| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
Resinlab® EP1285HD-12 Highly Filled, Medium Viscosity Casting Resin
Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Recommended |
|
Nye Lubricants 380C (RL) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Recommended |
|
Nye Lubricants 774F-1 (NG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Recommended |
|
Nye Lubricants UniFlor 8771 (UF) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Temperature at which modulus shall not exceed 70 Mpa |
|
Precision Polymer Engineering F80R Fluorosilicone Rubber
Red Fluorosilicone, 76-85 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification DTD5583A Grade 80.Applications:
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
Precision Polymer Engineering H60B Epichlorohydrin
Peroxide Cured, Epichlorohydrin Rubber, 55-65 °IRHD. Terpolymer of epichlorohydrin, ethylene oxide and an unsaturated monomer. To ASTM D2000 line call-out: M3CH608, A25, B14, EO16, EO36, F17. AS..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
Termopol Termoton® K4GA4070A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
Termopol Termoton® V2GA1065A TPV Compound
Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;..
|
|||
| Minimum Service Temperature, Air | <= -50.0 °C | <= -58.0 °F | |
|
Kazanorgsintez 158BK-20 Low Density Polyethylene Composite
Production Method: Produced from low density polyethylene grades 15803-020 and 15813-020. Application: Designed for production of sealing coatings on industrial items.Information Provided by Kaz..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Retains Stretch |
|
Freudenberg Simrit 92 AU 21100 Low Temperature Polyurethane Elastomer
With the new low temperature material 92 AU 21100, Simrit has succeeded in developing a polyurethane material that is specially designed to meet the specific requirements for use at low temperatures..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
GEHR Plastics PE-HD Polyethylene HDPE
Polyethylene has a good chemical resistance against almost all acids and bases, detergents and hot water. PE has good insulation properties and is easy to weld. The operating temperature is from -50..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
GEHR Plastics PPSU Polyphenylenesulfone
Polyphenylenesulfone is an amorphous material, with improved impact and hydrolysis resistance compared to PSU. The usual operating temperature is approximately 180°C. The extremely high notched i..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Continuous; DIN 52612 |
|
Isoflon PEHD 300 High Density Polyethylene
Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon.
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Continuous; DIN 52612 |
|
Isoflon POM C Polyacetal C
Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon.
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | Continuous useful temperature. |
|
Momentive Performance Materials RTV6166 Clear Potting/Encapsulating Gel
Two-part addition cure. Two-part addition cure RTV silicones can be cured very quickly with the use of high heat. Addition cure products have no cure by-products and can be used to unlimited depth..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
Seals Eastern 7346 Extreme Low Temperature Service Rubber
HNBR for cold temp (-50°C) and/or aqueous serviceInformation provided by Seals Eastern.
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
Dow Corning MOLYKOTE® G-2001
Lithium thickened bearing grease based on synthetic hydrocarbonInformation provided by Dow Corning
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
ELASTO UK Dryflex® 500500S SEBS Based Material, Unfilled Qualities, 50A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
ELASTO UK Dryflex® 500900S SEBS Based Material, Unfilled Qualities, 90A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
ELASTO UK Dryflex® 502400S SEBS Based Material, Unfilled Qualities, 40A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
ELASTO UK Dryflex® 502900S SEBS Based Material, Unfilled Qualities, 90A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
ELASTO UK Dryflex® 600900S SEBS Based Material, Filled Qualities, 90A Hardness, Natural
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
ELASTO UK Dryflex® 602650S SEBS Based Material, Filled Qualities, 65A Hardness, Black
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
ELASTO UK Dryflex® 662800S SEBS Based Material, Semi-Filled Qualities, 80A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
ELASTO UK Dryflex® 662900S SEBS Based Material, Semi-Filled Qualities, 90A Hardness, Black
The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
ELASTO UK Dryflex® 600450S SEBS Based Material, Filled Qualities, 45A Hardness, Natural
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | DSC |
|
Adamas Adalon® 808 PTFE, Bronze + PEEK+ Carbon Fiber
Information provided by Adamas, HPM
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
Atom Adhesives AA-DUCT 906 Epoxy Adhesive
AA-DUCT 906 represents the newest technology since the introduction of electrically conductive silver compounds. This unique formulation is based on a silver coated ceramic that results in lower mat..
|
|||
| Minimum Service Temperature, Air | -50.0 °C | -58.0 °F | |
|
GEHR Plastics Noryl PPO
(discontinued **)
PPO belongs to the group of the amorphous materials and can be used in temperatures ranging from -58 °F to +302 °F. PPO exhibits a high impact strength and a very high dimensional stability. The e..
|
|||