Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 97.0 °C | 207 °F | 10 N - 50°C/h; ISO 306/A |
Polimeri Europa Edistir N 2560 Polystyrene High molecular weight general purpose polystyrene with good mechanical strength and good thermal resistance. It is recommended for in-line forming of disposable packaging, for sheet
extrusion in ble.. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycolac® EX58F ABS (Europe-Africa-Middle East) High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | ASTM D1525 |
Petroquimica Triunfo Trithene® TN 7006 LDPE - Coextruded Film The Trithene® TS 7006 resin is a low-density polyethylene (LDPE) with high molecular weight and very good clarity. The unique combination of good processability, bubble stability, gloss, and streng.. |
|||
Vicat Softening Point | 97.0 °C @Load 1.00 kg |
207 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T CMH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CMH 108 show e.. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | 10N (T° increase = 50°C/h); ISO 306A50 |
Total Lacqrene® 1240 Crystal Polystyrene
(discontinued **) LACQRENE® 1240 is a high molecular weight crystal polystyrene, used in the dilution of high impact grades of polystyrene such as LACQRENE® 7240 or clear impact polystyrene such as Finaclear 520. .. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | |
Ineos ABS Lustran® QE 1006, Extrusion Grade
(discontinued **) Extrusion grade with high impact.Applications: High impact plates.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majo.. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | ASTM D1525 |
LyondellBasell Microthene® F FN51900 Low Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Vicat Softening Point | 97.0 °C @Load 5.00 kg |
207 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical MP220 ABS, High Adhesion, Heat Resistance Feature: Injection Molding, High Adhesion, Metal PlatingApplication: Automobiles Radiator Grill, MoldingCAS No. 9003-56-9 and 9003-54-7Information provided by LG Chemical |
|||
Vicat Softening Point | 97.0 °C | 207 °F | ASTM D1525 |
Ineos Styrenics Avantra® 594E High Impact Styrenic Polymer (NAFTA) Description: Avantra® 594E is a super high-impact polystyrene grade that delivers excellent processing efficiency along with toughness and high gloss in a wide variety of injection molding applic.. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | ISO 306A |
Lucite International Diakon® ST25G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | 1000 g; ASTM D1525 |
LG Chemical 60HR-G HIPS High flow, Heat resistance, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include TV sets, tape reco.. |
|||
Vicat Softening Point | <= 97.0 °C | <= 207 °F | Compounding 21-200 |
Sibur ABS 2020 (30,31) Molding Grade ABS Plastic With high thermal and light resistance for automobile building, stable to atmospheric conditions in thermal and electric ageing, contacting with food products, as well as with compounding with PC. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | B/120; ISO R306 |
Samsung Cheil Industries Starex® LX-0981 ABS, Unreinforced Metallic-Look Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® SP-0170 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | ISO 306/B50 |
Styron MAGNUMâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. It can be processed by injection molding, extrusion or thermoforming. The mass (c.. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | VST/A/120; ISO 306 |
Styrolution Polystyrol 165 H GR 21 PS Description: Polystyrol 165 H is a high molecular weight, good flowing grade, often blended with high impact extrusion grades.Applications: In blends with high impact Polystyrene or Styrolux; thermo.. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® WX-9120 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | ISO 306 |
Borealis FT5232 Low Density Polyethylene FT5232 is a Low Density Polyethylene for Film Extrusion. Tubular Technology. Includes medium slip additive and antioxidant. This grade is developed for the production of packaging film with good op.. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | ASTM D1525 |
PlastxWorld DAICEL STYROL® GH10 HIPS High heat resistance and flame retarded HIPS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | ASTM-D1525 |
Polyram BondyRam® 6000 Maleic Anhydride grafted Acrylonitrile-Butadiene-Styrene coupling agent Maleic Anhydride grafted Acrylonitrile-Butadiene-Styrene recommended as coupling agent in Styrene composites with glass or other minerals.Information provided by Polyram Ram On Ind. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | ASTM D3418 |
Westlake Tymax™ GA4402 Anhydride Modified Linear Low Density Polyethylene (Developmental Resin) Westlake GA4402 is an anhydride modified linear low density polyethylene designed for blown film extrusion that contains no slip and no antiblock additives. This resin is designed to function as a c.. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | 50°C/hr; 50N |
Arkema Group Orgalloy® LE 60ES03 Flexible Nylon Alloy (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents).higher in viscosity than LE 6000, suited to the blow molding of tec.. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | 49 N; ISO 306 |
A.D. Compound Adene NCTA Homopolymer 50% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Vicat Softening Point | 97.0 °C @Load 1.02 kg |
207 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem IJ33D LLDPE Injection Molding Polyethylene Copolymer IJ33D is a linear low-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high fluidity, excellent flexibi.. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL FP5140HF PPE+PS Noryl*FP5140HF is an unfilled, injection moldable modified polyphenylene ether resin with an ISO306 Vicat B/120 of 100 deg C. Designed for good dimensional stability and high flow, this resin also u.. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | 50°C/hr; 50N |
Arkema Group Oroglas® MI-7T Acrylic
(discontinued **) OROGLAS MI-7T is a medium impact grade combining excellent thermal resistance with good impact performance.Key features : impact resistance: up to 7 times more impact-resistant than standard acr.. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | 50°C/hr; 50N |
Polimeri Europa SINKRAL H220 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-09-25 General purpose, high flow injection moulding grade having good rigidity coupled with an excellent.. |
|||
Vicat Softening Point | 97.0 °C | 207 °F | 50°C/hr; 50N |
Polimeri Europa SINKRAL L320 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-25 General purpose, high flow injection moulding grade having good impact resistance coupled with an .. |