| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® 123X PC Copolymer
Improved flow PC with excellent processability and mold release.
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® 1278R PC (Europe-Africa-Middle East)
LEXAN 1278R is a medium viscosity, 20% glass reinforced, flame retardant grade, offering a very high rigidity. It is especially designed for applications like industrial enclosures and fuse boxes re..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® 505R PC
Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm...
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Lexan® 915AU PC
LEXAN resin grade 915AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in transparent colors, inte..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Lexan® 916R PC (Europe-Africa-Middle East)
Lexan* 916R Polycarbonate (PC) resin is a low viscosity, non-filled, injection molding grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating at 0.8 mm properties. Lexan* ..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific)
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® 9945A PC
Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® EXL1443T PC Copolymer (Asia Pacific)
Lexan* EXL1443T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance. This resin offers excellent low temperature (-30 C) ductility in co..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® EXL6414 PC
PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ASTM D1525 |
|
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific)
PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® FXG141R PC (Europe-Africa-Middle East)
LEXAN FXG141R is a transparent/translucent medium viscosity grade for special effects colors with a diamond sparkle appearance. Color package may affect performance.This data was supplied by SABIC-I..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ASTM D1525 |
|
SABIC Innovative Plastics Lexan® FXM1413T PC Copolymer (Asia Pacific)
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® HPX4EU PC Copolymer (Europe-Africa-Middle East)
Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ASTM D1525 |
|
SABIC Innovative Plastics Lexan® IR2110 PC (Europe-Africa-Middle East)
IR2110 resin is a medium-high flow (MFR = 15 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate A/50; ASTM D1525 |
|
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer
Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) ..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Lexan® EXL9134 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL9134 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high flow opaque injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, ..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® FXD144R PC (Europe-Africa-Middle East)
LEXAN FXD144R is a transparent/translucent medium viscosity grade for light diffusion effects. FDA compliant. Internal mold release. The color package may affect performance.This data was supplie..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate A/50; ASTM D 1525 |
|
SABIC Innovative Plastics Lexan® FXE1413T PC Copolymer
Clear PC-siloxane copolymer with excellent processability, for Visual fX capability in "Energy" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color packa..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Lexan® FXM921A PC (Europe-Africa-Middle East)
LEXAN FXM921A is a transparent/translucent, medium viscosity, flame retardant grade with a metallic-luster appearance. Color package may affect performance.This data was supplied by SABIC-IP for the..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Lexan® HFD4211 PC (Europe-Africa-Middle East)
Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release.
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Lexan® HP2NR PC (Asia Pacific)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no..
|
|||
| Vicat Softening Point |
141
°C <br>@Load 5.00 kg
|
286
°F <br>@Load 11.0 lb
|
50°C/h; ASTM D1525 |
|
LG Chemical LUPOY GP1000L PC, Transparent
Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, E&E Housing and Components Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical
|
|||
| Vicat Softening Point |
141
°C <br>@Load 5.00 kg
|
286
°F <br>@Load 11.0 lb
|
50°C/h; ASTM D1525 |
|
LG Chemical LUPOY GP1000M PC, Transparent
Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA, Electric & Electronic Housing and Components, Automotive Exterior and InteriorCAS: 103598-77-2Information provide..
|
|||
| Vicat Softening Point |
141
°C <br>@Load 5.00 kg
|
286
°F <br>@Load 11.0 lb
|
50°C/h; ASTM D1525 |
|
LG Chemical LUPOY GP1000MR PC, Transparent
Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics PC1800 PC (Europe-Africa-Middle East)
PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold ..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ASTM D1525 |
|
SABIC Innovative Plastics PC1800 PC (Europe-Africa-Middle East)
PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Noryl GFN1420V PPE+PS (Asia Pacific)
Noryl* GFN1420V resin is a high flow blend of polyphenylene ether (PPE) and polystyrene (PS) resin that contains 20 % glass reinforcement. The resin is suitable for injection molding and is designe..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics NORYL PX1736 PPE+PS
Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/50; ASTM D1525 |
|
SABIC Innovative Plastics NORYL PX1736 PPE+PS
Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica..
|
|||
| Vicat Softening Point | 141 °C | 286 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics NORYL ENG265 PPE+PS
PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a..
|
|||