Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Minimum Service Temperature, Air = -240 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -240 °C
-400 °F
Manifattura Cattaneo PTFE Polytetrafluoroethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Minimum Service Temperature, Air -240 °C
-400 °F
Manifattura Cattaneo RULON® W2 Polytetrafluoroethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Minimum Service Temperature, Air -240 °C
-400 °F
Garlock GRAPH-LOCK® 3124/3126 Graphite Sheet Gasketing, Steel Wire Insert
A laminated graphite sheet with a 316SS wire mesh insert.Pure exfoliated graphite flake material excels in extreme conditions, withstanding heat, pressure, and aggressive chemicalsProven fire-safeSe..
Minimum Service Temperature, Air -240 °C
-400 °F
Garlock GRAPH-LOCK® 3125TC Graphite Sheet Gasketing, Steel Insert
A laminated graphite sheet with a 316SS tang insert.Pure exfoliated graphite flake material excels in extreme conditions, withstanding heat, pressure, and aggressive chemicalsProven fire-safeSeals e..
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® GHC Standard Internal Combustion Laminate
GRAFOIL® Grade GHC is a laminate made from Grade GTC flexible graphite. Laminate Construction: GRAFOIL® Grade GTC ? Micro-thin, phenolic-based adhesive ? GRAFOIL® Grade GTC
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® GHE Standard Fluid Sealing Laminate, Metal Reinforced
GRAFOIL® Grade GHE laminate is made with GTB flexible graphite mechanically bonded to both faces of a 316 or 316L stainless steel tang metal insert. Surface identifiable, the laminate is branded ..
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® GHL Standard Fluid Sealing Grade GHL Laminate
GRAFOIL® Grade GHL is a laminate made with GRAFOIL® Grade GTB flexible graphite. Laminate thicknesses > 0.060" will be adhesively bonded to final thickness. Laminate thicknesses
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® GHN Standard Fluid Sealing Laminate, Non-Metal Reinforced
GRAFOIL® Grade GHN is an unbranded laminate made with GRAFOIL® Grade TG-337 flexible graphite, thermally bonded to both faces of a plastic insert. It is not certified to any industry standards..
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® GTA Standard Fluid Sealing Graphite Single Layer Gasketing Material
GRAFOIL® GTA premium flexible graphite is a non-inhibited grade developed for use in nuclear or semiconductor applications. It is certified to meet the most rigorous purity specifications of the ..
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® GTB Standard Fluid Sealing Graphite Single Layer Gasketing Material
GRAFOIL® GTB flexible graphite sheet is a gasketing material containing no binders or fillers. Standard industrial grade GTB flexible graphite has an oxidation/corrosion inhibitor and is typicall..
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® GTJ Standard Fluid Sealing Graphite, Single Layer Material
GRAFOIL® GTJ premium flexible graphite is an oxidation/corrosion inhibited grade developed for use in nuclear and high temp, high purity applications. It is certified to meet the most rigorous pu..
Minimum Service Temperature, Air -240 °C
-400 °F
GrafTech GRAFOIL® SUPER GTO® Standard Internal Combustion Single Layer Gasketing Material
GRAFOIL® SUPER GTO® flexible graphite sheet is a gasketing material containing no binders, which will seal a wide variety of liquids and gases over an extremely large temperature range (-240Â..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Norton® Fluorglas® Chemfilm® DF1400 Non-Conductive PTFE Tape
Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Norton® Fluorglas® Chemfilm® DF1900 Heat Bondable PTFE Film
Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super..
Minimum Service Temperature, Air -240 °C
-400 °F
Embrittlement Temp
Saint-Gobain Rulon® 125 Bearing/Seal PTFE
Rulon 125 is used primarily in applications that are not severe such as dryer drum slides and piston rings in pneumatic or hydraulic controls.Information provided by distributor TriStar Plastics Cor..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Rulon® 1337 Bearing/Seal PTFE
Rulon® 1337 is a tan material made entirely from FDA compliant components. It has excellent physical properties and is chemically compatible with most chemicals, except concentrated sulfuric acid..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Rulon® 1439 Bearing/Seal PTFE
Rulon® 1439 is a white FDA compliant material that is suitable for immersed service with better wear characteristics than most other PTFE compounds. Its color makes it aesthetically pleasing for ..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Rulon® 488 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Minimum Service Temperature, Air -240 °C
-400 °F
Embrittlement Temp
Saint-Gobain Rulon® AMR Bearing/Seal PTFE
Same base material as Rulon AR but Rulon AMR contains a percentage of molybdenum disulfide for increased wear resistance and lower coefficient of friction. Typically used as a seal or gasket, Rulon ..
Minimum Service Temperature, Air -240 °C
-400 °F
Embrittlement Temp
Saint-Gobain Rulon® DC1042 Bearing/Seal PTFE
Can be used in a wide range of sealing and bearing applications. Rulon DC1042 is ideal for applications in which the bearing, seal is in contact with harsh chemicals or in applications where electri..
Minimum Service Temperature, Air -240 °C
-400 °F
Embrittlement Temp
Saint-Gobain Rulon® DC7035 Bearing/Seal PTFE
Offers electrical conductivity in a low wear, self lubricating bearing material. This material is ideal in applications where static dissipation is needed. DC7035 is often used as a static bleed mec..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Rulon® F Grade Bearing/Seal PTFE
F Grade Bearing/Seal PTFE is used for applications requiring a long wearing material, especially in dry applications and those requiring high abrasion resistance. Standard tape liner material for Ru..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Rulon® LR Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Rulon® W2 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Rulon® XL Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Norton® Fluorglas® Chemfilm® DF2919 Fluoropolymer Tape
Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super..
Minimum Service Temperature, Air -240 °C
-400 °F
Saint-Gobain Norton® Fluorglas® Chemfilm® DF2929 Fluoropolymer Tape
Description: Chemfilm® Fluoropolymer Cast Films and Tapes for Wire and Cable Industry: Multi-layer cast film process ensures inherently pin-hole free structure, therefore cast films possess super..
Minimum Service Temperature, Air -240 °C
-400 °F
Embrittlement Temp
TriStar Ultracomp UC-400 Composite Bearing
Ultracomp UC-400 - Designed for high loads, low speeds, impact and vibration applications. UC-400 has a MOS2 additive for salt water applications where cathodic reactions could occur. Excellent dry ..
Minimum Service Temperature, Air -240 °C
-400 °F
Embrittlement Temp
TriStar Ultracomp UC-500 Composite Bearing
Ultracomp UC-500 - Multiple sources of lubrication make this Ultracomp an excellent choice for full rotary or higher speed linear applications. High strength, high impact resistance and long wear li..
Minimum Service Temperature, Air -240 °C
-400 °F
Chesterton Valvelon® 3500 PTFE Sealant
Description: Chesterton® 3500 Valvelon® is a dense, pure PTFE sealant that can be used as a non-hardening valve packing or flange gasket. The unique construction of the product allows it to squeez..
Copyright © lookpolymers.com All Rights Reserved