Polymer Property : CTE, linear, Parallel to Flow = 66.7 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 120 µm/m-°C
<br>@Temperature -30.0 - 30.0 °C
66.7 µin/in-°F
<br>@Temperature -22.0 - 86.0 °F
ASTM E831
PolyOne Edgetek® X TR2-10GF/000 NATURAL Copolyester
The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea..
CTE, linear, Parallel to Flow 120 µm/m-°C
<br>@Temperature 20.0 °C
66.7 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359-1/-2
DSM Akulon® S223-TP4 (Dry) Impact Modified Nylon 66 (North America) &nbsp;(discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® B 1300 000000 PBT
PBT, non-reinforced, injection molding, extrusion
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® KU 2-7003 000000 PBT
PBT, non-reinforced, injection molding
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® B 1505 000000 PBT
PBT, non-reinforced, injection molding, extrusion
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)
Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance..
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
CTE, linear, Parallel to Flow 120 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
66.7 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-LOY 63000CTC PC+POLYESTER (Asia Pacific)
A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications
CTE, linear, Parallel to Flow 120 µm/m-°C
<br>@Temperature 20.0 °C
66.7 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359-2
Polyplastics Tepcon M90 Acetal-copolymer (POM), General
Information provided by PolyPlastics.
CTE, linear, Parallel to Flow 120 µm/m-°C
<br>@Temperature 20.0 °C
66.7 µin/in-°F
<br>@Temperature 68.0 °F
ASTM D696
Lubrizol Estane® 2102-65D Thermoplastic Polyurethane Elastomer
Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® L 20 G grey 9280 PA12
Product Description: Grilamid L 20 G grey 9280 is a medium viscosity, unreinforced, heat stabilized polyamide 12 for injection molding and cable sheathing. The main features of this product are: Low..
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® L 20 LM PA12
Product Description: Grilamid L 20 LM is a medium viscosity Polyamide 12 (PA12) extrusion grade. Grilamid L 20 LM is UV and heat stabilized and has been modified with a nucleation agent which result..
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® L 25 nat 6112 PA12
Product Description: Grilamid L 25 natural 6112 is a high viscous, Polyamide 12 extrusion grade. Grilamid L 25 natural 6112 fulfils the requirements of DIN 73378, Type PA 12-H. Application examples:..
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® L 25H FWA nat PA12
Product Description: Grilamid L 25 H FWA natural is a highviscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 25 H FWA natural is designed for technical injection moulded com..
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® XE 3817 black 9992 PA12
Product description: Grilamid XE 3817 black 9992 is a medium viscosity, heat and UV-stabilized Polyamid 12. Grilamid XE 3817 black 9992 is especially suitable for the coating of metal tubes and offe..
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® XE 3926 black 9992 PA12
Product description: Grilamid XE 3926 black 9992 is a low viscosity extrusion type, based on Polyamide 12 (PA 12). The special features of Grilamid XE 3926 black 9992 are: Very good chemical resista..
CTE, linear, Parallel to Flow 120 µm/m-°C
<br>@Temperature 23.0 - 60.0 °C
66.7 µin/in-°F
<br>@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starflam MX05075 PP, Flame Retardant, Injection Molding
Starflam MX05075 is an Unfilled Halogen Free Flame Retardant PP Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TR 90 NZZ nat PAMACM12-I
Product description: Grilamid TR 90 NZZ natural is an amorphousthermoplastic polyamide, based on aliphatic and cycloaliphatic units. Grilamid TR 90 NZZ natural offers a variety of interesting proper..
CTE, linear, Parallel to Flow 120 µm/m-°C
<br>@Temperature 20.0 °C
66.7 µin/in-°F
<br>@Temperature 68.0 °F
Arkema Group Rilsan® AMN P20 TLD Nylon 12, Flexible, Injection Grade (Conditioned)
Designation ISO 1874-PA12-P,MHLR,14-005Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and ..
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Barlog Plastics KEBAFORM C 130.2 POM Copolymer unreinforced
POMInformation provided by BARLOG plastics GmbH.
CTE, linear, Parallel to Flow 120 µm/m-°C
66.7 µin/in-°F
ISO 11359-1/-2
Barlog Plastics KEBAFORM C 901 FA POM Copolymer unreinforced, reduced formaldehyde emission
POMInformation provided by BARLOG plastics GmbH.
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
ASTM D696
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA) &nbsp;(Unverified Data**)
Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista..
CTE, linear, Parallel to Flow 120 - 200 µm/m-°C
66.7 - 111 µin/in-°F
ASTM D696
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA) &nbsp;(Unverified Data**)
Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista..
CTE, linear, Parallel to Flow 120 µm/m-°C
<br>@Temperature 20.0 °C
66.7 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359-1/-2
DSM Akulon® K223-TP4 (Dry) Impact Modified Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..