| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 90.0 °C | 194 °F | ASTM D-1525 |
|
Plaskolite West Optix® CA - 41 UVT LL General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | B |
|
Plastcom SLOVALEN PC 81 T 30 PP, 30% mineral filling
FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | 10 N - 50°C/h; ISO 306/A |
|
Polimeri Europa Edistir SR 550 Polystyrene
High impact, easy flow polystyrene with good elasticity at low temperatures.Suitable for injection moulding of large or complex parts with low thickness and high impact strength.
Designation: Thermo..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | Rate B/50; ASTM D1525 |
|
SABIC Innovative Plastics Cycolac® FR23 ABS (Asia Pacific)
Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated.
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | ISO 306/B50 |
|
Premix Thermoplastics PRE-ELEC® PP 1398 Conductive Thermoplastic Compound
PRE-ELEC® PP 1398 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Asia Pacific)
Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics GELOY CR7020 ASA (Europe-Africa-Middle East)
GELOY CR7020 is a profile extrusion and co-extrusion grade, blend of ASA/SAN. In co-extrusion it can be used over CYCOLAC, PVC or other compatible polymers.
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics GELOY CR7520 ASA
General purpose ASA. Excellent weatherability, good flow/aesthetics and high impact. Rated F2 by UL.
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
|
Eastman D4044A Polyethylene
(discontinued **)
D4044-A is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on automatic molding equipme..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
|
Eastman Voridian E6838-010A Polyethylene
(discontinued **)
Voridian polyethylene E6838-010A is a low density formulation with medium slip used for injection molding. It is an outstanding material for molding lids and other container closures because it pro..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
|
LyondellBasell Petrothene® NA951000 Low Density Polyethylene
ApplicationsPETROTHENE NA 951 is a series of homopolymer resins specially designed for industrial and consumer packaging and liner and bag applications. NA 951 has an excellent balance of processab..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | molding; ASTM D1525 |
|
LyondellBasell Petrothene® NA967000 Low Density Polyethylene, Film Extrusion Grade
Petrothene NA967000 is a low density polyethylene resin designed for blown film, general purpose and industrial packaging applications. NA967000 exhibits good processing characteristics and impact s..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | B120; ISO 306 |
|
Inno-Comp INNOPOL® CS 1-5120 BLH 20% Talc-Filled Polypropylene Homopolymer
INNOPOL® CS 1-5120 BLH is a 20% talc-filled polypropylene homopolymer compound /PP-H TD20 (ISO 1043)/.INNOPOL® CS 1-5120 BLH is recommended especially for producing products, where high stiffn..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | B/50; ISO R306 |
|
Samsung Cheil Industries Starex® NT-7310 ABS, Unreinforced FR
Flame-retardant ABS that can be used in printer frames etc.Information provided by Samsung Cheil Industries.
|
|||
| Vicat Softening Point |
90.0
°C <br>@Load 5.10 kg
|
194
°F <br>@Load 11.2 lb
|
120°C/h; ASTM D 1525 |
|
Styrolution PS 485N HIPS
Styrolution PS 485N is a high impact grade of polystyrene for extruded sheets with a matte surface.Matte SurfaceUL 94 HBInformation provided by Styrolution
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | Unannealed; ISO R 306 |
|
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS
VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | B/50; ISO R306 |
|
Samsung Cheil Industries Starex® SF-0505HWR MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Noryl HIPS3191 PS
This data was supplied by SABIC-IP for the Americas region.
|
|||
| Vicat Softening Point |
90.0
°C <br>@Load 1.02 kg,<br> Temperature 120 °C
|
194
°F <br>@Load 2.25 lb,<br> Temperature 248 °F
|
ASTM D1525 |
|
Styrolution Styrolux® GH 58 SBC
Description: Styrolux® GH 58 is a high flow thermoplastic styrene-butadiene block copolymer with excellent mold release properties. It has crystal clarity, good toughness, good stiffness and warp..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
|
UBE F522 Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..
|
|||
| Vicat Softening Point |
90.0
°C <br>@Load 5.10 kg
|
194
°F <br>@Load 11.2 lb
|
50°C per hour; ISO 306B50 |
|
Total PS CPDS FT875 Flame Retardant Polystyrene
POLYSTYRENE (PS) COMPOUND (CPDS) FT875 is a high impact, halogen free flame retardant polystyrene. PS CPDS FT875 offers high heat stability and is recommended for the manufacturing of articles whic..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | B50 (50N); ISO 306 |
|
Domo 1104K Polypropylene Homopolymer
Information provided by Domo.
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | |
|
Dow LDPE 4012M Low Density Polyethylene
DOW LDPE 4012M resin is a broad molecular weight distribution homopolymer designed to provide good impact strength, excellent flexibility and high stress crack resistance for housewares, toys and ge..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
|
Huntsman PE2030 Injection Molding Polyethylene
(discontinued **)
Homopolymer, Drug Master File listed product, and FDA compliant.Features: High mechanical flexing properties, excellent processability, good stress crack resistance, and very good low temperature st..
|
|||
| Vicat Softening Point | 90.0 - 105 °C | 194 - 221 °F | Rate A (50°C/h), Loading 2 (50 N); ASTM D1525 |
|
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**)
Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
|
Plaskolite West Optix® CA-41 General Purpose Acrylic Resin
Injection Molding Grade Pellets only. Lowest Heat Resistance and maximum flow.
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | 120°C/hr, 9.8N; ASTM D1525 |
|
Lubrizol Estane® 2103-90AENH Film Grade Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: NSF Standard 61 Certified, FDA ComplianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane prod..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
|
Huntsman PE1345 EVA Film Extrusion
(discontinued **)
3.4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
|
Huntsman PE1403 EVA Film Extrusion
(discontinued **)
4% Vinyl Acetate EVA Copolymer, DMF listed and FDA compliantFeatures: High clarity film with good toughness and flexibility at low temperatures.Applications: Film extrusion: frozen food and general ..
|
|||
| Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
|
Samyang Triel® 5302FR Thermoplastics Polyetherester Elastomer, Non-Halogen Flame Retardancy
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5302FR is a non-halogen, flame retardant grade.Information provided by Samyang.
|
|||