| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 130 °C | 266 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Asia Pacific)
PC+ ABS Automotive applications
|
|||
| Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer
7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only
|
|||
| Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer
11 MFR LEXAN High Flow Ductile Copolymer
|
|||
| Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® HFD1413 PC Copolymer (Asia Pacific)
11 MFR LEXAN High Flow Ductile Copolymer
|
|||
| Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® EXRL0684 PC Copolymer
7 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region.
|
|||
| Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® HFD1433 PC Copolymer (Asia Pacific)
11 MFR LEXAN High Flow Ductile Copolymer UV stabilized
|
|||
| Vicat Softening Point | 130 - 170 °C | 266 - 338 °F | Average value: 150 °C Grade Count:3 |
|
Overview of materials for Thermoplastic Polyimide, Unfilled |
|||
| Vicat Softening Point | 130 °C | 266 °F | ASTM D1525 |
|
Ineos G50-100 HDPE
Ineos G50-100 is a high molecular weight, high density polyethylene copolymer developed for sheet extrusion, thermoforming and large part blowmolding where the finished product demands outstanding p..
|
|||
| Vicat Softening Point | 130 °C | 266 °F | ASTM D1525 |
|
IRPC Polimaxx Polene GA2850 High Density Polyethylene
CHARACTERISTICS: HIGH MOLECULAR WEIGH FOR BLOW MOLDING GRADE, RIGID, STACKABLE AND HIGHLY SHOCK RESISTANT CONTAINERS, EXCELLENT IMPACT STRENGTH APPLICATIONS: BLOW MOLDING FOR L-RING DRUMS (200 LITRE..
|
|||
| Vicat Softening Point | 130 °C | 266 °F | ASTM D1525 |
|
IRPC Polimaxx Polene GM2865 High Density Polyethylene
CHARACTERISTICS: EXCELLENT STIFFNESS, GOOD PROCESSABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, DAIRY PRODUCT BOTTLES MILK BOTTLES AND GALL..
|
|||
| Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics NORYL V01525 PPE+HIPS
Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
|
|||
| Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ASTM D1525 |
|
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Asia Pacific)
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
|
|||
| Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ASTM D 1525 |
|
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Europe-Africa-Middle East)
PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Noryl HB1525 PPE+HIPS (Europe-Africa-Middle East)
NORYL HB1525 is a 15 % short glass fibre reinforced material with a HDT/A of 115°C according ISO 75. NORYL HB1525 is an easy flow material designed for applications where dimensional stability an..
|
|||
| Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ASTM D1525 |
|
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
|
|||
| Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics NORYL N1150 PPE+PS (Asia Pacific)
Noryl* N1150 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and good flow, this resin also uses non-chlorinated, non-brominated FR add..
|
|||
| Vicat Softening Point | 130 °C | 266 °F | 5kg / 120°C; ASTM D1525 |
|
Supreme Petrochem SP 6460 High Heat Polystyrene
Characteristics High impact and modulus Easy flow High heat resistance & strength Available in any dark colorProcessing Injection moldingApplications Instrument enclosures Automobile interior pa..
|
|||
| Vicat Softening Point | 130 °C | 266 °F | 10N-50°C per hour; ISO 306 |
|
Total PPC 9712 Polypropylene, Heterophasic Copolymer
ATOFINA Propylene 9712 is heterophasic copolymer. PPC 9712 is characterized by excellent impact resistance and antistatic properties and has been formulated to allow faster cycling through early de..
|
|||
| Vicat Softening Point | 130 °C | 266 °F | A (10N); ISO 306 |
|
Borealis Daplen™ EE260AE Scratch Resistant Polypropylene Compound
Daplen EE206AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE206AE is optimized to provide excellent scratch resistance on gained and unpai..
|
|||
| Vicat Softening Point | 130 °C | 266 °F | Loading 1, Rate A; ASTM D1525 |
|
Chevron Phillips Marlex® K605 HDPE Blow Molding Resin
Resin Type: Ethylene HomopolymerCharacteristics: Good ESCRExceptional rigidityExcellent melt strengthApplications: Automotive bumper beamsInformation provided by Chevron Phillips.
|
|||
| Vicat Softening Point | 130 °C | 266 °F | 0.125 inch, 1 Kg; ASTM D1525 |
|
Diamond Polymers ASA 5946
Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc.
|
|||
| Vicat Softening Point | 130 °C | 266 °F | 50 N - B method; ISO 306 |
|
Arkema Group Orgalloy® R 60 ES Polyamide Alloy
Polyamide Alloy, Film and PackagingInformation provided by Arkema Group
|
|||
| Vicat Softening Point | 130 °C | 266 °F | ISO 306 |
|
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Vicat Softening Point | 130 °C | 266 °F | B |
|
Plastcom SLOVALEN PH 91 GF 10 PP, 10% glass fibre
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10% glass fibre. Increased strength in comparison with unfilled PP. Applied in all industry branches. Increased str..
|
|||
| Vicat Softening Point | 130 °C | 266 °F | B; STN EN ISO 306 |
|
Plastcom SLOVALEN PH 91 GF 15 Polypropylene Homopolymer, 15% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 15% glass fiber, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suit..
|
|||
| Vicat Softening Point | 130 - 160 °C | 266 - 320 °F | Average value: 148 °C Grade Count:20 |
|
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
|
|||
| Vicat Softening Point | 130 °C | 266 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Asia Pacific)
25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only
|
|||
| Vicat Softening Point | 130 °C | 266 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Asia Pacific)
25 MFR LEXAN High Flow Ductile Copolymer
|
|||
| Vicat Softening Point | 130 °C | 266 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Valox® VX4915 ASA+PBT (Europe-Africa-Middle East)
15% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||