| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 200 °C | 392 °F | STN EN ISO 306 |
|
Plastcom PLASTAMID® 6 GF 25 002 PA6 reinforced with glass fiber
PA 6 for injection molding, reinforced with 25% glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, ..
|
|||
| Vicat Softening Point | 200 °C | 392 °F | B; STN EN ISO 306 |
|
Plastcom SLOVAMID 6 GF 5 FRA 5 Polyamide 6, 5% Glass Fiber, Halogen Flame Retardant
FeaturesPA 6 for injection moulding, chemically reinforced with 5% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C, ..
|
|||
| Vicat Softening Point |
>=
200
°C @Load 5.001 kg |
>=
392
°F @Load 11.03 lb |
50°C/h; ISO 306 |
|
Polykemi AB SCANMID 6 B12^ F20 Nylon 6, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Vicat Softening Point | 200 °C | 392 °F | B; STN EN ISO 306 |
|
Plastcom SLOVAMID 6 G 10 Polyamide 6, 10% Graphite
FeaturesPA 6 for injection moulding with addition of 10% graphite, the PA surface rolling resistance force is significantly lowered. Used mainly in the product of crates and cases for bearings, sli..
|
|||
| Vicat Softening Point | 200 °C | 392 °F | B |
|
Plastcom SLOVASTER® B FRN 3 LS PBT, flame retarder, light stable
FeaturesPBT basic type for injection molding. Melt is characterised by outstanding fluidity, which enables injection molding of complicated and divided products also on multiple molds. Anisotropy of..
|
|||
| Vicat Softening Point |
>=
200
°C @Load 5.001 kg |
>=
392
°F @Load 11.03 lb |
50°C/h; ISO 306 |
|
Polykemi AB SCANMID 6 B12^ QF2515 Nylon 6, Glass Fiber and Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Vicat Softening Point | 200 - 265 °C | 392 - 509 °F | Average value: 238 °C Grade Count:15 |
|
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
|
|||
| Vicat Softening Point | >= 200 °C | >= 392 °F | 50 N; ISO 306 |
|
Grupo Repol Dinalon® B1S25 N Fast Cycling, Nucleated Nylon 6
Mechanical properties are for dry as molded samples.Information provided by Grupo Repol.
|
|||
| Vicat Softening Point | >= 200 °C | >= 392 °F | 50N; ISO 306 |
|
Grupo Repol Dinalon® B1V25 PA6 Unreinforced
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
|
|||
| Vicat Softening Point | 200 °C | 392 °F | 50°C/h 50N; ISO 306 |
|
Lanxess Durethan® B 30 S 000000 Nylon 6
PA 6, injection molding-grade, non-reinforced, easy-flow, easy-release, rapid solidification
|
|||
| Vicat Softening Point |
>=
200
°C @Load 5.10 kg |
>=
392
°F @Load 11.2 lb |
120°C/hour; ISO 306 |
|
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced
PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| Vicat Softening Point | 200 °C | 392 °F | 50°C/h 50N; ISO 306 |
|
Lanxess Pocan® BF 8230 000000 PBT, 30% Glass Fiber
PBT, 30% glass spheres/glass fibers, injection molding, flame retardant, low tendency to warp, improved surface finish
|
|||
| Vicat Softening Point |
200
°C @Load 5.00 kg |
392
°F @Load 11.0 lb |
|
|
LATI Laticonther 62 GR/70 PA 6, 70% Graphite Reinforced
High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te..
|
|||
| Vicat Softening Point | 200 °C | 392 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Ultem 1100R PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Vicat Softening Point | 200 °C | 392 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Ultem 1110V PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Vicat Softening Point | 200 °C | 392 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Valox® IQNH4550 PBT (Asia Pacific)
Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT..
|
|||
| Vicat Softening Point | 200 °C | 392 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Valox® SHF434HR PBT
PBT, Super High Flow, 20% glass reinforced,hydrolytically resistant.
|
|||
| Vicat Softening Point | 200 °C | 392 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Valox® SHF436HR PBT (Europe-Africa-Middle East)
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
|
|||
| Vicat Softening Point | 200 °C | 392 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Asia Pacific)
NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance.
|
|||
| Vicat Softening Point | 200 °C | 392 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66
NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe..
|
|||
| Vicat Softening Point | 200 °C | 392 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics NORYL GTX GTX973 PPE+PA (Europe-Africa-Middle East)
NORYL GTX973 is a material especially designed for electrostatic painting and powder coating applications. The material combines high heat resistance with impact and conductivity in a unique way.
|
|||
| Vicat Softening Point | 200 °C | 392 °F | Rate B/120; ISO 306 |
|
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Europe-Africa-Middle East)
Conductive GTX, CTE 7
|
|||
| Vicat Softening Point | 200 °C | 392 °F | 50 N; ISO 306 |
|
CP-Polymer-Technik Wellamid® 6000 GX 350 HWCP Combination Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Vicat Softening Point | 200 °C | 392 °F | 50 N; ISO 306 |
|
CP-Polymer-Technik Wellamid® 6000 MX 400 CP Combination Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Vicat Softening Point | 200 °C | 392 °F | 50 N; ISO 306 |
|
CP-Polymer-Technik Wellamid® 6600/58 HWCP Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Vicat Softening Point | 200 °C | 392 °F | 50N; ISO 306 |
|
Eurotec® Tecomid® NB40 MR30 NL PA 6 30% mineral reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Vicat Softening Point | 200 °C | 392 °F | 50 N; ISO 306 |
|
CP-Polymer-Technik Wellamid® 6000 GV 30 HWCP 30% Glass Fiber Nylon 6, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Vicat Softening Point |
200
°C @Load 5.10 kg |
392
°F @Load 11.2 lb |
ISO 306 |
|
Azoty Tarnow™ Tarnamid® T-27 MF30 Polyamide 6 - Mineral Reinforced
30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani..
|
|||
| Vicat Softening Point | >= 200 °C | >= 392 °F | 50N; ISO 306 |
|
Grupo Repol Dinalon® B2S35 V2-7035 PA6 High Viscosity, V2 Halogen Free, RAL 7035
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
|
|||