Polymer Property : Transformation Temperature, Tg = 1260 °F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Transformation Temperature, Tg 680 °C
1260 °F
ISO 7884-8
Schott 8235 Dental Glass
Remarks: Ba-containing, without FApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SCHOTT North ..
Transformation Temperature, Tg 680 °C
1260 °F
ISO 7884-8
Schott G018-310 Dental Glass
Remarks: Zr-containing, high refractive indexApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by S..
Transformation Temperature, Tg 680 °C
1260 °F
ISO 7884-8
Schott GM32087 Dental Glass
Remarks: Sr-containing, low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SC..
Transformation Temperature, Tg 683 °C
1260 °F
Schott N-LASF9 Glass
Information Provided by SCHOTT North America, Inc.