| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow |
30.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
16.7
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® 3412R PC (Europe-Africa-Middle East)
LEXAN 3412R is a high viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat.
|
|||
| CTE, linear, Parallel to Flow |
30.0
µm/m-°C <br>@Temperature -30.0 - 30.0 °C
|
16.7
µin/in-°F <br>@Temperature -22.0 - 86.0 °F
|
|
|
Idemitsu Kosan Xarec® N WA 7020 SPS, 20% Glass Filled
Crystalline Polymer Blend, Glass Filled, Impact Modified. Used in Automotive Electronics applications.
|
|||
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM D696 |
|
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant
Feature: Injection Molding, PA66+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
|
|||
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ASTM D696 |
|
LG Chemical LUMID GP2339B(W) PA66+GF33%, General Purpose
Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
|
|||
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
|
Lanxess Durethan® AKV 30 HR H2.0 901510 Nylon 66, 30% Glass Fiber
PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance
|
|||
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
|
Lanxess Pocan® B 3225 901510 PBT, 20% Glass Fiber
PBT, 20% glass fibers, injection molding
|
|||
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
|
Lanxess Pocan® B 4225 000000 PBT, 20% Glass Fiber
PBT, 20% glass fibers, injection molding, flame retardant
|
|||
| CTE, linear, Parallel to Flow |
30.0
µm/m-°C <br>@Temperature 23.0 - 55.0 °C
|
16.7
µin/in-°F <br>@Temperature 73.4 - 131 °F
|
ISO 11359-1, -2 |
|
Lanxess Pocan® ECO T 3220 000000 PBT + PET, 20% Glass Fiber
PBT + PET, 20% glass fibers, injection molding, improved surface finish, contains 28% post-consumer recycled material, increased temperature peak loadInformation provided by LANXESS.
|
|||
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
|
Lanxess Pocan® T 7331 000000 PBT + PET, 30% Glass Fiber
PBT+PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load
|
|||
| CTE, linear, Parallel to Flow |
30.0
µm/m-°C <br>@Temperature 23.0 - 55.0 °C
|
16.7
µin/in-°F <br>@Temperature 73.4 - 131 °F
|
ISO 11359-1, -2 |
|
Lanxess Durethan® BKV 15 DUS008 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 15% glass fibers, injection moldingInformation provided by LANXESS.
|
|||
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
|
Lanxess Durethan® BKV 30 G H2.0 900116 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance
|
|||
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
|
Lanxess Durethan® BKV 35 H2.0 EF 901510 Nylon 6, 35% Glass Fiber
PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow)
|
|||
| CTE, linear, Parallel to Flow |
30.0
µm/m-°C <br>@Temperature 23.0 - 85.0 °C
|
16.7
µin/in-°F <br>@Temperature 73.4 - 185 °F
|
ISO 11359 |
|
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim..
|
|||
| CTE, linear, Parallel to Flow |
30.0
µm/m-°C <br>@Temperature 23.0 - 60.0 °C
|
16.7
µin/in-°F <br>@Temperature 73.4 - 140 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics LNP LUBRICOMP MFL36S PP (Europe-Africa-Middle East)
LNP* Lubricomp* MFL36S is a compound based on Polypropylene resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized.
|
|||
| CTE, linear, Parallel to Flow |
30.0
µm/m-°C <br>@Temperature -40.0 - 40.0 °C
|
16.7
µin/in-°F <br>@Temperature -40.0 - 104 °F
|
ASTM E 831 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL26 PA 66
LNP LUBRICOMP* RFL26 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 10% PTFE. Added features of this material include: Wear Resistant.
|
|||
| CTE, linear, Parallel to Flow |
30.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
16.7
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics NORYL GFN3 PPE+HIPS (Europe-Africa-Middle East)
Noryl GFN3 is a standard 30 % glass filled material with a HDT/A of 145C according to ISO 75
|
|||
| CTE, linear, Parallel to Flow |
30.0
µm/m-°C <br>@Temperature 20.0 °C
|
16.7
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Covestro Makrolon® 8035 Polycarbonate
High viscosity extrusion and injection molding grade with 30% short glass fibers and easy mold release, low anisotropy, for stiff moldings requiring good dimensional stability.Information provided b..
|
|||
| CTE, linear, Parallel to Flow |
30.0
µm/m-°C <br>@Temperature 20.0 °C
|
16.7
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Covestro Makrolon® 9125 Polycarbonate
Medium viscosity, flame retardant extrusion and injection molding grade with 20% standard glass fibers and easy mold release agent.Information provided by Bayer.As of 1 September 2015, Bayer Materia..
|
|||
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
|
Covestro Makrolon® GF8001* Polycarbonate, 20% Glass Filled
ISO 7391-PC,MR,(,,)-18-3,GF20Developmental productFormerly Makrolon DP1-1951MVR (300 °C/1.2 kg) 16 cm3/10 min20 % Glass fiber reinforcedLow viscosityEasy releaseInjection molding - Melt temperature..
|
|||
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® B 70 GFE 30 H PA6-GF30
Product description: Grilon B 70 GFE 30 H is a heat stabilized and impact modified PA 6 injection molding grade with 30% glass fiber reinforcement. Grilon B 70 GFE 30 H has the following important p..
|
|||
| CTE, linear, Parallel to Flow |
30.0
µm/m-°C <br>@Temperature 20.0 °C
|
16.7
µin/in-°F <br>@Temperature 68.0 °F
|
ISO 11359-1/-2 |
|
DSM Stanyl® TW200F3 Nylon 46-15% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
|
|||
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® TSG-30/4 LF 15 PA666-(GF+Z)45
Product description: Grilon TSG-30/4 LF 15 natural is a normal viscosity, heat stabilized PA 66 + PA 6- molding type with 30% glass fibre reinforcement and 15% of a combination PTFE and siliconoil. ..
|
|||
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C | 16.7 µin/in-°F | dry; ISO 11359-1/-2 |
|
DSM Akulon® K224-G3-FC NA99001 PA6-GF15
15% Glass Reinforced
|
|||
| CTE, linear, Parallel to Flow |
30.0
µm/m-°C <br>@Temperature 20.0 °C
|
16.7
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
BASF Procom® GC30S 403 Polypropylene
Uses: Electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF.
|
|||
| CTE, linear, Parallel to Flow |
30.0
-
35.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
16.7
-
19.4
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
ISO 11359-1/-2 |
|
BASF Ultramid® B3ZG3 BK30564 15% Glass Filled PA6 (Dry)
Ultramid B3ZG3 BK30564 is an impact-modified, pigmented black, 15% glass fiber reinforced injection molding PA6 grade.
|
|||
| CTE, linear, Parallel to Flow |
30.0
µm/m-°C <br>@Temperature 20.0 °C
|
16.7
µin/in-°F <br>@Temperature 68.0 °F
|
|
|
Arkema Group Rilsan® AZM 43 G9 T6LD Nylon 12, 43% Glass Fiber Filled (Conditioned)
Designation ISO 1874-PA12,MHLS,16-080,(G+C)(F+D)(43+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab..
|
|||
| CTE, linear, Parallel to Flow |
30.0
-
35.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
16.7
-
19.4
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
DIN 11359-1/-2 |
|
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry)
Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat..
|
|||
| CTE, linear, Parallel to Flow |
30.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
16.7
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics Lexan® ML3286 PC (Europe-Africa-Middle East)
LEXAN ML3286 is a 17% glass reinforced grade for use in less demanding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| CTE, linear, Parallel to Flow |
30.0
-
40.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
16.7
-
22.2
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
ISO 11359-1/-2 |
|
BASF Ultradur® B 4300 G4 FC 20% Glass Filled PBT
Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation..
|
|||