| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 11.0 µm/m-°C | 6.11 µin/in-°F | ASTM D696 |
|
PolyOne Therma-Tech™ SF-4500 TC Polyphenylene Sulfide (PPS)
Information provided by PolyOne
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
6.11
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics LNP THERMOCOMP OE004A PPS - BRANCHED (Europe-Africa-Middle East)
LNP* STATKON* OE004A is a compound based on PPS (branched) resin containing Carbon Fiber. Added features include: Electrically Conductive. (only Black is UL listed)
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
6.11
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics LNP Stat-kon DE0049 PC (Europe-Africa-Middle East)
LNP* Stat-kon* DC-1004 FR is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant.This..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 23.0 - 150 °C |
6.11
µin/in-°F @Temperature 73.4 - 302 °F |
ASTM E 228 |
|
DuPont Performance Polymers VESPEL TP-8549 Polyimide
Thermoplastic parts from filled PI (polyimide) for high mechanical properties and low wear and friction performance in high temperature hostile environmentsInformation provided by DuPont Performance..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 55.0 - 160 °C |
6.11
µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
|
DuPont Performance Polymers Zytel® HTN FR55G50NHLW BK046 Polyphthalamide (PPA)
(Unverified Data**)
55% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Low Warpage and High Stiffness Zytel HTNFR55G50NHLW BK046 is a 50% glass reinforced flame retardant high perf..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
|
BASF Ultraform N 2310P Q600 POM
Ultraform N2310P Q600 is a general-purpose injection molding POM grade containing special lubricant. Low frictional coefficient giving extremely low wear with otherwise unaltered mechanical propert..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
|
BASF Ultraform N 2320 003 UNC Q600 POM
Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent.
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
|
BASF Ultraform S 2320 003 UNC Q600 POM
Ultraform S2320 003 UNC Q600 is an easy flowing and rapidly freezing injection molding POM grade. Contains a mold release agent.
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
|
BASF Ultraform® N2320 U035 POM
Description: Is a POM, UV-stabilized injection-molding grade.Information provided by BASF
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
|
BASF Ultraform® S1320 003 POM
Description: Is a POM, free-flowing, rapidly solidifying grade for moldings difficult to produce by injection molding and having low wall thicknesses, higher stiffness and thermal stability.Informat..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
|
BASF Ultraform® S2320 0035 POM
Description: Is a POM, free-flowing and rapidly solidifying standard grade with improved impact strength for injection molding.Information provided by BASF
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
|
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM
Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
|
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
|
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM
Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
|
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
|
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
|
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 23.0 - 80.0 °C |
6.11
µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/2 |
|
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
|
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
|
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
|
BASF Ultraform W 2320 003 UNC Q600 POM
Ultraform W2320 003 UNC Q600 is a very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties are lower. Contains ..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
|
BASF Ultraform® S2320 003 PRO BK 00120 POM
Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
|
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
|
BASF Ultraform S 1320 0021 UNC POM
Ultraform S1320 0021 UNC is an easy flowing, rapidly freezing injection molding POM grade with enhanced stiffness and heat distortion resistance. It is highly stabilized to resist aggressive fuels,..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 23.0 - 60.0 °C |
6.11
µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
|
SABIC Innovative Plastics LNP STAT-KON OE004A PPS - BRANCHED (Europe-Africa-Middle East)
LNP* STATKON* OE004A is a compound based on PPS (branched) resin containing Carbon Fiber. Added features include: Electrically Conductive.
|
|||
| CTE, linear, Parallel to Flow | 11.0 µm/m-°C | 6.11 µin/in-°F | TMA |
|
Vyncolit Neopreg Kinel® SK4525 S5 Glass Fiber Reinforced Molding Compound
BMI molding compound long glass fiber reinforced with excellent mechanical and thermal properties. Especially suited to be used for injection molding.Information provided by Sumitomo Bak North Ameri..
|
|||
| CTE, linear, Parallel to Flow |
11.0
µm/m-°C @Temperature 23.0 - 55.0 °C |
6.11
µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
|
BASF Ultraform® W2320 0035 LEV POM
Description: Is a POM, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF
|
|||