| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 97.0 °C | 207 °F | Rate B/50; ASTM D1525 |
|
SABIC Innovative Plastics Cycoloy® CM6240 PC+ABS (Asia Pacific)
CYCOLOY CM6240 resin is a flame retardant PC/ABS blend featuring balanced properties of high modulus, good flow and ductility. It is of Br- & Cl-free flame retardant systems intended to meet thin wa..
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | ASTM D1525 |
|
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film
The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng..
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | ASTM D1525 |
|
Resirene Resirene® 6420 Super High Impact Polystyrene
Features:Super High ImpactEasy ProcessingLow ModulusFlexibilityFDA Rating: 21 CFR 177.1640Applications:ExtrusionDeep ThermoformingGPPS/HIPS BlendsPoint of Purchase DisplaysInformation provided by US..
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | ASTM D1525 |
|
Ineos Nova Zylar® 390 Clear Impact Modified Acrylic Copolymer
(discontinued **)
Features: Excellent clarityHigh flexural modulusGood toughness and elongationStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specification..
|
|||
| Vicat Softening Point | >= 97.0 °C | >= 207 °F | ASTM D1525 |
|
Iran Petrochemical (PCC) Tabriz 1209AA LLDPE
(discontinued **)
Information provided by Iran Petrochemical Commercial Co.
|
|||
| Vicat Softening Point | 97.2 °C | 207 °F | ASTM D1525 |
|
I. Stern HIPS SH03 High Impact Polystyrene
Features:High flowExcellent toughnessExcellent processabilityApplicationsInjection moldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & Co. Inc.
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | ASTM D1525 |
|
Ineos Styrenics 495F High-Impact Polystyrene Resin (Global)
Description: High-impact, high-flow grade for a wide variety of applications, including appliance components, consumer electronics housings, magnetic and optical media, building and construction, pa..
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | 1000 g; ASTM D1525 |
|
LG Chemical 60HR-G HIPS
High flow, Heat resistance, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include TV sets, tape reco..
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | ASTM D1525 |
|
KKPC Kuhmo HI 425TVG High Flow/High Heat Resistant HIPS
Key features: High-impact, High-fluidity Common Uses: TV cover (gas injection).HIPS is a functional resin made by copolymerization of styrene monomer and PBR. It shows excellent balance between im..
|
|||
| Vicat Softening Point | 97.2 °C | 207 °F | ASTM D1525 |
|
Shuman SP880 Grey Polystyrene High Impact
Good impact strength, easy processability, good surface appearance, ULInformation provided by Shuman Plastics, Inc.
|
|||
| Vicat Softening Point | <= 97.0 °C | <= 207 °F | Compounding 21-200 |
|
Sibur ABS 2020 (30,31) Molding Grade ABS Plastic
With high thermal and light resistance for automobile building, stable to atmospheric conditions in thermal and electric ageing, contacting with food products, as well as with compounding with PC.
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | VST/A/120; ISO 306 |
|
Styrolution Polystyrol 165 H GR 2 PS
Description: Polystyrol 165 H is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.Applications: In blends with high impact Polystyrene or Styrolux; thermo..
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | B/120; ISO R306 |
|
Samsung Cheil Industries Starex® LX-0981 ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | B/50; ISO R306 |
|
Samsung Cheil Industries Starex® NH-0926 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | B/50; ISO R306 |
|
Samsung Cheil Industries Starex® NH-0926 ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | B/50; ISO R306 |
|
Samsung Cheil Industries Starex® SL-0110 ABS, Unreinforced
Information provided by Samsung Cheil Industries.
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | 1kg / 120°C; ASTM D1525 |
|
Supreme Petrochem SP 562 Flame Retardant Polystyrene
Characteristics Very good flow properties Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU Low specific gravity Processing Injection moldingApplications Large size T.V. Cabinets Aud..
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | ISO 306 |
|
Borealis FT5230 Low Density Polyethylene
FT5230 is a Low Density Polyethylene for Film Extrusion. This grade is developed for the production of packaging film with good optical properties for medium duty film applications. Applications: ..
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | A50; ISO 306 |
|
Lubrizol ESTANE® GP80AE Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
|
|||
| Vicat Softening Point |
97.0
°C @Load 1.02 kg |
207
°F @Load 2.25 lb |
50°C per hour; ASTM D1525 |
|
Total PS CPDS 814 UV Stabilized, Flame Retardant Polystyrene
Total Petrochemicals Polystyrene 814 is a heat resistant, UV stabilized V0 Non Deca Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensi..
|
|||
| Vicat Softening Point |
97.0
°C @Load 5.00 kg |
207
°F @Load 11.0 lb |
50°C/hr; ASTM D 1525 |
|
Cossa Polimeri ESTAPROP H 1080 TG Polypropylene, 40% Mineral Filled
PP homopolymer 40% mineral fillerExcellent stiffness, good dimensional stabilityInformation provided by Cossa Polimeri S.r.l.
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | ASTM D1525 |
|
Dow 608A Low Density Polyethylene (LDPE)
A formulated clarity film resin for thin gauge optical packaging Optimum gauge range: 0.8 - 2.5 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | 50°C/hr; 50N |
|
Arkema Group Orgalloy® LE 6000 Nylon Alloy, Flexible Grade (Conditioned)
LE series, flexible polyamide alloys: processable on PE screws, low moisture absorption, chemical resistance (no known solvents).medium viscosity and stiffness, specially suited to the extrusion of ..
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | 49 N; ISO 306 |
|
A.D. Compound Adene NTQA Homopolymer 40% Talc Filled Polypropylene
Information provided by A.D. Compound
|
|||
| Vicat Softening Point |
97.0
°C @Load 5.001 kg |
207
°F @Load 11.03 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYfill PP 150ENH Polypropylene, Flame Retardant, Halogen Free
Information provided by Polykemi AB
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | Rate B/50; ASTM D1525 |
|
SABIC Innovative Plastics NORYL FP5140HF PPE+PS
Noryl*FP5140HF is an unfilled, injection moldable modified polyphenylene ether resin with an ISO306 Vicat B/120 of 100 deg C. Designed for good dimensional stability and high flow, this resin also u..
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | 50°C/hr; 50N |
|
Polimeri Europa SINKRAL G323 ABS
(discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-20 General purpose injection moulding grade. Main properties are: good impact resistance high flow e..
|
|||
| Vicat Softening Point | 97.0 °C | 207 °F | 50°C/hr; 50N |
|
Polimeri Europa SINKRAL L320 ABS
(discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-25 General purpose, high flow injection moulding grade having good impact resistance coupled with an ..
|
|||