| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 213 °C | 415 °F | 49 N; ISO 306, ASTM D1525 |
|
Nilit Nilitop BT G6 General Purpose, 30% Glass Fiber Reinforced PBT
Description: Nilitop BT G6 is a general purpose, 30% glass fiber reinforced PBT. This product has good overall mechanical performance, low moisture absorption and excellent UV resistance. It is used..
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics ULTEM 2300 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics ULTEM 2300F PEI
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors.
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics ULTEM 2300F PEI (Europe-Africa-Middle East)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. US FDA and European Food Contact compliant. Effective June, 2007 this grade will no longer be supported with ..
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics ULTEM 2300R PEI (Europe-Africa-Middle East)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics ULTEM 2310 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics ULTEM 2310F PEI
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors.
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics ULTEM 2310F PEI (Europe-Africa-Middle East)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be..
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics ULTEM 2312 PEI (Europe-Africa-Middle East)
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics ULTEM 2312EPR PEI
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific)
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East)
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Ultem 2412EPR PEI (Asia Pacific)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the As..
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics ULTEM HU2110 PEI
10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP ..
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics ULTEM HU2300 PEI
30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP ..
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics ULTEM HU2310 PEI
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics ULTEM HU2310 PEI (Asia Pacific)
30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics ULTEM PW2300 PEI (Europe-Africa-Middle East)
30% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Specific grade-colors are designed and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified...
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Valox® VX8015U PBT+PET (Europe-Africa-Middle East)
VALOX VX8015U is a UV stabilized, 15% glass reinforced PBT+PET injection moulding resin with improved surface finish quality characteristics versus VALOX 815. This grade is 815 with improved gloss a..
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics LNP THERMOCOMP EX00781H PEI
LNP* THERMOCOMP* EX00781H is a compoud based on Polyetherimide containng Proprietary Filler(s). Added feature of this material is: Healthcare.
|
|||
| Vicat Softening Point | 213 °C | 415 °F | B/120; ISO 306 |
|
Sax Polymers SAXAMID 126F2K4 Nylon 6, Glass Fiber/Bead Filled
SAXAMID 126F2K4 is a 10% glass fibers and 20% glass beads filled polyamide 6 injection-molding-grade.Information provided by SAX Polymers
|
|||
| Vicat Softening Point | 213 °C | 415 °F | B/120; ISO 306 |
|
Sax Polymers SAXAMID 126F3 Nylon 6, 15% Glass Fiber
SAXAMID 126F3 is a polyamide 6 injection-molding-grade reinforced with 15% glass fibers.Information provided by SAX Polymers
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Valox® VX4029 PBT (Europe-Africa-Middle East)
VALOX VX4029 is a 30% glass reinforced PBT injection moulding resin with excellent strength, stiffness, dimensional stability and high heat resistance. This grade is a 420 with reduced additive load..
|
|||
| Vicat Softening Point | 213 °C | 415 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Valox® VX4029 PBT (Europe-Africa-Middle East)
VALOX VX4029 is a 30% glass reinforced PBT injection moulding resin with excellent strength, stiffness, dimensional stability and high heat resistance. This grade is a 420 with reduced additive load..
|
|||