Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Minimum Service Temperature, Air = -65.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Recommended
Nye Lubricants 572H-10 Dispersion
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Recommended
Nye Lubricants 719G (RL) Rheolube Grease
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Non-brittle after 3 minutes
Precision Polymer Engineering S50D Silicone Rubber
Black Silicone Rubber, 46-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated to meet UK Ministry of Defence Aircraft Materials Specificatio..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Precision Polymer Engineering S50N Silicone Rubber
Silicone Rubber, 45-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ. To meet UK Ministry of Defence Aircraft Materials ..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Precision Polymer Engineering S60N Silicone Rubber
Red Silicone Rubber, 56-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aircraft Materials Specification DTD5582A Gr..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Non-brittle after 3 minutes
Precision Polymer Engineering S80D Silicone Rubber
Black Silicone Rubber, 76-85 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. ASTM & ISO designation = VMQ. Formulated to meet UK Ministry of Defence ..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
NextGen Adhesives G907-25 Optical Epoxy Adhesive
Description: NGAC G907-25 is a low viscosity and clear adhesive system that is specifically formulated for optical and laser applications.Advantages and Applications: The NGAC G907-25 provides high ..
Minimum Service Temperature, Air >= -65.0 °C
>= -85.0 °F
Low Temp Flex - Reinforced Material, TR10
Parker Chomerics CHO-SEAL 1285R Reinforced Conductive Elastomer Seal
These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Parker Chomerics CHO-SHIELD® 610 A/B Conductive Epoxy Paint
Highly Conductive Epoxy Paint. This is a two-component, silver plated, copper-filled, highly conductive epoxy paint. This coating was developed for application to non-conductive plastic substrates t..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Resin Technology Group 301 Plastics, Wicking Grade Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Resin Technology Group 301 Plastics, Wicking Grade Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Resin Technology Group 310 Porous Fill, Slow Set Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Resin Technology Group 310 Porous Fill, Slow Set Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Resin Technology Group 395 Plastics, Large Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Resin Technology Group 395 Plastics, Large Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Resin Technology Group 85 Metal Bonder Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Resin Technology Group 85 Metal Bonder Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Brittleness Temperature
DuPont Performance Polymers Hypalon® 45 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound  (d
Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Recommended
Nye Lubricants UniFlor 8920U (491UV) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -65.0 - -30.0 °C
-85.0 - -22.0 °F
Average value: -52.0 °C Grade Count:48
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Humiseal 1A27 Urethane Conformal Coating
Humiseal 1A27 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedPasses thermal shock test (MIL-I-46058C)Flammabilit..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Humiseal 1C55 Silicone Conformal Coating
Humiseal 1C55 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock ..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Trelleborg Emerson & Cuming Eccobond® 24 Two-Component High Strength-Impact Resistant Epoxy Adhesive
Emerson & Cuming 24 Eccobond® Two-Component High Strength-Impact Resistant Epoxy AdhesiveClear, low viscosity, room temperature curing, epoxy adhesive. Exhibits resilient bonds when joining dissimi..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Trelleborg Emerson & Cuming Stycast® 2651-40/23LV Two-Component General Purpose Encapsulant
Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as ..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Trelleborg Emerson & Cuming Stycast® 4952/25 Two-Component Silicone High Service Temp Encapsulant
Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Dow Corning 737 NEUTRAL CURE SEALANT
RTV adhesive/sealant with primerless adhesion to most materialsInformation provided by Dow Corning
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Cytec EN-2541 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Cytec EN-2550 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Aremco Aremco-Bond™ 631 High Performance Epoxide
Clear-Amber, 1:1, Good Bond Strength and Corrosion Resistance.Also available filled with aluminum oxide (Alumina) or pigments.
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Recommended
Nye Lubricants 761 (NG) Synthetic Oil
Information provided by Nye Lubricants.
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Parker Chomerics CHO-SHIELD® 2002 Conductive Coating
Electrically conductive coatings provide corrosion protection for enclosure flanges which mate with EMI shielding gaskets. They can also provide a corrosion resistant conductive surface coating on a..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Resinlab® RC8009 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Resinlab® RC8035 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Resinlab® RC8080 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
Copyright © lookpolymers.com All Rights Reserved