| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -50.0 - 50.0 °C
|
27.8
µin/in-°F <br>@Temperature -58.0 - 122 °F
|
TMA; ASTM E831 |
|
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK)
(Unverified Data**)
KetaSpire KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standar..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -30.0 - 30.0 °C
|
27.8
µin/in-°F <br>@Temperature -22.0 - 86.0 °F
|
ASTM D696 |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL12 PC
LNP* Lubricomp* DFL12 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated.
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM 1010FC PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM 1100F PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no longer be supported with b..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM 1110F PEI (Europe-Africa-Middle East)
Enhanced flow PolyetherimiEnhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant. Effective June, 2007 this grade will no long..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM 9075 PEI (Europe-Africa-Middle East)
High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution.
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM CRS5001 PEI (Europe-Africa-Middle East)
Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing.
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature 23.0 - 150 °C
|
27.8
µin/in-°F <br>@Temperature 73.4 - 302 °F
|
ISO 11359-2 |
|
SABIC Innovative Plastics ULTEM PW1000 PEI (Europe-Africa-Middle East)
Unfilled Standard flow Polyetherimide (Tg 217°C). Specific grade-colors aredesigned and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified. US FDA and Euro..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -50.0 - 50.0 °C
|
27.8
µin/in-°F <br>@Temperature -58.0 - 122 °F
|
1 |
|
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK)
KetaSpire® KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -50.0 - 50.0 °C
|
27.8
µin/in-°F <br>@Temperature -58.0 - 122 °F
|
1 |
|
Solvay Specialty Polymers Ryton® QC200N Polyphenylene Sulfide (PPS)
Ryton® PPS Fiber Grade Resins are high molecular weight polyphenylene sulfide polymers suitable for monofilament and/or multifilament fiber extrusion. They exhibit excellent thermal stability and..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -50.0 - 50.0 °C
|
27.8
µin/in-°F <br>@Temperature -58.0 - 122 °F
|
1 |
|
Solvay Specialty Polymers Ryton® QC200P Polyphenylene Sulfide (PPS)
Ryton® PPS Fiber Grade Resins are high molecular weight polyphenylene sulfide polymers suitable for monofilament and/or multifilament fiber extrusion. They exhibit excellent thermal stability and..
|
|||
| CTE, linear, Parallel to Flow |
50.0
µm/m-°C <br>@Temperature -30.0 - 30.0 °C
|
27.8
µin/in-°F <br>@Temperature -22.0 - 86.0 °F
|
ASTM D696 |
|
SABIC Innovative Plastics LNP STAT-KON EX02598C PEI
LNP* STAT-KON* EX02598C is a compound based on Polyetherimide containing Proprietary Filler(s). Added features of this material include: Clean Compound System, Electrically Conductive.
|
|||
| CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
|
Covestro Makroblend® DP 7665 MBS162 Polycarbonate + PET, Mineral Filled Impact Grade
Developmental product(PC+PET)-blendsimpact modifiedInjection molding grade 20 % mineral filledAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new..
|
|||
| CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
|
DSM Arnite® TV4 230 S PBT-GF15 FR(17)
15% Glass Reinforced, Flame Retardant
|
|||
| CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® BG-15 S PA6-GF15
Product description: Grilon BG-15 S is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15 S has the following important properties: Excellent surface finishEasy flowin..
|
|||
| CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® BG-15/2 PA6-GF15
Product description: Grilon BG-15/2 is a heat stabilized PA6 injection molding grade with 15% glass fibers. Grilon BG-15/2 has the following important properties: Good surface finishEasy processingG..
|
|||
| CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
|
EMS-Grivory Grivory® LV-3 ESD PA12-GF30
Product description: Grilamid LV-3 ESD is an antistatic PA12 injection molding grade, with fiber reinforcement of 30%. Due to its special formulation, the material can be used for applications where..
|
|||
| CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
|
DuPont Performance Polymers Crastin® SK642FR NC010 Polybutylene Terephthalate (PBT)
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR is a 15% glass fibre reinforced flame retardant polybutylene terephthalate for injection moulding.It has a UL94 V-0 ra..
|
|||
| CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | DAM; ISO 11359-1/-2 |
|
DuPont Performance Polymers Zytel® 79G13HSL NC010 Nylon 66
(Unverified Data**)
13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL is a 13% glass fiber reinforced heat stabilized lubricated slightly toughened polyamide 66 for injection molding. It has im..
|
|||
| CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | DAM; ISO 11359-1/-2 |
|
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**)
14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS BKB085 is a 14% glass reinforced toughened heat stabilized black polyamide 66 resin.Information provided by DuPont Performanc..
|
|||
| CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
|
Covestro Makrolon® DP1-1888* Polycarbonate, 20% Glass Filled
ISO 7391-PC,MR,(,,)-09-3,GF20Developmental productMVR (300 °C/1.2 kg) 10 cm3/10 min20 % Glass fiber reinforcedMilled fiberMedium viscosityEasy releasegood surface qualityInjection molding - Melt te..
|
|||
| CTE, linear, Parallel to Flow | 50.0 µm/m-°C | 27.8 µin/in-°F | ISO 11359-1/-2 |
|
Barlog Plastics KEBATER BF110 PBT, 10% glass fiber reinforced
PBT-GF10Information provided by BARLOG plastics GmbH.
|
|||
| CTE, linear, Parallel to Flow |
50.0
-
90.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
27.8
-
50.0
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
DIN 11359-1/-2 |
|
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry)
Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°..
|
|||
| CTE, linear, Parallel to Flow |
50.0
-
60.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
27.8
-
33.3
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
DIN 11359-1/-2 |
|
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
|
|||
| CTE, linear, Parallel to Flow |
50.0
-
60.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
27.8
-
33.3
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
DIN 11359-1/-2 |
|
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Dry)
Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
|
|||
| CTE, linear, Parallel to Flow |
50.0
-
60.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
27.8
-
33.3
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
DIN 11359-1/-2 |
|
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Dry)
Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi..
|
|||
| CTE, linear, Parallel to Flow |
50.0
-
80.0
µm/m-°C <br>@Temperature 23.0 - 80.0 °C
|
27.8
-
44.4
µin/in-°F <br>@Temperature 73.4 - 176 °F
|
ISO 11359-1/-2 |
|
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry)
ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase..
|
|||