Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 15.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F

@Temperature -58.0 - 122 °F
TMA; ASTM E831
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical chemic..
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-2
Solvay Specialty Polymers Ixef® 1023 Polyarylamide (PARA)  (discontinued **)
Ixef 1023 is a 50% glass-fiber reinforced, UV stabilized polyarylamide for interior applications, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resis..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
8.33 µin/in-°F

@Temperature -22.0 - 86.0 °F
Idemitsu Kosan Xarec® WA 214 SPS, 40% Glass Filled
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature -30.0 - 100 °C
8.33 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND G3220A PP
SABIC® PPcompound G3220A is a general purpose, 20% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS is 209767996.
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 23.0 - 150 °C
8.33 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2410R PEI (Europe-Africa-Middle East)
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing.
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-2
Solvay Specialty Polymers Ixef® HC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® HC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat..
CTE, linear, Parallel to Flow 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
ASTM E-831
Sumitomo Bakelite North America RX® 3-2-530-P Long-Glass Reinforced Diallyl Phthalate
Long glass fiber reinforced, flame retardant, diallyl meta-phthalate molding compound which meets the requirements of ASTM D5948 Type GII-30F.Information provided by Vyncolit, a Sumitomo Bak Group
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® GV-4 FWA nat PA*-GF40
Product description: Grivory GV-4 FWA natural is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam..
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® GV-5H EF nat PA*-GF50
Product description: Grivory GV-5H EF natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam..
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® GV-6H EF black 9915 PA*-GF60
Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® HTV-6H1 black 9205 PA6T/6I-GF60
Product description: Grivory HTV-6H1 black 9205 is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I...
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® LV-50H FWA nat PA12-GF50
Product description: Grilamid LV-50H FWA natural is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w..
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TSG-50 FA PA666-GF50
Information provided by EMS Grivory
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TSG-50 PA666-GF50
Product description: Grilon TSG-50 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50 has the following important properties: High stiffne..
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TSG-50/4 W PA666-GF50
Product description: Grilon TSG-50/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® XE 3915 PA12-GF50
Product description: Grilamid XE 3915 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following produce profile:Good UV StabilityHigh impact strengthVe..
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® GV-6H black PA*-GF60
Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® HT1V-5 FWA black 9225 PA6T/6I-GF50
Product description: Grivory HT1V-5 FWA black 9225 is a 50 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: ..
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® HT1V-5 HY black 9205 PA6T/6I-GF50
Product description: Grivory HT1V-5 HY black 9205 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-5 HY bl..
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® HT1V-6 FWA black 9225 PA6T/6I-GF60
Product description: Grivory HT1V-6 FWA black 9225 is a 60 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: ..
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® HT1V-65H black 9205 PA6T/6I-GF65
Product description: Grivory HT1V-65H black 9205 is a 65% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I..
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
Barlog Plastics KEBATRON C2065X3 PPS, cross-linked, 65% glass fiber / mineral reinforced, reduced residual chlorine
PPS-GF/MD 65Information provided by BARLOG plastics GmbH.
CTE, linear, Parallel to Flow 15.0 - 20.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
8.33 - 11.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry)
Ultramid A3X2G7 is a 35% glass fiber reinforced injection molding PA66 grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stif..
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® GV-6H EF nat PA*-GF60
Product description: Grivory GV-6H EF black 9915 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol..
CTE, linear, Parallel to Flow 15.0 µm/m-°C
8.33 µin/in-°F
Above Tg; ISO 11359
Victrex® PEEK 150FC30 Easy Flow
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy ..
Copyright © lookpolymers.com All Rights Reserved