is a maleic anhydride grafted polypropylene used in the manufacturing of three layer PP coating for steel pipeline. OREVAC 18760 is also used in multilayer EVOH – PP structures. OREVAC..
|
|||
| Vicat Softening Point | 126 °C | 259 °F | ASTM D1525 |
|
NOVA Chemicals Sclair® 59D HDPE Blow Molding Resin
(discontinued **)
Features: High impact resistance, good stiffness, moderate ESCR.Applications: Food packaging, small parts (HIC), oil bottles.Data provided by the manufacturer.
|
|||
| Vicat Softening Point | 126 °C | 259 °F | A50; ISO 306 |
|
Breplast Bretene SPF Thermoplastic Composite, 40% PP + 60% PE
Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A.
|
|||