Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Lexan® EX1632T PC
Lexan* EX1632T polycarbonate resin is designed for use in multi-wall sheet or profile extrusion applications. It contains branched polycarbonate resin, release, and UV stabilizer. It is available ..
CTE, linear, Parallel to Flow 65.0 - 100 µm/m-°C
36.1 - 55.6 µin/in-°F
ASTM D696
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact
Feature: Injection Molding, PA6/ABS+MF6%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Mitsubishi Xantar® 18 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Mitsubishi Xantar® 24 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Mitsubishi Xantar® 27 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Mitsubishi Xantar® F 23 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Mitsubishi Xantar® F 25 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Mitsubishi Xantar® FC 25 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Mitsubishi Xantar® MX 1021 FD MX 1021 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
Mitsubishi Xantar® MX 2021 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
CTE, linear, Parallel to Flow 65.0 µm/m-°C
36.1 µin/in-°F
ASTM D696
Kuraray Genestarâ„¢ N1001A-M41 Nylon
Low friction unreinforced injection grade. Main Features:Low friction coefficientHigh impact strengthExamples of applications are:Friction and wear applicationGear and wheel
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Mitsui Arlenâ„¢ AE4200N Modified Nylon 6T, for Tribolic Applications, Flame Retardant (COND)
ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
36.1 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP D7002IXH PC
LNP* THERMOCOMP* D7002IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces, housings, etc., in healthcare an..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Makrolon® 1881 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Impact modified• Imp..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Makrolon® 1952 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me..
CTE, linear, Parallel to Flow 65.0 µm/m-°C
36.1 µin/in-°F
ISO 11359-1/-2
Covestro Makrolon® 2556 Polycarbonate
MVR (300 °C/1.2 kg) 14 cm3/10 minEasy releaseGood hydrolysis resistanceInjection moldingAvailable in transparentTranslucent and opaque colorsFood contact gradePreprocessingMax. Water content
CTE, linear, Parallel to Flow 65.0 µm/m-°C
36.1 µin/in-°F
ISO 11359-1/-2
Covestro Makrolon® 2665 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt temp..
CTE, linear, Parallel to Flow 65.0 µm/m-°C
36.1 µin/in-°F
ISO 11359-1/-2
Covestro Makrolon® 6585 Polycarbonate, Flame Retardant Grade
ISO 7391-PC,MFR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minFlame retardantUL 94V-0/1.2 mm5VA/3.0 mm and 5VB (WT) /2.0 mmHigh viscosityEasy releaseInjection molding - Melt temperature 28..
CTE, linear, Parallel to Flow 65.0 µm/m-°C
36.1 µin/in-°F
ISO 11359-1/-2
Covestro Makrolon® AL2447 Polycarbonate
ISO 7391-PC,MLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minAutomotive lightingLow viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in transpa..
CTE, linear, Parallel to Flow 65.0 µm/m-°C
36.1 µin/in-°F
ISO 11359-1/-2
Covestro Makrolon® LQ3147 Polycarbonate
ISO 7391-PC,MLR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 minOptical lensHigh viscosityUV stabilizedEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in clear tints ..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Makrolon® Rx2435 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Low..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Makrolon® ET3127 Polycarbonate
Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Makrolon® ET3227 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Makrolon® Rx2635 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices• Med..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
BASF Luranyl® KR 2401 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade
Base grade with a balanced combination of impact strength and stiffness. Uses include: parts of vehicle interiors, air ducts and loudspeaker housings.Data was collected by ISO methods and provided ..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Makrolon® LED2643 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, ..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
BASF Luranyl® KR 2451/3 Polyphenylene Ether + Styrene-Butadiene Blend
Especially easy flowing grade containing halogen-free, flame-retardant; mainly used for housings for electrical equipment and in the electronics sector.Data was collected by ISO methods and provided..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
Arkema Group Oroglas® V 045 Acrylic, Extrusion Grade  (discontinued **)
OROGLAS V 045 is a lubricated extrusion grade offering good combination of physical and optical properties.OROGLAS V 045 provides easy processing behavior.OROGLAS V 045 is recommended for extrusion..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
Arkema Group Oroglas® V 825 HID Acrylic, UV, Heat Resistant  (discontinued **)
OROGLAS HID is an acrylic resin formulated to withstand continuous exposure to high intensity discharge ( HID ) sources up to 90°c.Above 80°c, OROGLAS V 825 HID resin retains its original appearan..
CTE, linear, Parallel to Flow 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
Arkema Group Oroglas® V 920 Acrylic, Injection Molding Grade  (discontinued **)
OROGLAS V 920 is an injection molding grade with a good balance of properties :Superior flow with medium thermal resistance.The processing of OROGLAS V 920 is easy in terms of injection molding, mo..