Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 19.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
10.6 µin/in-°F

@Temperature -58.0 - 122 °F
TMA; ASTM E831
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
10.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
Idemitsu Kosan Xarec® EA 513 SPS, 30% Glass Filled
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
10.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
Idemitsu Kosan Xarec® EA 533 SPS, 30% Glass Filled
Glass Filled, Ignition Resistant, Impact Modified. Used in electronic and electrical applications.
CTE, linear, Parallel to Flow 19.0 µm/m-°C
10.6 µin/in-°F
ASTM D696
Kuraray Genestarâ„¢ G1350A-M42 Nylon, 35% Glass Filled
35% Glass reinforced injection grade. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment.Main Features:Hydrolysis resistanceHeat resista..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
10.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 3452 PEI (Europe-Africa-Middle East)
45% Glass fiber and mineral filled, enhanced flow Polyetherimide (Tg 217C) with enhanced dimensional stability. Resin is RoHS compliant. UL94 V0 and 5VA listing in recognized colors.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
10.6 µin/in-°F

@Temperature -58.0 - 122 °F
1
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical streng..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
10.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® V9561 PET
Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
10.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66 (Europe-Africa-Middle East)
LNP* Thermocomp* RF00C is a compound based on Nylon 66 resin containing Glass Fiber.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
10.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP UF009AXP PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UF009AXP is a compound based on Polyphthalamide resin containing 45% Glass Fiber.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
10.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP YF006A Polyester Elastomer (Europe-Africa-Middle East)
LNP* THERMOCOMP* YF006A is a compound based on Polyester Elastomer containing Glass Fiber.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 20.0 °C
10.6 µin/in-°F

@Temperature 68.0 °F
ASTM E-831
Sumitomo Bakelite North America RX® 1366FR-P Short-Glass Reinforced Diallyl Phthalate
Short glass fiber reinforced, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type SDG-F.Information provided by Vyncolit, a Sumitomo Bak Group
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Thickness 1.50 mm,
Temperature 55.0 - 160 °C
10.6 µin/in-°F

@Thickness 0.0591 in,
Temperature 131 - 320 °F
ISO 11359-1/-2
DuPont Performance Polymers Rynite® FR515 BK507 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8m..
CTE, linear, Parallel to Flow 19.0 µm/m-°C
10.6 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
CTE, linear, Parallel to Flow 19.0 µm/m-°C
10.6 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® FR50 NC010A Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 NC010A is a 25% glass fiber reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performanc..
CTE, linear, Parallel to Flow 19.0 µm/m-°C
10.6 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® HTN 53G50LWSF BK702A Polyphthalamide (PPA)  (Unverified Data**)
50% Glass Reinforced High Performance Polyamide with Low Warpage and High Stiffness Information provided by DuPont Performance Polymers
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
10.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded
AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
10.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide RFC16 PA66/6, Glass/Carbon Fiber Filled, Injection Molded
RFC16 is a Glass Fiber and Carbon Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding Resin (also known as STAR C PA66 C 303VY Z3)Information provided by Eurostar.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
10.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/2
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 20.0 °C
10.6 µin/in-°F

@Temperature 68.0 °F
Arkema Group Orgalloy® RS 6030 AT Nylon 6 Alloy, 30% Glass Fiber (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties...
CTE, linear, Parallel to Flow 19.0 µm/m-°C
10.6 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Rynite® FR530L NC010 Polyethylene Terephthalate (PET)
Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
10.6 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East)
Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances.
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 20.0 °C
10.6 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Sumitomo Bakelite North America FM 4005 Fiberglass Reinforced Phenolic Novolac
FM 4005 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is compliant with the specificat..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 20.0 °C
10.6 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Sumitomo Bakelite North America FM 4008 Fiberglass and Mineral Reinforced Phenolic Resole
FM 4008 is a fiberglass and mineral reinforced phenolic resole compound, with excellent dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North A..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 20.0 °C
10.6 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Sumitomo Bakelite North America FM 4017F Fiberglass and Mineral Reinforced Phenolic
FM 4017F is a fiberglass and mineral reinforced phenolic molding compound, with excellent dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North..
CTE, linear, Parallel to Flow 19.0 µm/m-°C

@Temperature 20.0 °C
10.6 µin/in-°F

@Temperature 68.0 °F
Arkema Group Orgalloy® RS 6030 Nylon 6 Alloy, 30% Glass Fiber (Conditioned)
RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties..
Copyright © lookpolymers.com All Rights Reserved