Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Minimum Service Temperature, Air = -53.9 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
ND Industries 226 Structural Adhesive
Light Cure Structural Adhesive gel
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
ND Industries StudGrade® 131 Permanent CT Threadlocker
General DescriptionHigh strength threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical Usesstuds and bolts, and threaded pipe fittings.Meets m..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Cured State
Palm Labs Adhesives Turbo Fuse Series 110 (5 Viscosity) Rapid Bonding Adhesive
Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 110 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Cured State
Palm Labs Adhesives TURBO FUSE SERIES 110 MEDICAL DEVICES APPROVED (100 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130 - MEDICAL DEVICES APPROVED advanced formula is designed to polymerize instantly by absorbing surface moistur..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Cured State
Palm Labs Adhesives TURBO FUSE SERIES 160 LOW ODOR/LOW BLOOM (1000 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 160 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Permabond HH190 Anaerobic Gasketmaker
Permabond® HH190 Gasketmaker is an anaerobic curing flange sealant that can replace, or be used as a dressing for, conventional pre-cut gaskets. Since HH190 is a flowable paste, it conforms to the ..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Permabond HM161 Anaerobic Retaining Compound
Permabond® HM161 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space’ between parts and upon cure unitiz..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Resinlab® CYNERGY CA6206 Adhesive
Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Permabond TA440 Toughened Acrylic Adhesive
PERMABOND TA440 is a two component structural acrylic adhesive suitable for bonding metals, glass, wood, ferrites, ceramics and some rigid plastics. This adhesive may be used in a variety of structu..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Resinlab® CYNERGY CA6401 Adhesive
Description: The CYNERGY 6400 SERIES are clear, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Continuous
Dielectric Polymers NT-141PLT Double Liner Tape  (discontinued **)
Acrylic adhesive with moisture stable PE coated kraft base release and high density PE interliner.Features: Clear releases liner allows easy inspection of back lighted panelsPlasticizer migration re..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Resinlab® CYNERGY CA6603 Adhesive
Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a ..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Saint-Gobain COHRlastic® 1025 General-Purpose Electrical-Grade Silicone Coated Fabric
Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Master Bond MasterSil 153Med Silicone Paste for Medical Applications
Description: Master Bond MasterSil 153Med is a two component silicone compound with a paste consistency for high performance bonding and sealing. It can be used for medical device applications as it..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Loctite® 3104 Acrylic Light Cure Adhesive
Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Loctite® 349 Acrylic Light Cure Adhesive
Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Loctite® 222 Threadlocker
ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Loctite® 3381 Light Cure Acrylic Adhesive
Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Loctite® 3526 Acrylic Light Cure Adhesive
Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Loctite® 392 Rapid Fixture Structural Adhesive
Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. ..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Loctite® 499 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Loctite® 635 High Strength/Slow Cure Retaining Compound
RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. ..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Loctite® Depend© 330 Acrylic Bonding Adhesive
Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. ..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Loctite® PRISM® 454 Instant Adhesive Gel
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Cytec CE-1171 (Conap) Acrylic Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Cytec Conathane® CE-1175 (Conap) Polyurethane Dielectric Conformal Coating
Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Armstrong A-7 Epoxy Adhesive
Clear, flexible, 5-minute cure structural bonding plastic adhesive. Develops high performance, high impact durable bonds for operating temperatures from -65° to +250°. Supplied in 1:1 ratio dispe..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Loctite® 574 Semi-rigid Cure Anaerobic Sealant
Anaerobic GasketingLoctite® 574 Semi-rigid Cure Anaerobic SealantRecommended Primer: 7649 (N). Typical Use: Fast curing, large gaps
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Loctite® 620 High Temperature Retaining Compound
RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. ..
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Loctite® 661 Retaining Compound
RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. ..
Copyright © lookpolymers.com All Rights Reserved