Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Minimum Service Temperature, Air = -30.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Recommended
Nye Lubricants 1252 Grease
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Recommended
Nye Lubricants 185D (SO) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Recommended
Nye Lubricants 334 (SO) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Recommended
Nye Lubricants 570H-10 (NT) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Recommended
Nye Lubricants 570H-25 (NT) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Recommended
Nye Lubricants 752 (NG) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Recommended
Nye Lubricants 774F-MS (NG) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Recommended
Nye Lubricants 782LC (NG) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Recommended
Nye Lubricants 824A-1 (FG) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
impact conditions and heavy loads not considered (dry sample)
Omnia Plastica Omniamid PA6 GHR - HR - at 50% RH
Cast nylon 6 produced with the addition of graphite and a special lubricator which gives to this product better properties than natural PA6G. Whilst retaining the general features of OMNIAMID G it i..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Precision Polymer Engineering N50C Nitrile Rubber
Nitrile Butadiene Rubber, 45-55 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet British Gas Specification BGC/PS/LC6 Class B, approval ref.: 67/6.11.iv. M..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Precision Polymer Engineering Q65B Polyurethane Rubber
Sulphur cured, Polyurethane Rubber, 55-65 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG621, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resist..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Manifattura Cattaneo PA 6.6 Nylon
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Greene Tweed CHEMRAZ® 517 Perfluoroelastomer
Greene Tweed’s Chemraz® 517, a perfluoroelastomer, is a white specialty compound, perfect for applications where contamination from carbon black must be prevented. Chemraz 517 has a Shore A..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Greene Tweed CHEMRAZ® 585 Perfluoroelastomer
Chemraz® 585, a perfluoroelastomer, is a specialty cream compound formulated to outlast the most demanding chemical process applications. With its outstanding overall chemical resistance, Chemra..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Greene Tweed CHEMRAZ® 520 Perfluoroelastomer
Chemraz® 520 is recommended for a wide variety of semiconductor equipment dry processing applications where seal reliability with minimal contaminations is required. Additionally, Chemraz 520 of..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Gehman T100
Zeon Chemicals HyTemp® PV-04 AR Polyacrylate Elastomer
HyTemp PV-04 contains one or more acrylic esters. This polymer is specific to the peroxide vulcanized cure system.Peroxide curable elastomer suitable for O-rings, seals, and gaskets. Also used for b..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Trelleborg Neoprene® C627 Chloroprene
CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Trelleborg Neoprene® C626 Chloroprene
CR or Chloroprene is a homopolymer of chloroprene or chlorobutadiene. NEOPRENE®PropertiesExcellent mechanical and abrasion properties even without reinforcing fillers.Reasonable resilience in grade..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Trelleborg R525 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Donnelly Bros HT 250 High Temperature Mold Grease
Off white, smooth appearance. Works well in constant metal temperature of 200° F to 250° F. (Note: The plastic molding material itself might be >600° F.)A stiff, silica thickened, medium viscos..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
ASTM D 3575
Eurofoam Evacell EVA 30 EVA + PE Foam
Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Dura-Bar 60-40-18 Continuously Cast Ductile Iron Bar Stock ASTM A536, 4018
Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Dura-Bar 80-55-06 Continuously Cast Ductile Iron Bar Stock ASTM A536
Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Bond Laminates TEPEX® dynalite 102-RG600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate
Within the TEPEX® composite laminate, Polyamide 6 is a resin known for its toughness, stiffness, abrasion resistance, heat and chemical resistances. Roving E-Glass fibers have an excellent impact ..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Biomer P226 PHB Biodegradable Polymer
PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Brittleness Temperature
DuPont Performance Polymers Hypalon® 30 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound  (d
Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato..
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
CENTROPLAST CENTROMID 6.6 Polyamide 6.6
This material has good hardness, wear resistance, abrasion strength and impact strength. It is used for bearing cages, sliding bearings and articulated joint blocks.Information provided by CENTROPL..
Copyright © lookpolymers.com All Rights Reserved