| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 240 °C | 464 °F | B; STN EN ISO 306 |
|
Plastcom SLOVAMID 66 T 40 Polyamide 66, 40% Mineral Filled
FeaturesPA 66 with the content of 40% chemically modified mineral filling. Used for holders of electric hand tools, hobby tools, gears, covers of electric tools, flat products, automobile wheel cov..
|
|||
| Vicat Softening Point | 240 °C | 464 °F | 49 N; ASTM D1525 |
|
Nilit Polynil® P40 Low Viscosity Nylon 66
Description: Low viscosityApplication: CompoundingInformation provided by NILIT.
|
|||
| Vicat Softening Point | 240 °C | 464 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate..
|
|||
| Vicat Softening Point | 240 °C | 464 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific)
Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate..
|
|||
| Vicat Softening Point |
240
°C <br>@Load 5.10 kg
|
464
°F <br>@Load 11.2 lb
|
50°C/h |
|
Radici Radiflam® A RV300AF (dry) Nylon 66-30GF
Radiflam® A is a range of flame retardant polyamides 66 (PA 66) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided by Radici g..
|
|||
| Vicat Softening Point | 240 °C | 464 °F | ISO 306 |
|
Radici Radilon® ALX14080 (dry) Nylon 66
Medium high viscosityInformation provided by Radici group.
|
|||
| Vicat Softening Point | 240 °C | 464 °F | 49 N; ASTM D1525 |
|
Nilit Polynil® P50FI Internally Lubricated Nylon 66
Description: Polynil P50 FI is an internally lubricated NYLON 66 with excellent flow characteristics and high elongation. It is widely used throughout many industries for applications that have long..
|
|||
| Vicat Softening Point | 240 °C | 464 °F | 49 N; ASTM D1525 |
|
Nilit Polynil® P50FL Externally Lubricated, Lightly Nucleated Nylon 66
Description: Polynil P50FL is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips.Key characteristics: Excellent flowGood toughnessGood overall mechan..
|
|||
| Vicat Softening Point | 240 °C | 464 °F | DIN ISO 306 |
|
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Vicat Softening Point | 240 °C | 464 °F | DIN ISO 306 |
|
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15/BK PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Vicat Softening Point | 240 °C | 464 °F | DIN ISO 306 |
|
Lehmann & Voss LUVOCOM® 1301-7449 PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni..
|
|||
| Vicat Softening Point | 240 °C | 464 °F | DIN ISO 306 |
|
Lehmann & Voss LUVOCOM® 1301-8456 PPS, linear, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Vicat Softening Point | 240 °C | 464 °F | DIN ISO 306 |
|
Lehmann & Voss LUVOCOM® 1301-8524 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Vicat Softening Point |
240
°C <br>@Load 5.10 kg
|
464
°F <br>@Load 11.2 lb
|
120°C/hour; ISO 306 |
|
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber
PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS.
|
|||
| Vicat Softening Point |
240
°C <br>@Load 5.00 kg
|
464
°F <br>@Load 11.0 lb
|
|
|
LATI Latamid 66 B H-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. High fluidity. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Blended with PA6.Availability: Africa & Middle East..
|
|||
| Vicat Softening Point |
240
°C <br>@Load 5.00 kg
|
464
°F <br>@Load 11.0 lb
|
|
|
LATI Latamid 66 PA 66
Polyamide 66 (PA66). Unfilled.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
|
|||
| Vicat Softening Point |
240
°C <br>@Load 5.00 kg
|
464
°F <br>@Load 11.0 lb
|
|
|
LATI Latilub 66-02S PA66, Silicone Filled
Self-lubricating product based on Polyamide 66 (PA66). Silicone. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
|
|||
| Vicat Softening Point | 240 °C | 464 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Valox® V9280LW PET (Europe-Africa-Middle East)
40% Glassfiber / Mineral Filled PET, Impact Modifier, Mold Release, Heat StabilizedThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Vicat Softening Point | 240 °C | 464 °F | Rate A/50; ISO 306 |
|
SABIC Innovative Plastics NORYL GTX GTX924 PPE+PA (Europe-Africa-Middle East)
NORYL GTX 924 is an UV stabilized unfilled Noryl GTX grade with improved processability. Noryl GTX 924 is specially designed for wheeltrim applications.
|
|||
| Vicat Softening Point | 240 °C | 464 °F | Rate B/50; ASTM D1525 |
|
SABIC Innovative Plastics NORYL GTX GTX810 PPE+PS+PA (Asia Pacific)
GR 10%. Increased stiffness of 200000 psi (3000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: lighting.
|
|||
| Vicat Softening Point | 240 °C | 464 °F | ISO 306 |
|
Tisan TISLAMID® 66 30% Mineral Reinforced Nylon 66
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
|
|||
| Vicat Softening Point | 240 °C | 464 °F | B/120; ISO 306 |
|
Eurostar Staramide AS3 PA66, 15% Glass Bead Reinforced, Injection Molding
Staramide AS3 is a 15% Glass Bead Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Vicat Softening Point | 240 °C | 464 °F | A/50; ISO 306 |
|
Eurostar Staramide RF00AES PA66/6, 50% Glass Filled, Injection Molded
Staramide RF00AES is a 50% Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as Staramide 66 C 50V S3)Information provided by Eurostar.
|
|||
| Vicat Softening Point | 240 °C | 464 °F | B/50; ISO 306 |
|
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded
AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
|
|||
| Vicat Softening Point | 240 °C | 464 °F | 50N; ISO 306 |
|
Eurotec® Tecomid® NA40 GR30 NL IH PA 6.6 30% glass fiber reinforced, impact modified
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Vicat Softening Point | 240 °C | 464 °F | 50N; ISO 306 |
|
Eurotec® Tecomid® NA40 MR30 NL PA 6.6 30% mineral reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Vicat Softening Point |
240
°C <br>@Load 5.10 kg
|
464
°F <br>@Load 11.2 lb
|
50°C/h |
|
Radici Radilon® A 38 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Vicat Softening Point |
240
°C <br>@Load 5.10 kg
|
464
°F <br>@Load 11.2 lb
|
50°C/h |
|
Radici Radilon® A 42 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
|
|||
| Vicat Softening Point | 240 °C | 464 °F | DAM; 50°C/h 50N; ISO 306 |
|
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**)
Unreinforced UV Stabilized Polyamide 66 Zytel 105F BK010 is a lubricated fast cycling weather resistant PA 66 resin. Zytel 105F BK010 contains finely dispersed carbon black.Information provided by D..
|
|||
| Vicat Softening Point | 240 °C | 464 °F | 50 N; 120 °C/h; ISO 306 |
|
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber
PA 66, 25% glass fiber, injection molding, flame retardantInformation provided by LANXESS.
|
|||