| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
|
Chesterton 601 Chain Drive Pin & Bushing Lubricant
Description: Chesterton® 601 Chain Drive Pin & Bushing Lubricant is and has been the premium quality light lubricant of choice in industry for over thirty years. This superior lubricant was special..
|
|||
| Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
|
Chesterton 622 White Grease
Description: Chesterton® 622 White Grease is a pure mineral oil grease with PTFE added designed for applications where a clean, nonstaining, food grade lubricant is required. It is a superior, mult..
|
|||
| Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | See Note 1. |
|
ChevronTexaco 904 Grease NLGI Grade 1/2
Texaco 904 Grease is a calcium soap grease. It contains graphite which enhances its lubricity.Typical test data are average values only. Minor variations which do not affect product performance are ..
|
|||
| Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | See Note 1. |
|
ChevronTexaco EP 1 Aluminum Complex
Texaco Aluminum Complex EP 1 is manufactured using selected, high viscosity base oils, EP additives, rust and oxidation inhibitors. It has a high dropping point, which reduces the need for addition..
|
|||
| Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | See Note 1. |
|
ChevronTexaco Marfak® Heavy Duty 3
Texaco Marfak grease delivers value through:Good film strengthGood rust and corrosion protection, even in wet conditions.Texaco Marfak greases are fibrous sodium soap greases. It resists oil separat..
|
|||
| Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | See Note 1. |
|
ChevronTexaco Thermatex® EP NLGI Grade 1
Texaco Thermatex EP greases deliver value through:High temperature stability — Will not melt at high temperatures, but will remain in place on bearing surfaces and continue to provide excellent lub..
|
|||
| Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | See Note 1. |
|
ChevronTexaco Thermatex® EP NLGI Grade 2
Texaco Thermatex EP greases deliver value through:High temperature stability — Will not melt at high temperatures, but will remain in place on bearing surfaces and continue to provide excellent lub..
|
|||
| Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
|
3M 3334 Aluminum Foil/Scrim/PE Facing Tape
3M™ Aluminum Foil Tape 3334 has a high performance aluminum foil/bidirectional fiberglass scrim/polyethylene film laminate backing coated with a special pressure sensitive acrylic adhesive which ex..
|
|||
| Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
|
3M 9737 Double Coated Splicing Tape
3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres..
|
|||
| Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
|
3M 9738 Double Coated Splicing Tape
3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres..
|
|||
| Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
|
3M 9738R Double Coated Splicing Tape
3M™ Double Coated Tape 9737 is a Clear 3.5 mil acrylic double coated tape on a polyester film carrierFeatures:High tack, acrylic adhesive offers good low and elevated temperature resistance.Adheres..
|
|||
| Minimum Service Temperature, Air | -23.0 °C | -9.40 °F | |
|
Chesterton 652 Pneumatic Lubricant & Conditioner
Description: Chesterton® 652 Pneumatic Lubricant & Conditioner is a high performance, low viscosity, lubricating formula designed to creep into the internal workings of air tools, reduce wear and e..
|
|||