Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Minimum Service Temperature, Air = -20.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Recommended
Nye Lubricants 368AX-F (RL) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Recommended
Nye Lubricants 759X (NG) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Recommended
Nye Lubricants 794 (RL) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Recommended
Nye Lubricants 838G (FG) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
impact conditions and heavy loads not considered
Omnia Plastica ABS Acrylonitrile-butadiene-styrene
Acrylonitrile-butadiene-styrene is an amorphous thermopolymer used largely for injection moulded items. The stock shapes are mainly used for the production of prototypes.Features:Good machinability ..
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Precision Polymer Engineering V80B Fluoroelastomer Compound
Fluoroelastomer Rubber, 76-85 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M2HK814, A1-10, B37, B38, EF31, EO78, F15, Z1. Where Z1 = compressi..
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Precision Polymer Engineering V80G Fluoroelastomer Compound
Green Fluoroelastomer Rubber, 75-85 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK810, A1-10, B38, EF31, EO78, F15, Z1, Z2. Where Z1 = gre..
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Precision Polymer Engineering V80L Fluoroelastomer Compound
Special steam resistant, Fluoroelastomer Rubber, 75-85 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK810, A1-10, B38, EF31, EO78, F15, Z1...
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Precision Polymer Engineering V94E Fluoroelastomer Compound
Special steam resistant, Brown Fluoroelastomer Rubber, 85-95 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M3HK910, A1-10, B38, EF31, EO78, Z1..
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Precision Polymer Engineering Z85B Hydrogenated NBR Compound
Peroxide cured, Hydrogenated Nitrile Rubber, 76-85 °IRHD. Medium acrylonitrile content (ACN =36%). ASTM designation = HNBR. ASTM D2000 line call-out MDH814, A26, B36, EO16, EO36, F14.Applications..
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Quadrant EPP Ketron® CA30 LSG PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone (ASTM Product Data Sheet)
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Recommended
Nye Lubricants UniFlor 8612 (849) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
impact conditions and heavy loads not considered
Omnia Plastica Akulon® PET Arnite Omnialite
Arnite is a relatively new semi-crystalline polymer developed for technical applications. It is suitable for mechanical parts which require dimensional stability and a low friction coefficient. Omni..
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Precision Polymer Engineering V60K Fluoroelastomer Compound
Fluoroelastomer Rubber, 55-65 °IRHD. Terpolymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethylene. To meet ASTM D2000 line call-out: MHK610, A1-10, B37, B38, EF31, EO78. ASTM d..
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Polynorbornene Rubber (PNR)
High glass temperature - plasticizer needed to make a 'rubbery' compound.
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Freudenberg Simrit V169 Fluoroelastomer Self-Lube
Additives to elastomer compounds can improve the lubricity or non-stick performance of a seal. Specific compound ingredients may include fluoropolymer (TEFLON) additives, silicone additives or molyb..
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Freudenberg Simrit V174 Fluoroelastomer Self-Lube
Additives to elastomer compounds can improve the lubricity or non-stick performance of a seal. Specific compound ingredients may include fluoropolymer (TEFLON) additives, silicone additives or molyb..
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Continuous; DIN 52612
Isoflon PETP Polyethylene terephthalate
Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon.
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Trelleborg B600 Commercial Nitrile Rubber
Nitrile rubber or acrylonitrile-butadiene rubber is a copolymer of butadiene and acrylonitrile.PropertiesGood general resistance to oils.Good mechanical properties especially tensile strength, flexi..
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Trelleborg Emerson & Cuming Eccobond® 17 M 1 Heat Cure Catalyst
Emerson & Cuming 17 M 1 Eccobond® Heat Cure CatalystVery high temperature resistance, highest temperature strength, lowest shrink. Non-crystallizing. Long working life. Imparts excellent chemical r..
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
DSC
Adamas Adalon® 206 PTFE, 15/5% Glass/MoS2 Filled
Information provided by Adamas, HPM
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
CENTROPLAST CENTRODAL LF Polyoxymethylene conductive
This material is electrically conductive, with high mechanical strength and dimensional stability. Applications include structural components in potentially explosive areas, components for divertin..
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Recommended
Nye Lubricants 760K-MS (NG) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
CENTROPLAST CENTRODAL TF Polyoxymethylene + PTFE
This material is high strength and high heat strength dimensional stability. Applications include racks and annular gears, dimensionally accurate structural components for pumps, and housings and t..
Copyright © lookpolymers.com All Rights Reserved