Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 39.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature 20.0 °C
21.7 µin/in-°F
<br>@Temperature 68.0 °F
ISO data
BASF Capron® GR15 HS 15% Glass-Filled Nylon 6 (Dry) &nbsp;(discontinued **)
Capron GR15 HS is a heat stabilized 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
21.7 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN
LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati..
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature 20.0 °C
21.7 µin/in-°F
<br>@Temperature 68.0 °F
ASTM data
BASF Capron® 5233G 33% Glass-Filled Nylon 66 (Dry) &nbsp;(discontinued **)
Capron 5233G is a 33% glass fiber reinforced, polyamide 6,6 injection molding compound offering excellent strength, stiffness, creep resistance and dimensional stability. This balance of engineerin..
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature 20.0 °C
21.7 µin/in-°F
<br>@Temperature 68.0 °F
ISO data
BASF Capron® 8231G 14% Glass-Filled Nylon 6 (Dry) &nbsp;(discontinued **)
Capron 8231G is a 14% glass fiber reinforced polyamide 6 molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also av..
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
21.7 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Lubricomp EFP36G PEI
LNP* EFP36G is a Polyetherimide base resin containing a Mixed Glass Fiber and PTFE/Silicone.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
21.7 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP LX82803 PEEK (Europe-Africa-Middle East)
LNP* LUBRICOMP* LX82803 is a compound based on Polyetheretherketone resin containing Proprietary Lubricant. Added features include : Internally Lubricated.
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
21.7 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE.
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
21.7 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 4001 PEI (Europe-Africa-Middle East)
PTFE filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
21.7 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp 9X06477 SPS
LNP* Thermocomp* 9X06477 is a compound based on Syndiotactic Polystyrene resin containing Glass Fiber. Characteristics of this grade is Heat Stabilized.This data was supplied by SABIC-IP for the Am..
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
21.7 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP DF002ER PC (Europe-Africa-Middle East)
LNP* THERMOCOMP* DF002ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features include Easy Molding, Mold Release.
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
21.7 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP SF004S PA12
LNP* Thermocomp* SF004S is a compound based on Nylon 12 containing 20% glass fiber. Added features include: Heat Stabilized, Healthcare
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
21.7 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP WFB44 PBT (Europe-Africa-Middle East)
LNP* Thermocomp* WFB44 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Glass Bead.
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
21.7 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOTUF IX02582 PA6.12
LNP* Thermotuf* IX02582 is a compound based on Nylon 6/12 resin containing Proprietary Filler(s). Added features of this material include: High Impact.
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
21.7 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP IF006 PA6.12 (Europe-Africa-Middle East)
LNP THERMOCOMP* IF006 is a compound based on nylon 6/12 resin containing glass fibre
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
21.7 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT
LNP* THERMOCOMP* WF004 is a compound based on PBT resin containing 20% Glass Fiber.
CTE, linear, Parallel to Flow 39.0 µm/m-°C
21.7 µin/in-°F
ISO 11359
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry)
Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla..
CTE, linear, Parallel to Flow 39.0 µm/m-°C
<br>@Temperature 20.0 °C
21.7 µin/in-°F
<br>@Temperature 68.0 °F
ISO data
BASF Capron® GR15 15% Glass-Filled Nylon 6 (Dry) &nbsp;(discontinued **)
Capron GR15 is a 15% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aesthetics. It is also..
Copyright © lookpolymers.com All Rights Reserved