| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
|
Nye Lubricants 371B (RL) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
|
Nye Lubricants 5301 (SVLG) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
|
Nye Lubricants 719G (RL) Rheolube Grease
Information provided by Nye Lubricants.
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
|
Nye Lubricants UniFlor 8921 (892-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
|
Nye Lubricants UniFlor 8981 (899-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
|
Nye Lubricants UniFlor 8981SR (899S-1-RP) (UF) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Precision Polymer Engineering F80R Fluorosilicone Rubber
Red Fluorosilicone, 76-85 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification DTD5583A Grade 80.Applications:
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Precision Polymer Engineering S50D Silicone Rubber
Black Silicone Rubber, 46-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated to meet UK Ministry of Defence Aircraft Materials Specificatio..
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Non-brittle after 3 minutes |
|
Precision Polymer Engineering S50D Silicone Rubber
Black Silicone Rubber, 46-55 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Formulated to meet UK Ministry of Defence Aircraft Materials Specificatio..
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Precision Polymer Engineering S60N Silicone Rubber
Red Silicone Rubber, 56-65 °IRHD. Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aircraft Materials Specification DTD5582A Gr..
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
NextGen Adhesives G907-32 Structural Adhesive
Description: NGAC G907-32 is a thixotropic, epoxy adhesive system utilized extensively in staking, as well as, other industrial and structural applications.Advantages and Applications: The NGAC G907..
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Resin Technology Group 370 Wire Tacking Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Resin Technology Group 370 Wire Tacking Fusion™ Cyanoacrylate Instant Ethyl Adhesive
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Resin Technology Group 388 Metals, Small Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Resin Technology Group 388 Metals, Small Gap Fill Fusion™ Cyanoacrylate Instant Ethyl Adhesive
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Resin Technology Group 390 Surface Insensitive Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Resin Technology Group 390 Surface Insensitive Fusion™ Cyanoacrylate Instant Ethyl Adhesive
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Resin Technology Group 60 Low Odor, Low Bloom Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Resin Technology Group 60 Low Odor, Low Bloom Fusion™ Cyanoacrylate Instant Ethyl Adhesive
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Resin Technology Group 85 Metal Bonder Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Resin Technology Group 85 Metal Bonder Fusion™ Cyanoacrylate Instant Ethyl Adhesive
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Resinlab® RC8038 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Resinlab® RC8041 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Resinlab® RC8060 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Resinlab® RC8075 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Humiseal 1A33 Urethane Conformal Coating
Humiseal 1A33 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL..
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Humiseal 1C61 UV Cure Conformal Coating
Humiseal 1C61 UV Cure Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock t..
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Humiseal 2A64 Urethane Conformal Coating
Humiseal 2A64 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-46058C)F..
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Tra-Con Tra-Bond 813J01 Silicone Encapsulant
TRA-BOND 813J01 is a silicone adhesive system formulated to provide excellent thermal conductivity. This unique product bonds well to difficult substrates. Typical applications include encapsulation..
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Dow Corning 737 NEUTRAL CURE SEALANT
RTV adhesive/sealant with primerless adhesion to most materialsInformation provided by Dow Corning
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Cytec EN-2550 (Conap) Potting and Encapsulation Adhesive
Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s..
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Aremco Aremco-Bond™ 631 High Performance Epoxide
Clear-Amber, 1:1, Good Bond Strength and Corrosion Resistance.Also available filled with aluminum oxide (Alumina) or pigments.
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
|
Nye Lubricants UniFlor 8921R (892RP-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
|
|||
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | |
|
Resinlab® RC8009 Anaerobic Retaining Compound
The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products ..
|
|||
| Minimum Service Temperature, Air | -65.0 - 2.22 °C | -85.0 - 36.0 °F | Average value: -20.0 °C Grade Count:299 |
|
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..
|
|||