Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 90.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS (Asia Pacific)
Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics GELOY XP4020R ASA+PC (Asia Pacific)
ASA+PC may contain up to 20% post-industrial recycle. Excellent flow, weatherability, toughness and high heat for exterior uses.
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM data
Americas Styrenics Styron® 489M High Impact Polystyrene  (discontinued **)
STYRON® 489M high impact polystyrene resin is a high flow resin with excellent impact. When used unmodified for the manufacture of food contact articles STYRON 489M complies with the US Food, Drug ..
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM data
Americas Styrenics Styron® 613 Polystyrene  (discontinued **)
STYRON® 613 high heat, high strength general purpose polystyrene is typically used in applications requiring a clear, tough part such as office products and magnetic media enclosures. It offers goo..
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM data
Americas Styrenics Styron® 678C Polystyrene  (discontinued **)
STYRON® 678C general purpose polystyrene resin is a high flow, medium strength resin with good scuff resistance. It is typically used in thin-wall or consumer electronic applications. When used unm..
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM data
Americas Styrenics Styron® 685 Polystyrene  (discontinued **)
STYRON® 685 general purpose polystyrene resin is a high heat resin used in consumer electronics and housewares. It offers excellent clarity, good moldability for use in hot runner systems. When use..
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Ineos ABS Lustran® 723-1, Extrusion Grade  (discontinued **)
Extrusion grade for refrigerator inliner.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a..
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Ineos ABS LUSTROPAK® 1020 ABS, Extrusion Grade  (discontinued **)
Extrusion grade.Applications: Food containers, blister packs.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority ..
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Lanxess Durethan® B 30 S FN40 000000 Nylon 6
PA 6, injection molding grade, non- reinforced, good flowability, easy-release, fast cycling, UL 94V-2 off 0,75 mm, GWIT 775°C bei 0,75/1,5mm
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Lanxess Pocan® KU 2-7503/1 000000 PBT
PBT, non-reinforced, injection molding, extrusion, flame retardant
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1, -2
Lanxess Pocan® C 1202 000000 PET + PC
PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS.
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Styrolution NOVODUR® P3H-AT ABS, Injection Grade
Injection molding grade, antistatic, high gloss, improved chemical and dynamic resistance.Applications: Housings for telephones and household appliances.
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics NORYL GTX GTX924 PPE+PA (Europe-Africa-Middle East)
NORYL GTX 924 is an UV stabilized unfilled Noryl GTX grade with improved processability. Noryl GTX 924 is specially designed for wheeltrim applications.
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ASTM D696
Techmer ES Plastiblend® ABS CR X BK
Availability: North AmericaForms: PelletsFeatures: Good Chemical ResistanceUses: Electrical PartsAppearance: BlackInformation provided by TP Composites, Inc.
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
PlastxWorld CEVIAN®-V 660SF ABS
High Flow ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Covestro Bayblend® T 44 Polycarbonate/ABS Blend
Easier flowing than BAYBLEND T 45 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Covestro Baydur® 110 FR Polyurethane
Rigid microcellular RIM polyurethane material. Fast demold times; self releasing; long flow paths possible, therefore suitable for production of large moldings. Parts are injected through only one ..
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TR 55 LX PA12/MACMI
Product description: Grilamid TR 55 LX natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 55 LX natural offers outstanding prop..
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
Covestro Makroblend® DP UT3905 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseinjection molding grade Makroblend DP UT3905* offers superior flowability, good impact strength and excellent chemical resist..
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Covestro Makroblend® UT5205 PC/PBT Blend
Main characteristics:• High toughness even at low temperatures• Good chemical resistance• Good paintability• Good flowability• Low moisture intakeGrade characteristics:• Impact modified•..
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® TR 90 NZ PAMACM12-I
Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 90 NZ offers a variety of interesting properties such as: o..
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Arkema Group Rilsan® AMN Y TLD Nylon 12, MoS2 Filled (Conditioned)
Designation ISO 1874-PA12,MHLS,14-010,MD05Grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient. Goo..
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Arkema Group Rilsan® 6733 Nylon 11, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA11/xx,E,18-002Transparent and flexible copolymer for tubes extrusion. Additive free.High flexibility. Very good transparency. High chemical resistance.USP XXIII class VI appro..
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Polimeri Europa SINKRAL L320/G ABS, Platable Grade  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-20 Injection moulding grade, tailored for electroplating. It is a high flow grade with a good impact ..
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 23.0 - 55.0 °C
50.0 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1, -2
Lanxess Pocan® C 1206 000000 PET + PC
PET + PC, non-reinforced, injection molding, improved impact strengthInformation provided by LANXESS.
CTE, linear, Parallel to Flow 90.0 µm/m-°C
50.0 µin/in-°F
ISO 11359-1/-2
DSM Arnite® T06 204 XL PBT
Low Viscosity, Injection Molding, Low outgassing
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Polimeri Europa SINKRAL C443 ABS, Heat Stabilized  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-08-25-20 Medium heat injection moulding grade. The availability of different industrial processes to manufa..
Copyright © lookpolymers.com All Rights Reserved