| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 15.0 - 20.0 µm/m-°C @Temperature 50.0 - 150 °C |
8.33 - 11.1 µin/in-°F @Temperature 122 - 302 °F |
ISO 11359-2 |
| Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel.. |
|||
| CTE, linear, Parallel to Flow | 15.0 - 35.0 µm/m-°C @Temperature 50.0 - 100 °C |
8.33 - 19.4 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
| Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-2 |
| Solvay Specialty Polymers Ixef® 1023 Polyarylamide (PARA)
(discontinued **) Ixef 1023 is a 50% glass-fiber reinforced, UV stabilized polyarylamide for interior applications, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resis.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 20.0 °C |
8.33 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
| DSM Akulon® Ultraflow™ K-FHG7 Nylon 6-35% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -30.0 - 100 °C |
8.33 µin/in-°F @Temperature -22.0 - 212 °F |
ISO 11359-2 |
| SABIC Innovative Plastics SABIC PPCOMPOUND G3220A PP SABIC® PPcompound G3220A is a general purpose, 20% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS is 209767996. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 23.0 - 150 °C |
8.33 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
| SABIC Innovative Plastics ULTEM 2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 23.0 - 150 °C |
8.33 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
| SABIC Innovative Plastics Ultem PW2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water
applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
8.33 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
| SABIC Innovative Plastics LNP THERMOCOMP EFB26ER PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* EFB26ER is a compound based on Polyetherimide containing Glass Fiber, Glass Bead. Added features include: Easy Molding, Mold Release. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
8.33 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
| SABIC Innovative Plastics LNP THERMOCOMP RC006XXH PA 66 LNP* THERMOCOMP* RC006XXH is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 20.0 °C |
8.33 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Sumitomo Bakelite North America 2-530 Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Am.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® GV-5 FWA black 9225 PA*-GF50 Product description: Grivory GV-5 FWA black 9225 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copoly.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® GV-5H PA*-GF50 Product description: Grivory GV-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® GV-5HL black 9914 PA*-GF50 Product description: Grivory GV-5HL black 9914 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® GVN-35H black 9915 PA*-GF35 Product description: Grivory GVN-35H is a 35% glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® GVS-5H nat PA*-GF50 Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® HTV-6H1 black 9205 PA6T/6I-GF60 Product description: Grivory HTV-6H1 black 9205 is a 60% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® LV-50H FWA nat PA12-GF50 Product description: Grilamid LV-50H FWA natural is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® LV-65H FWA black 9225 PA12-GF65 Product description: Grilamid LV-65H FWA black 9225 is a 65 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® LVX-50H nat PA12-GF50 Product description: Grilamid LVX-50H natural is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and st.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® TSG-50 PA666-GF50 Product description: Grilon TSG-50 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50 has the following important properties: High stiffne.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® TSG-50/4 FA PA666-GF50 Information provided by EMS Grivory |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® XE 3915 PA12-GF50 Product description: Grilamid XE 3915 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following produce profile:Good UV StabilityHigh impact strengthVe.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | DAM; ISO 11359-1/-2 |
| DuPont Performance Polymers Zytel® HTN FR52G45BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G45BL BK337 is a 45% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® GV-4H PA*-GF40 Product description: Grivory GV-4H natural is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide... |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® GV-6H black PA*-GF60 Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® GVX-6 H black 9915 PA*-GF60 Product description: Grivory GVX-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® HT1V-45 HY black 9205 PA6T/6I-GF45 Product description: Grivory HT1V-45 HY black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-45 HY .. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® HTV-5H1 nat PA6T/6I-GF50 Product description: Grivory HTV-5H1 natural is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
8.33 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/2 |
| Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
| CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
| EMS-Grivory Grivory® GV-4H black PA*-GF40 Product description: Grivory GV-4H black 9915 is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||