| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Transformation Temperature | 138 - 143 °C | 280 - 289 °F | Temp at Max Expansion |
|
Akzo Nobel Expancel® 007 WUF 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Transformation Temperature | 138 - 146 °C | 280 - 295 °F | Temp at Max Expansion |
|
Akzo Nobel Expancel® 053 DU 40 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Transformation Temperature | 138 - 146 °C | 280 - 295 °F | Temp at Max Expansion |
|
Akzo Nobel Expancel® 053 WU 40 Wet unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Transformation Temperature | 138 - 148 °C | 280 - 298 °F | Expansion Starting Temperature |
|
Akzo Nobel Expancel® 950 DU 80 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Transformation Temperature | 138 - 148 °C | 280 - 298 °F | Expansion Starting Temperature |
|
Akzo Nobel Expancel® 950 DU 120 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||