| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Transformation Temperature | 188 - 200 °C | 370 - 392 °F | Temp at Max Expansion |
|
Akzo Nobel Expancel® 950 DU 80 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||
| Transformation Temperature | 190 - 200 °C | 374 - 392 °F | Temp at Max Expansion |
|
Akzo Nobel Expancel® 091 DU 140 Dry unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
|
|||