Thermal Properties Metric English Comments
Minimum Service Temperature, Air -70.0 - -20.0 °C
-94.0 - -4.00 °F
Average value: -55.4 °C Grade Count:17
Overview of materials for Silicone Foam
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW..
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Freudenberg Simrit SC1217 S317 Silicone Elastomer
Excellent material for static service at extreme (hot or cold) temperatures. Outstanding flex and fatigue life. Very good for ozone and UV radiation service as well as for resistance to fungal and b..
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Isoflon Tisoflon® 6S Silicone Coated Glass Fabric
Silicone coated Glass fabric TISOFLON®Information provided by Isoflon.
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Continuous; DIN 52612
Isoflon PUR Polyurethane
Very high wear resistanceHighly resilientInformation provided by Isoflon.
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Zotefoams Plastazote® LD24MC Low Density Polyethylene Foam, Medium Cell
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Zotefoams Plastazote® LD33 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Tra-Con Tra-Bond 716C01 Medium Viscosity Epoxy Adhesive
TRA-BOND 716C01 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications. This two-part amber adhesive is easily mixed, used and cured at room temperature..
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Tra-Con Tra-Bond FDA12 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA12 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Admin..
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Tra-Con Tra-Cast 3010 Flexible Clear Epoxy Casting Compound
TRA-CAST 3010 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties, good clarity, long pot life..
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Trelleborg S662 Silicone Rubber
PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering...
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Goodfellow Polyvinyl Fluoride (PVF) Film
A semi-crystalline, colorless, transparent-translucent fluoropolymer with excellent weathering resistance, good chemical resistance and low permeability to gases; it is very slow burning and has a v..
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Trelleborg S665 Silicone Rubber
PropertiesExcellent resistance to heat (dry air), at +200°C continuous and +220°C intermittent.Remains flexible at low temperatures of -70°C.Resistant to ultra-violet light, ozone and weathering...
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Zotefoams Plastazote® HD115 High Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Zotefoams Plastazote® LD50CN Conductive Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Zotefoams Plastazote® MP45 Metallocene Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Dow Corning FLUOROGEL® Q3-6679 DIELECTRIC GEL KIT
Two-part, clear, RT or heat cure, solvent and fuel resistant.Information provided by Dow Corning
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
ASTM D 3575
Eurofoam Polycell PLZ 45 Polyethylene Foam
Information provided by Eurofoam s.r.l.
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Atom Adhesives AA-BOND 2110 Epoxy Adhesive
AA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, no..
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Atom Adhesives AA-BOND FDA2T Epoxy Adhesive
AA-BOND FDA2T is a thixotropic epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and received ..
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
3M 4014/Silver Damping Foils
Foil/foam sheet laminateInformation provided by 3M
Copyright © lookpolymers.com All Rights Reserved