| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 230 °C | 446 °F | B |
|
Plastcom SLOVAMID 66 MI PA66, improved strength
FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe..
|
|||
| Vicat Softening Point |
>=
230
°C @Load 5.001 kg |
>=
446
°F @Load 11.03 lb |
50°C/h; ISO 306 |
|
Polykemi AB SCANAMID 66 A12^ F35 Nylon 66, Glass Fiber Reinforced, Modified
Information provided by Polykemi AB
|
|||
| Vicat Softening Point |
>=
230
°C @Load 5.001 kg |
>=
446
°F @Load 11.03 lb |
50°C/h; ISO 306 |
|
Polykemi AB SCANAMID 66 A12^ F50 Nylon 66, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Vicat Softening Point | 230 - 245 °C | 446 - 473 °F | Average value: 241 °C Grade Count:4 |
|
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi..
|
|||
| Vicat Softening Point | >= 230 °C | >= 446 °F | 50N; ISO 306 |
|
Grupo Repol Dinalon® A1S25 G15 PA66 15% Glass Fiber
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
|
|||
| Vicat Softening Point | >= 230 °C | >= 446 °F | 50 N; ISO 306 |
|
Grupo Repol Dinalon® A1S25 G25PV0 25% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 66
Mechanical properties are for dry as molded samples.Information provided by Grupo Repol.
|
|||
| Vicat Softening Point | >= 230 °C | >= 446 °F | 50 N; ISO 306 |
|
Grupo Repol Dinalon® A1S25 G35PV0 35% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 66
Mechanical properties are for dry as molded samples.Information provided by Grupo Repol.
|
|||
| Vicat Softening Point | >= 230 °C | >= 446 °F | 50N; ISO 306 |
|
Grupo Repol Dinalon® A3S25 PA66 Unreinforced
Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol
|
|||
| Vicat Softening Point | 230 °C | 446 °F | 50°C/h 50N; ISO 306 |
|
Lanxess Durethan® AKV 30 H2.0 901510 Nylon 66, 30% Glass Fiber
PA 66, injection molding-grade, 30% glass fibers, good heat-ageing resistance
|
|||
| Vicat Softening Point |
230
°C @Load 5.10 kg |
446
°F @Load 11.2 lb |
120°C/hour; ISO 306 |
|
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant
PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS.
|
|||
| Vicat Softening Point |
230
°C @Load 5.00 kg |
446
°F @Load 11.0 lb |
|
|
LATI Latiohm 57-05 PD01 G/15 PPA, 15% Glass Fiber Reinforced
Semiconductive/dissipative product based on Semi-aromatic polyamide (PPA). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by..
|
|||
| Vicat Softening Point |
230
°C @Load 5.00 kg |
446
°F @Load 11.0 lb |
|
|
LATI Latiohm 66-08 PD02 G/35 PA66, 35% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
|
|||
| Vicat Softening Point | 230 °C | 446 °F | Rate A/50; ISO 306 |
|
SABIC Innovative Plastics ULTEM 2400 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
|
|||
| Vicat Softening Point | 230 °C | 446 °F | Rate A/50; ISO 306 |
|
SABIC Innovative Plastics ULTEM 2410 PEI (Europe-Africa-Middle East)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
|
|||
| Vicat Softening Point | 230 °C | 446 °F | Rate A/50; ISO 306 |
|
SABIC Innovative Plastics ULTEM 2410R PEI (Europe-Africa-Middle East)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
|
|||
| Vicat Softening Point | 230 °C | 446 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Valox® V9260CS PET (Europe-Africa-Middle East)
Color Stable Glass filled PET
|
|||
| Vicat Softening Point | 230 °C | 446 °F | Rate B/50; ISO 306 |
|
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A..
|
|||
| Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
|
CP-Polymer-Technik Wellamid® 6600 CF20 HWCP 20% Carbon Fiber Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
|
CP-Polymer-Technik Wellamid® 6600 GS 20 HWCP 20% Glass Sphere Filled Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
|
CP-Polymer-Technik Wellamid® 6600 HW Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
|
CP-Polymer-Technik Wellamid® 6600 HWS Nylon 66, Finely Crystalline, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
|
CP-Polymer-Technik Wellamid® 6600 MR 309 HWCP 30% Mineral Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
|
CP-Polymer-Technik Wellamid® 6600 MRGV 20/20 HWCP 20% Mineral and 20% Glass Fiber Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
|
CP-Polymer-Technik Wellamid® 6600/58 GV 30 HWCP 30% Glass Fiber Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Vicat Softening Point | 230 °C | 446 °F | B/120; ISO 306 |
|
Eurostar Staramide BK8 PA6, 40% Mineral Fiber Filled, Injection Molded
Staramide BK8 is a 40% Mineral Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Vicat Softening Point | 230 °C | 446 °F | 50 N; ISO 306 |
|
CP-Polymer-Technik Wellamid® 6600 GS 15 HWCP 15% Glass Sphere Filled Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
|
|||
| Vicat Softening Point | 230 °C | 446 °F | DIN ISO 306 |
|
Lehmann & Voss LUVOCOM® 1-7497 Polyamide 66, with PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
|
|||