| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 152 °C | 306 °F | STN EN ISO 306 |
|
Plastcom PLASTALEN® PH 91 T 20 Polypropylene reinforced with mineral filler
Modified homopolymer PP for injection molding with the content of 20 % mineral filler. General application in all industry branches. Delivered in natural mode and in the full RAL color scale.Informa..
|
|||
| Vicat Softening Point |
152
°C @Load 5.001 kg |
306
°F @Load 11.03 lb |
50°C/h; ISO 306 |
|
Polykemi AB POLYform POM C M270 Polyoxymethylene
Information provided by Polykemi AB
|
|||
| Vicat Softening Point | 152 °C | 306 °F | ASTM D1525 |
|
PolyMirae Moplen EP300C Sheet and Thermoforming Grade Polypropylene
Moplen EP300C is the polypropylene blockpolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300C is a block copolymer particularly suitable for sheet and t..
|
|||
| Vicat Softening Point | 152 °C | 306 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Lexan® XHT1141 PC
XHT1141 is a high flow, high heat polycarbonate copolymer. It is the lowest heat product in the LEXAN* XHT portfolio. It is available in a range of opaque and limited transparent colors.
|
|||
| Vicat Softening Point | 152 °C | 306 °F | 50°C/h 50N; ISO 306 |
|
LATI LATILUB 73/13-01M Polyoxymethylene Base (POM), 1% Molybdenum Disulfide Self Lubricating Plastic
(Unv
Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri..
|
|||
| Vicat Softening Point | 152 °C | 306 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Lexan® XHT1141 PC (Europe-Africa-Middle East)
XHT1141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
|
|||
| Vicat Softening Point |
152
°C @Load 1.00 kg |
306
°F @Load 2.20 lb |
ASTM D1525 |
|
LG Chemical SEETEC M1700 Polypropylene Impact Copolymer
Features: SEETEC M1700 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1700 exhibits a very high flowability and a good balance of stiffness and impact strength..
|
|||
| Vicat Softening Point | 152 °C | 306 °F | ASTM D1525-97 |
|
Ipiranga Petrochem PH 1710 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
|
|||
| Vicat Softening Point | 152 °C | 306 °F | ASTM D1525-97 |
|
Ipiranga Petrochem PH 3515 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
|
|||
| Vicat Softening Point | 152 °C | 306 °F | 50°C/h 50N; ISO 306 |
|
Mitsubishi Xantar® G6F 23 R Polycarbonate-30% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
|
|||
| Vicat Softening Point | 152 °C | 306 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics LNP STAT-LOY ZF3021 PPE+PS (Europe-Africa-Middle East)
LNP* STAT-LOY* ZF3021 is a compound based on PPE + PS Blend resin containing Glass Fiber. Added features include Antistatic, Flame Retardant.
|
|||
| Vicat Softening Point | 152 °C | 306 °F | 50°C/hr, 50N; ISO 306 |
|
Teijin Panlite® GS-3430 Friction and Abrasion Resistant, Glass Fiber Reinforced Polycarbonate Resin
GF 30% reinforced grade, meeting UL 94 V-2. It is compounded with fluorine powder to improve friction and abrasion resistance, maintaining excellent characteristics of polycarbonate resin.Applicatio..
|
|||
| Vicat Softening Point | 152 °C | 306 °F | |
|
Styron CALIBREâ„¢ 300EP 22 Polycarbonate, General Purpose
CALIBRE® 300EP series resins are general purpose polycarbonate resins and can be supplied with a mold release package, a UV stabilizer package or both. CALIBRE 300EP resins exhibit an excellent p..
|
|||
| Vicat Softening Point |
152
°C @Load 5.10 kg |
306
°F @Load 11.2 lb |
A50; ISO 306 |
|
Borealis HD204CF Polypropylene
HD204CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD204CF is recommended for medical applications, inner layer in co extru..
|
|||
| Vicat Softening Point | 152 °C | 306 °F | A50; ISO 306 |
|
Lubrizol ESTANE® GP65DE Ester Based Thermoplastic Polyurethane
Type: Estane® GP 65DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b..
|
|||
| Vicat Softening Point | 152 °C | 306 °F | ISO 306 |
|
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
|
|||
| Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
|
ExxonMobil PP1014H1 Polypropylene Homopolymer
Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.Availability: Europe and North America Features:Autoclave SterilizableE..
|
|||
| Vicat Softening Point |
152
°C @Load 1.00 kg, Thickness 3.17 mm |
306
°F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
|
Diamond Polymers DIAMALOY PC 1008 Impact Modified Polycarbonate
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
|
|||
| Vicat Softening Point | 152 °C | 306 °F | -1kg; ASTM D1525 |
|
Braskem H 306 Fiber Extrusion Polypropylene
Applications: Staple fibers for carpets and blankets. Information provided by Braskem
|
|||
| Vicat Softening Point | 152 °C | 306 °F | -1kg; ASTM D1525 |
|
Braskem H 605 Thermoforming Polypropylene
Applications: Flat and corrugated sheets with high transparency; thermoformed packing with high transparency. Information provided by Braskem
|
|||
| Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
|
Addiplast Addilene J 220 M20 Polypropylene Copolymer
Mineral reinforced, improved rigidityInformation provided by Addiplast.
|
|||
| Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
|
Addiplast Addilene J 490 S Flame Retardant Polypropylene
Flame retardant, unreinforced, with halogensInformation provided by Addiplast.
|
|||
| Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
|
Addiplast Addilene J 520 M20 Polypropylene Copolymer
Mineral reinforced, improved rigidityInformation provided by Addiplast.
|
|||
| Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
|
Addiplast Addilene J 522 M20 Polypropylene Copolymer
Mineral reinforced, improved rigidityInformation provided by Addiplast.
|
|||
| Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
|
Addiplast Addilene J 522 N30 Polypropylene Copolymer
Mineral reinforced, improved scratch resistanceInformation provided by Addiplast.
|
|||
| Vicat Softening Point | 152 °C | 306 °F | -1kg; ASTM D1525 |
|
Braskem CP 405 XP Injection Molding Polypropylene
Applications: Caps for soft drinks. Information provided by Braskem
|
|||
| Vicat Softening Point | 152 °C | 306 °F | ISO 306/A50 |
|
Addiplast Addilene J 490 M40S Flame Retardant Polypropylene, 40% Mineral Filled
Flame retardant, mineral filled, with halogensInformation provided by Addiplast.
|
|||
| Vicat Softening Point | 152 °C | 306 °F | 50°C/hr, 50N; ISO 306 |
|
Teijin Panlite® B-8120R Carbon Fiber Reinforced Polycarbonate Resin
CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.Applica..
|
|||
| Vicat Softening Point |
152
°C @Load 1.02 kg |
306
°F @Load 2.25 lb |
ISO 306 |
|
Borealis HD214CF Polypropylene Homopolymer
HD214CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: food packaging, lamination films, stationary films, multi layer co-extrus..
|
|||
| Vicat Softening Point | 152 °C | 306 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics NORYL FE1740PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1740PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
|
|||