Polymer Property : Minimum Service Temperature, Air = -60.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Resinlab® AR 4305 Metal Bonding Methacrylate Adhesive
Resinlab™ AR 4305 is a 1:1 mix methacrylate-based structural adhesive designed for general purpose bonding of a wide variety of materials in industrial applications. AR 4305 forms tough, durable bo..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Dielectric Polymers NT-4511 High Temperature Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing of silicone coated paper and film. For applicati..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Dielectric Polymers NT-2012-2 Photo Processing Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing photographic film to leader card during film proc..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Dielectric Polymers NT-5521-2 Photo Processing Tape  (discontinued **)
Crosslinked silicone adhesive with polyester film backing.Features: Chemical resistantTemperature resistantGood conformabilityApplications: Splicing photographic film to leader card during film proc..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Approx. Cold test
Lubriplate 5555 Anhydrous Calcium Grease For Special Applications / Conditions
This anhydrous calcium, semi-fluid type lubricant is made for automatic lubricating systems operating in cold temperatures. Applications: Automatic lube systems, light oil, cold temps. No. 5555 is a..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Master Bond EP15 High Tensile Strength One Component Epoxy
Master Bond Polymer System EP15 is a one component, heat curing epoxy featuring high tensile strength utilized in testing the adhesion and/or cohesive strength of flame-sprayed coatings. This standa..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Master Bond EP21ARHTND Two component epoxy adhesive, sealant, coating and encapsulating system
Product Description: Master Bond EP21ARHTND is a two component epoxy resin system for high performance bonding, sealing and coating. It has a convenient 100 to 50 mix ratio by weight and is formulat..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Master Bond EP39-2 Fast Curing Optically Clear Two Component Epoxy System
Master Bond Polymer System EP39-2 is a fast curing, low viscosity, optically clear two component epoxy system for high performance bonding, sealing, coating and casting. It is 100% reactive and does..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Master Bond EP51HT Fast Curing High Temperature Resistant Epoxy Adhesive
Master Bond Polymer Adhesive EP51HT represents a significant advance in epoxy adhesive technology featuring an excellent balance of performance properties, including convenient curing at ambient tem..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Master Bond EP65HT Fast Setting Epoxy Resists High Temperatures
Description: Master Bond EP65HT represents a highly innovative advance in epoxy technology in that it features the unusual combination of very fast cures and high temperature resistance. While typic..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Master Bond LED403Med USP Class VI, One Component, LED Curable System
Master Bond LED403Med is a one part LED system that cures fully upon exposure to a 405 nm wavelength light that is generated by an LED source and. In fact, this material will fully cure tack-free wi..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Master Bond MB295 Cyanoacrylate Adhesive System
Master Bond Polymer System MB295 is an ethyl cyanoacrylate adhesive system, recommended for use for combinations of plastics, lubber, ceramic or glass. Provides better general resistance to effects ..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Master Bond MB302 Cyanoacrylate Adhesive System
For rubber & plastic bonding, fills gap to 0.005Information provided by Master Bond Inc.
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Master Bond UV15 High Strength UV Curable Adhesive System
Master Bond UV15 is a high strength, low viscosity, epoxy based UV curable system for bonding, sealing and coating. It is 100% reactive and does not contain any solvents or other volatiles. It is al..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Master Bond EP21LV Low Viscosity Two Component Epoxy
Master Bond Polymer System EP21LV is a two component, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting. It is formulated to cure readily at ..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Master Bond EP30LV Optically Clear, Low Viscosity Epoxy Adhesive
Description: Master Bond Polymer System EP30LV is a low viscosity, two component epoxy adhesive for general purpose bonding, coating, sealing and casting formulated to cure at room temperature or mo..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Master Bond EP30M3LV Electrically Insulative, Low Viscosity Two Component Epoxy
Master Bond Polymer System EP30M3LV is a lower viscosity, two component epoxy system for high performance bonding, sealing and encapsulation. It is formulated to cure at ambient temperatures or mor..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Master Bond EP34AO Epoxy Compound Withstands High Temperatures
Description: Master Bond Polymer System EP34AO is a room temperature curing, two component epoxy compound for high temperature bonding and sealing applications especially where thermal conductivity ..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Master Bond UV10TK Dimensionally Stable One Component UV Curable Adhesive
Master Bond UV10TK is a moderate viscosity, one part UV system for bonding, sealing and coating featuring very good optical clarity and excellent physical properties as well as superior temperature ..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Arlon 910-10RXX-P0 0.010" (0.254 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Arlon 930-125Rxx-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Arlon HS930-10R##-P4 0.030" (0.762 mm) Self-Fusing Silicone Tape (Rectangular, Unsupported)
Description: High Strength, 1 inch wide, 30 mil thick, Red, Rectangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicat..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Arlon LW3015B##-P0 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1.5 inch wide, 30 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll leng..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Arlon LW301CxxFR-P0 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 30 mil thick, Brown, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Arlon LW401R##-P2 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Red, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length i..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Arlon Thermabond® 99180T010 Silicone Rubber/Fiberglass Laminate
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Arlon 920-15Rxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape
Design/Construction:Cross Section Type: RectangularWidth, inches: 1.5Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Arlon T2030-R004-12 0.030" Cured Self-Fusing Silicone Rubber Tape
1 inch wide, 30 mil thick, 12.0 yards long, red, triangular cross-section, self-fusing silicone tape.Design/Construction:Interleave: 1 mil PETProduct: Cured Silicone Self-fusing RubberCross-section..
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Master Bond EP21TP-2 Oil And Fuel Resistant Polysulfide Based Adhesive System
Master Bond Polymer Adhesive EP21TP-2 is a two component polysulfide/epoxy based adhesive/sealant formulated to cure at room temperature or more rapidly at elevated temperatures, with a 1 to 1 mix r..