| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
|
Premix Premi-Glas® 1100-20 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100-20 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti..
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
|
Premix Premi-Glas® 1200-30 Polyester SMC
Premi-Glas® 1200-30 is a fiberglass-reinforced, thermoset, sheet molding compound designed for Class A Heavy Truck and Marine body panels and interior structural components where smooth flat surfac..
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
|
Premix Premi-Glas® 1200H-22 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200H-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go..
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
|
Premix Premi-Glas® 1201-15 Polyester SMC
Premi-Glas® 1201-15 is a 15% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS..
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
|
Premix Premi-Glas® 2103-20 CR-SX Fiberglass Reinforced Thermoset BMC
Premi-Glas® 2103-20 CR-SX is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regu..
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
|
Premix Premi-Glas® 2200-30 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2200-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
|
Premix Premi-Glas® 2203-15 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2203-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
|
Premix Premi-Glas® 2203-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2203-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
|
Premix Premi-Glas® 2204-20 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2204-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Good dimensional stability, inclu..
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
|
Premix Premi-Glas® 2205-22 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
|
Premix Premi-Glas® 2205-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
|
Premix Premi-Glas® 2243-24 CR-SX Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 2243-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves..
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | Z Direction |
|
Premix Premi-Glas® 3101-10 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 3101-10 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and ..
|
|||
| CTE, linear, Parallel to Flow |
35.0
µm/m-°C @Temperature -30.0 - 30.0 °C |
19.4
µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL42 PC
LNP* Lubricomp* DFL-4042 a compound based on Polycarbonate resin containing 10% Glass Fiber, 20% PTFE. Added features include: Internally Lubricated.
|
|||
| CTE, linear, Parallel to Flow |
35.0
µm/m-°C @Temperature 20.0 °C |
19.4
µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
|
DSM Akulon® K-FHGM35 (Dry) 40% Glass/Mineral Reinforced, Nylon 6 (North America)
(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
|
|||
| CTE, linear, Parallel to Flow |
35.0
µm/m-°C @Temperature -30.0 - 30.0 °C |
19.4
µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
|
SABIC Innovative Plastics LNP LUBRICOMP QFN16 PA 6/10
LNP* LUBRICOMP* QFN16 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 5% MOS2. Added feature of this material is: Wear Resistant.
|
|||
| CTE, linear, Parallel to Flow |
35.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
19.4
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics LNP STAT-KON PFD04S PA 6 (Europe-Africa-Middle East)
LNP* Statkon* PFD04S is a compound based on PA 6 resin containing Glass Fiber, Carbon Powder. Added features include: Electrically Conductive, Heat Stabilized.
|
|||
| CTE, linear, Parallel to Flow |
35.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
19.4
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics LNP THERMOCOMP MFB63 PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MFB63 is a compound based on Polypropylene resin containing Glass Bead, Glass Fiber.
|
|||
| CTE, linear, Parallel to Flow |
35.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
19.4
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics LNP Thermocomp RFB24 PA 66 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RFB24 is a compound based on PA 66 resin containing Glass Bead, Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | ISO 11359-1/-2 |
|
DSM Arnite® TV4 260 SN PBT-GF30 FR(17)
30% Glass Reinforced, Flame Retardant
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | ISO 11359-1/-2 |
|
DSM Arnite® TV4 260 SXF PBT-GF30 FR(17)
30% Glass Reinforced, Flame Retardant, High Flow
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | ISO 11359-1/-2 |
|
DSM Arnite® TV4 261 SF PBT-GF30 FR(17)
30% Glass Reinforced, Flame Retardant, High Flow
|
|||
| CTE, linear, Parallel to Flow |
35.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
19.4
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
Eurostar Staramide AG3K PA66, 15% Glass Filled, Injection Molded
AG3K is a Heat and Hydrolytically Stabilized, 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl..
|
|||
| CTE, linear, Parallel to Flow |
35.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
19.4
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
Eurostar Starflam AFR682A1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding
Starflam AFR682A1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® BGK-30 X PA6-(GF+GB)30
Information provided by EMS Grivory
|
|||
| CTE, linear, Parallel to Flow |
35.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
19.4
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
Eurostar Staramide AG3 PA66, 15% Glass Filled, Injection Molded
AG3 is a 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| CTE, linear, Parallel to Flow |
35.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
19.4
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded
BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| CTE, linear, Parallel to Flow | 35.0 µm/m-°C | 19.4 µin/in-°F | ISO 11359-1/-2 |
|
DSM Arnite® TV4 264 SN PBT-GF30 FR(17)
30% Glass Reinforced, Flame Retardant
|
|||
| CTE, linear, Parallel to Flow |
35.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
19.4
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics Valox® VX5530 PBT (Europe-Africa-Middle East)
VALOX VX5530 is a flame retarded, 15% glass fibre reinforced, 10% mineral filled PBT+PC blend with excellent low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
|
|||