| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Garlock 502 Silicone Sheet Rubber
Style #502 will be used in sealing applications that require resistance to extreme temperatures, high ozone concentrations, and high ultraviolet content.Information provided by Garlock Rubber Techno..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Master Bond Mastersil 150 Two Part, Condensation Cured, Flexible Silicone
Master Sil 150 is a 2 part condensation cured liquid silicone which, after the addition of curing agent 150, cures at room temperature to a tough, resilient silicone rubber potting and encapsulation..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Master Bond Mastersil 151 Two Component Low Viscosity Silicone Compound
Master Bond MasterSil 151 is a two component, low viscosity
silicone compound for high performance potting and
encapsulation. MasterSil 151 is an addition cured system and does not require exposure..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Master Bond Mastersil 153 Two Component, High Temperature Resistance Silicone Adhesive
Master Bond MasterSil 153 is a two component, paste silicone compound for high performance bonding and sealing. MasterSil 153 is an addition cured system and does not require exposure to air for com..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Master Bond Mastersil 410 One Component Room Temperature Curing Silicon
Master Bond MasterSil 410 is a ready-to-use, one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. This compound has a pas..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Master Bond Mastersil 700 One Component High Temperature Resistant Silicon
Master Bond MasterSil 700 is a ready-to-use, one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. It remains flexible and..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Master Bond Mastersil 701 One Component, Room Temperature Curing Silicone Elastomer
Master Bond Master Sil 701 is a ready-to-use, one component, high performance silicone elastomer compound for bonding, and sealing protective coatings and formed-in-place gaskets. It cures at ambien..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Master Bond Mastersil 702 One Component, Room Temperature Curing Silicone Elastomer
Master Bond Master Sil 702 is ready-to-use, one component high performance silicone elastomer compound for bonding and sealing. Master Sil 702 is heat resistant to 450°F. It is supplied as an easy ..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Master Bond Mastersil 705 One Component Room Temperature Curing Silicon Elastomer
Master Bond Master Sil 705 is a one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. This material is a translucent nonco..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Master Bond MasterSil 709 One Part Silicone Meets MIL Spec
Description: MasterSil 709 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This unique product meets the MIL..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Master Bond MasterSil 710 Silicone Paste Meets MIL Spec
Description: MasterSil 710 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This product meets the Meets MIL-..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Master Bond Mastersil 711 Fast Curing One Component Silicone
MasterSil 711 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This specialty product features an exceptional..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Master Bond Mastersil 713 Low Viscosity One Component Silicone
Master Sil 713 is a ready-to use, exceptionally low viscosity, one component high performance silicone elastomer compound for bonding, sealing, protective coatings and formed-in-place gaskets. This ..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Master Bond Mastersil 773 Fast Curing Low Viscosity Silicone
Master Bond MasterSil 773 is a ready-to-use one component ultra-low viscosity silicone elastomer based conformal coating which provides excellent protection to electronic circuitry in high humidity ..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Master Bond Mastersil 800 One Component, Room Temperature Curing Silicone
MasterSil 800 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed-in-place gaskets. This specialty system features ultra high temp..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Master Bond Mastersil 801 One Component, Room Temperature Curing, Silicone System
MasterSil 801 is an easy to use, one component, high performance silicone elastomer compound. MasterSil 801 features non-corrosive cure and serviceability up to 300°C; it exhibits good stability at..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Dura-Bar G2 Continuously Cast Gray Iron Bar Stock ASTM A48
Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as an alternative to gray i..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Abatron L060330-2 Flexible Polyurea Compound
L060330-2 is used for castings, repairs, assemblies, coatings, and laminations that require fast hardening. It is also used for bonding most rigid materials such as metals, aluminum, copper, china, ..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
Abatron L060421-1 Heat-Resistant (-75~400°F) Non-Flammable Silicone Rubber
L060421-1 is a heat-resistant and non-flammable silicone rubber recommended as a potting compound for exceptional protection against thermal shock, vibration, moisture, ozone, dust, chemicals, and o..
|
|||
| Minimum Service Temperature, Air | -59.4 °C | -75.0 °F | |
|
BCC Products BC 9060 Silicone RTV Rubber
BC 9060 is a blue colored, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high strength and high..
|
|||