| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 152 °C | 305 °F | 120°C/h, 50 N; ASTM D1525 |
|
Polymer Resources PC-FD2-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p..
|
|||
| Vicat Softening Point | 152 °C | 305 °F | 120°C/h, 50 N; ASTM D1525 |
|
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow
Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on..
|
|||
| Vicat Softening Point | 152 °C | 305 °F | 120°C/h, 50 N; ASTM D1525 |
|
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release
Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
|
|||
| Vicat Softening Point | 152 °C | 305 °F | 120°C/h, 50 N; ASTM D1525 |
|
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant
Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
|
|||
| Vicat Softening Point | 152 °C | 305 °F | 120°C/h, 50 N; ASTM D1525 |
|
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release
Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa..
|
|||
| Vicat Softening Point | 152 °C | 305 °F | 120°C/h, 50 N; ASTM D1525 |
|
Polymer Resources PC-UV2-D-[color]-1 Polycarbonate, UV-stabilized, Medium Flow with Mold Release
Polycarbonate, UV-stabilized, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
|
|||
| Vicat Softening Point | 152 °C | 305 °F | 120°C/h, 50 N; ASTM D1525 |
|
Polymer Resources PPX-G30 Modified-PPO, 30% Glass Reinforced
Modified-Polyphenylene Oxide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr..
|
|||
| Vicat Softening Point | 152 °C | 305 °F | ASTM D1525 |
|
Ravago Manufacturing Americas Hylex® P10017FRMA Polycarbonate
Polycarbonate, General Purpose, Flame RetardantInformation provided by Ravago.
|
|||
| Vicat Softening Point | 152 °C | 305 °F | ASTM D1525 |
|
Ravago Manufacturing Americas Hylex® P1010FRMA Polycarbonate
Polycarbonate, General Purpose, Flame RetardantInformation provided by Ravago.
|
|||
| Vicat Softening Point | 152 °C | 305 °F | ASTM D1525 |
|
Ravago Manufacturing Americas Hylex® P1032L Polycarbonate, Unreinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
|
|||
| Vicat Softening Point | 152 °C | 305 °F | ASTM D1525 |
|
Ravago Manufacturing Americas Hylex® P1310FRMA Polycarbonate
Polycarbonate, General Purpose, Flame Retardant, UV StabilizedInformation provided by Ravago.
|
|||
| Vicat Softening Point | 152 °C | 305 °F | ASTM D1525 |
|
Ravago Manufacturing Americas Hylex® P1332L Polycarbonate, UV Stabilized, Unreinforced
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
|
|||
| Vicat Softening Point | 152 °C | 305 °F | 120°C/h, 50 N; ASTM D1525 |
|
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant
Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam..
|
|||
| Vicat Softening Point | 152 °C | 305 °F | 120°C/h, 50 N; ASTM D1525 |
|
Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow
Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by..
|
|||
| Vicat Softening Point | 152 °C | 305 °F | ASTM D1525 |
|
Entec Hylex® P1310FR Polycarbonate
Information provided by Ravago
|
|||
| Vicat Softening Point | 152 °C | 305 °F | ASTM D1525 |
|
Entec Hylex® P1010FR Polycarbonate
Information provided by Ravago.
|
|||
| Vicat Softening Point | 152 °C | 305 °F | ASTM D1525 |
|
Entec Hylex® P1025L2 HB Polycarbonate
Available in North America Additive: Mold Release Features: Good Mold Release and High Flow RoHS Compliant Form: Pellets Appearance: Blue Information provided by Entec
|
|||