| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
Lanxess Durethan® BC 304 H3.0 000000 Nylon 6
PA 6, injection molding grade, non-reinforced, elastomer-modified, extremely high notched impact strength, including in the dry state and at low temperatures, also applicable for barrier layers in e..
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 23.0 - 55.0 °C
|
83.3
µin/in-°F <br>@Temperature 73.4 - 131 °F
|
ISO 11359-1,-2 |
|
Lanxess Durethan® BC 550 DUSXBL 900116 Nylon 6
PA 6, non-reinforced, extrusion, Blastorm, impact modified, heat-ageing stabilizedInformation provided by LANXESS.
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 23.0 - 55.0 °C
|
83.3
µin/in-°F <br>@Temperature 73.4 - 131 °F
|
ISO 11359-1, -2 |
|
Lanxess Durethan® TP 142-011 900116 Nylon 6
PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
1 |
|
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE)
POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu..
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Covestro Desmopan® 385 Thermoplastic Polyurethane
Desmopan 385 is a TPU on the basis of a standard ester.Applications: Screen sections, films, hoses, seals, technical automotive parts.Information provided by Bayer.As of 1 September 2015, Bayer Mate..
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Arnitel® EM550 55 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Arnitel® EM550 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Arnitel® EM630 Polyether Ester Elastomer (European Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Arnitel® EM630-H Polyether Ester Elastomer (European Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Arnitel® PL380 38 Shore D, Injection Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Arnitel® PL381 Injection Molding Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Arnitel® PL381 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| CTE, linear, Parallel to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
DSM Arnitel® PL381-H TPC-ET
Injection Molding
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Arnitel® PM381 Polyether Ester Elastomer (European Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| CTE, linear, Parallel to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® AZ 3/2 PA66
Product description: Grilon AZ 3/2 is an unreinforced and impact modified PA66 injection molding grade. Grilon AZ 3/2 has the following important properties: Excellent toughness at low temperaturesE..
|
|||
| CTE, linear, Parallel to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® BRZ 347 W PA6
Product description: Grilon BRZ 347 W is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon BRZ 347 W has the following important properties: High flexibi..
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Arnitel® EL550 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
|
|||
| CTE, linear, Parallel to Flow | 150 µm/m-°C | 83.3 µin/in-°F | ISO 11359-1/-2 |
|
DuPont Performance Polymers Hytrel® HTR8068 Polyester Elastomer TPC-ET
(Unverified Data**)
44 Shore D Flame Retardant Polyester Elastomer Developed for Extrusion and Injection Molding Information provided by DuPont Performance Polymers
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Arkema Group Rilsan® BESN F15 TL Nylon 11, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA11-P,EHL,16-001High flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High burst pressure and impact strength..
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
BASF Novolen® 2448 L Polypropylene
Data was collected by ISO methods and provided by BASF.
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
BASF Novolen® 2500 H Polypropylene
Injection molded parts, blow moldings and thermoformed parts.Data was collected by ISO methods and provided by BASF.
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
BASF Novolen® 2500 MC Polypropylene
Data was collected by ISO methods and provided by BASF.
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
BASF Novolen® 2600 M Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
BASF Novolen® 2600 PC Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
BASF Novolen® 2600 TC Polypropylene, Injection Molding Grade
Injection molded partsData was collected by ISO methods and provided by BASF.
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 23.0 - 250 °C
|
83.3
µin/in-°F <br>@Temperature 73.4 - 482 °F
|
ASTM D696 |
|
Solvay Specialty Polymers Algoflon® 25CAR PTFE; Petroleum Coke and Graphite
(discontinued **)
Data provided by the manufacturer.25 wt.% Petroleum Coke and Graphite. Suspension polymer powder grade recommended for compression molding. Pure PTFE possesses high inertness, excellent dielectric p..
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
BASF Novolen® 2240 P Polypropylene
Nucleated grade for injection moldings.Data was collected by ISO methods and provided by BASF.
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
BASF Novolen® 2440 K Polypropylene
Data was collected by ISO methods and provided by BASF.
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
BASF Novolen® 2900 NC Polypropylene
Injection molded partsData was collected by ISO methods and provided by BASF.
|
|||
| CTE, linear, Parallel to Flow |
150
µm/m-°C <br>@Temperature 20.0 °C
|
83.3
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Arkema Group Kynar® 4000 HD PVDF
(discontinued **)
Designation ISO 12086-PVDF-E,GG1N,Q.?E5.I.B.E.C,, ?(6-10)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high b..
|
|||